Flexural Strength of Modern CAD/CAM Restoratives After Artificial Aging

被引:0
|
作者
Melc, Thomas [1 ]
Attin, Thomas [1 ]
Eyuboglu, Tan Firat [2 ]
Ozcan, Mutlu [3 ]
机构
[1] Univ Zurich, Ctr Dent Med, Clin Conservat & Prevent Dent, CH-8032 Zurich, Switzerland
[2] Istanbul Medipol Univ, Dept Endodont, Fac Dent, TR-34083 Istanbul, Turkiye
[3] Univ Zurich, Ctr Dent Med, Clin Masticatory Disorders & Dent Biomat, Zurich, Switzerland
关键词
aging; CAD/CAM; CAD/CAM materials; dental materials; lithium disilicate; prosthodontics; INFILTRATED CERAMIC-NETWORK; MECHANICAL-PROPERTIES; COMPOSITE; RESISTANCE; DEGRADATION; HARDNESS; SURFACE; WEAR;
D O I
10.3390/ma17215178
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Before clinical trials are initiated, studying the mechanical performance of modern CAD/CAM restorative materials exposed to aging conditions would provide insights on their performance in service. This study evaluated the impact of thermomechanical aging on various resin composite, ceramic, hybrid, and nano-filled resin composite materials after two polymerization modes. Specimens (3 x 4 x 14 mm(3)) were fabricated using (n = 12 per group) a universal composite (Filtek Supreme XTE photo-polymerized for either 40 s or 120 s per layer), hybrid ceramics (BRILLIANT Crios, GC Cerasmart, Lava Ultimate, VITA ENAMIC), glass ceramics (IPS e.max CAD, VITA Suprinity PC, Straumann n!ce), or feldspar ceramics (VITABLOCS Mark II, GC Initial LRF). In each group, half of the specimens underwent thermomechanical aging. A three-point bending test was applied to all specimens and the results were statistically analyzed (alpha = 0.05). Glass ceramics and hybrid ceramics presented higher flexural strength values than feldspar ceramics and the universal composite before and after aging (p < 0.05). Thermomechanical cycling affected the flexural strength of all materials (p < 0.05) except Lava Ultimate, Straumann n!ce, and GC Initial (p > 0.05). The highest decrease in flexural strength after aging was found in the universal composite (40 s polymerization) (p < 0.001) and Vita Enamic (p < 0.001), while the lowest decrease was in the hybrid ceramics, Cerasmart and Lava Ultimate (p < 0.05). Extending polymerization duration reduced the aging effect on the universal composite tested. Thermomechanical aging affected the flexural strength of most materials tested. Universal composites and feldspar ceramics presented similar flexural strength values.
引用
收藏
页数:13
相关论文
共 50 条
  • [41] Flexural strength of denture base acrylic resins processed by conventional and CAD-CAM methods
    Aguirre, Brian C.
    Chen, Jenn-Hwan
    Kontogiorgos, Elias D.
    Murchison, David F.
    Nagy, William W.
    JOURNAL OF PROSTHETIC DENTISTRY, 2020, 123 (04): : 641 - 646
  • [42] BALL-ON-THREE-BALLS BIAXIAL FLEXURAL STRENGTH OF BONDED AND UNBONDED CAD/CAM MATERIALS
    Shono, Nourah
    Elhejazi, Ahmed
    Maawadh, Ahmed
    Al Nahedh, Hend
    CERAMICS-SILIKATY, 2022, 66 (01) : 66 - 77
  • [43] Effect of Short-Term Aging on the Flexural Strength of a Novel Experimental CAD/CAM Fiber-Reinforced Composite Material: A Pilot Study
    Cekic-Nagas, Isil
    Nagas, Emre
    Egilmez, Ferhan
    Ergun, Gulfem
    Vallittu, Pekka K.
    Lassila, Lippo
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2020, 33 (05) : 523 - 526
  • [44] CAD/CAM GOES FROM STRENGTH TO STRENGTH
    WAKE, M
    NAVAL ARCHITECT, 1991, : E182 - &
  • [45] Evaluation of repair bond strength of a dental CAD/CAM resin composite after surface treatment with two Er,Cr:YSGG laser protocols following artificial aging
    Didangelou, Pavlina
    Dionysopoulos, Dimitrios
    Papadopoulos, Constantinos
    Strakas, Dimitrios
    Mourouzis, Petros
    Tolidis, Kosmas
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2023, 146
  • [46] Edge strength of CAD/CAM materials
    Pfeilschifter, Maria
    Preis, Verena
    Behr, Michael
    Rosentritt, Martin
    JOURNAL OF DENTISTRY, 2018, 74 : 95 - 100
  • [47] Comparative study of flexural strength test methods on CAD/CAM Y-TZP dental ceramics
    Xu, Yongxiang
    Han, Jianmin
    Lin, Hong
    An, Linan
    REGENERATIVE BIOMATERIALS, 2015, 2 (04) : 239 - 244
  • [48] Effect of Simulated Gastric Acid on Aesthetical Restorative CAD-CAM Materials' Microhardness and Flexural Strength
    Gulakar, T. L.
    Comert, G. N.
    Karaman, E.
    Cakan, U.
    Ozel, G. S.
    Ahmet, S. O.
    NIGERIAN JOURNAL OF CLINICAL PRACTICE, 2023, 26 (10) : 1505 - 1511
  • [49] Effectiveness of surface treatments on fatigue and static flexural bond strength of a CAD-CAM resin composite
    Pilecco, Rafaela Oliveira
    da Rosa, Lucas Saldanha
    Soares, Pablo Machado
    Rippe, Marilia Pivetta
    Valandro, Luiz Felipe
    Tribst, Joao Paulo Mendes
    dal Piva, Amanda Maria de Oliveira
    Kleverlaan, Cornelis Johannes
    Pereira, Gabriel Kalil Rocha
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2025, 140
  • [50] Effect of Thermocycling on Biaxial Flexural Strength of CAD/CAM, Bulk Fill, and Conventional Resin Composite Materials
    Benalcazar Jalkh, E. B.
    Machado, C. M.
    Gianinni, M.
    Beltramini, I
    Piza, M. M. T.
    Coelho, P. G.
    Hirata, R.
    Bonfante, E. A.
    OPERATIVE DENTISTRY, 2019, 44 (05) : E254 - E262