共 50 条
- [46] FRICTION AND WEAR CHARACTERISTICS OF ELECTROLESS NI-P-PTFE COMPOSITE COATINGS PLATING AND SURFACE FINISHING, 1994, 81 (01): : 48 - 50
- [47] Effect of surfactants on the behavior of the Ni-P bath and on the formation of electroless Ni-P-TiC composite coatings SURFACE & COATINGS TECHNOLOGY, 2019, 361 : 42 - 49
- [48] INFLUENCE OF CATHODIC POLARIZATION ON THE PLATING RATE AND PROPERTIES OF ELECTROLESS NI-P COATINGS TRANSACTIONS OF THE INSTITUTE OF METAL FINISHING, 1986, 64 : 24 - 29
- [49] Preparation and characterization of electroless Ni-P and Ni-P-Si3N4 composite coatings TRANSACTIONS OF THE INSTITUTE OF METAL FINISHING, 1999, 77 : 84 - 86
- [50] Electroless Ni-P and Ni-P-Al2O3 Nanocomposite Coatings and Their Corrosion and Wear Resistance Journal of Materials Engineering and Performance, 2013, 22 : 176 - 183