Deformation behavior and constitutive equation of Sn-37Pb solder alloy at cryogenic temperature

被引:0
|
作者
Zhou, Ning [1 ]
Li, Shengli [1 ]
Wu, Lin [2 ]
Hang, Chunjin [1 ,3 ]
Zhang, Wei [1 ]
Tian, Yanhong [1 ,3 ]
Ding, Ying [4 ]
机构
[1] Harbin Inst Technol, State Key Lab Adv Welding & Joining, Harbin 150001, Peoples R China
[2] Heilongjiang Univ, Harbin 150001, Peoples R China
[3] Harbin Inst Technol, Zhengzhou Res Inst, Zhengzhou 450041, Peoples R China
[4] Beijing Inst Control Engn, Beijing 100094, Peoples R China
来源
MATERIALS TODAY COMMUNICATIONS | 2024年 / 41卷
基金
中国国家自然科学基金;
关键词
Sn-37Pb solder alloy; Tensile property; Fracture behavior; Cryogenic temperature; Constitutive equation; MECHANICAL-PROPERTIES; STRAIN-RATE; 63SN/37PB; JOINTS; MODEL;
D O I
10.1016/j.mtcomm.2024.110554
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this work, the tensile property, ductile-to-brittle transition (DBT) mechanism and constitutive relations of 63Sn-37Pb (Sn-37Pb) solder alloy at cryogenic temperature were studied by uniaxial tensile experiments for different temperatures. The tensile strength of Sn-37Pb solder alloy increases from 38.2 MPa (293 K) to 178.9 MPa (123 K) and then declines to 145.2 MPa (77 K) with decreases of temperature, and its fracture elongation changes from 42.8% (293 K) to 10.2% (77 K). Mechanical behavior of Pb second phase in Sn-37Pb alloy at low temperatures is illustrated: when the temperature drops to 123 K and below, the fracture failure of beta-Sn matrix occurs in an open mode. As a result, Sn-37Pb solder alloy fails by brittle fracture mode. Anand model is adopted as a unified viscoplastic intrinsic law to describe the intrinsic relationship of Sn-37Pb solder alloys. Above 123 K, Anand model can effectively fit the stress-strain curves of Sn-37Pb solder alloys. When the temperature lower than 123 K, the deformation characters of Sn-37Pb solder alloys change from elastoviscoplastic to elasto-plastic, and Anand model is unable to continue to fit the intrinsic relationship of Sn37Pb solder alloys. Sn-37Pb solder alloy exhibits more obvious strain hardening at low temperature, and its low-temperature intrinsic response is successfully described by Hollomon's equation. The research method of the solder alloy is of great significance to solve the reliability problem of low temperature electronic devices.
引用
收藏
页数:9
相关论文
共 50 条
  • [1] Fracture behavior and constitutive relations of Sn-3.0Ag-0.5Cu solder alloy at cryogenic temperature
    Li, Shengli
    Hang, Chunjin
    Zhang, Wei
    Tian, Yanhong
    Yu, Dan
    Ding, Ying
    Wang, Xiuli
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 896
  • [2] Mechanical properties degradation of Sn-37Pb solder joints caused by interfacial microstructure evolution under cryogenic temperature storage
    Tian, Ruyu
    Chen, Shuai
    Feng, Jiayun
    Wang, Shang
    Hang, Chunjin
    Ding, Ying
    Tian, Yanhong
    MATERIALS CHARACTERIZATION, 2023, 201
  • [3] On the constitutive response of 63/37 Sn/Pb eutectic solder
    Skipor, AF
    Harren, SV
    Botsis, J
    JOURNAL OF ENGINEERING MATERIALS AND TECHNOLOGY-TRANSACTIONS OF THE ASME, 1996, 118 (01): : 1 - 11
  • [4] Influence of thermal shock cycles on Sn-37Pb solder bumps
    Gan, Guisheng
    Xia, Da-quan
    Liu, Xin
    Liu, Cong
    Cheng, Hanlin
    Ming, Zhongzhen
    Gao, Haoyang
    Yang, Dong-hua
    Wu, Yi-ping
    SOLDERING & SURFACE MOUNT TECHNOLOGY, 2019, 31 (02) : 85 - 92
  • [5] Using nanoindentation to investigate the temperature cycling of Sn-37Pb solders
    Wen, Hua-Chiang
    Chou, Wu-Ching
    Lin, Po-Chen
    Jeng, Yeau-Ren
    Chen, Chien-Chang
    Chen, Hung-Ming
    Jiang, Don Son
    Cheng, Chun-Hu
    MICROELECTRONICS RELIABILITY, 2017, 78 : 111 - 117
  • [6] The Effects of the Strain Rate and Temperature on the Cyclic Deformation Behavior of 63Sn-37Pb Solder Alloy under Uniaxial Cyclic Straining
    Yan, Luo
    2011 INTERNATIONAL CONFERENCE ON ENVIRONMENTAL SYSTEMS SCIENCE AND ENGINEERING (ICESSE 2011), VOL 1, 2011, : 207 - 212
  • [7] Strain Rate and Temperature-Dependent Deformation Behavior for Pb-10wt%Sn Solder Alloy
    Alsowidy, S. M.
    ARABIAN JOURNAL FOR SCIENCE AND ENGINEERING, 2012, 37 (01): : 163 - 169
  • [8] Influence of Interfacial Intermetallic Growth on the Mechanical Properties of Sn-37Pb Solder Joints under Extreme Temperature Thermal Shock
    Hang, Chunjin
    Tian, Ruyu
    Zhao, Liyou
    Tian, Yanhong
    APPLIED SCIENCES-BASEL, 2018, 8 (11):
  • [9] Strain Rate and Temperature-Dependent Deformation Behavior for Pb–10wt%Sn Solder Alloy
    S. M. Alsowidy
    Arabian Journal for Science and Engineering, 2012, 37 : 163 - 169
  • [10] Effects of Interaction Between Sn-Rich and Pb-Rich Phases on the Mechanical Properties of Sn-Pb Eutectic Solder Alloy at Cryogenic Temperature
    An, Qi
    Zhang, Minghua
    Wang, Ningning
    Fei, Jingming
    JOURNAL OF ELECTRONIC MATERIALS, 2025, 54 (03) : 2368 - 2387