The paper reports the conditions necessary to hydride wrought bar or swarf of Ti-6Al-4V alloy and demonstrates the need for close temperature control. The dehydriding stage does not require such close temperature control but for a reasonable rate of powder production with minimum sintering of the product a temperature of 600 degree C has proved necessary.