SLM Magnesium Alloy Micro-Arc Oxidation Coating

被引:1
作者
Yue, Xuejie [1 ]
Xu, Kangning [2 ]
Wang, Shuyi [2 ]
Liu, Hengyan [2 ]
Guo, Shiyue [3 ]
Zhao, Rusheng [4 ]
Xu, Gaopeng [2 ]
Wang, Hao [5 ]
Yue, Xuezheng [2 ]
机构
[1] Xinxiang Univ, Sch Civil Engn & Architecture, Xinxiang 453000, Peoples R China
[2] Univ Shanghai Sci & Technol, Dept Mat Sci & Chem, Shanghai 200093, Peoples R China
[3] Wuhan Univ Technol, Hubei Longzhong Lab, Xiangyang 441000, Peoples R China
[4] Tokyo Metropolitan Univ, Tokyo 1920397, Japan
[5] Chinese Acad Sci, Inst Met Res, Shenyang 110016, Peoples R China
基金
中国国家自然科学基金;
关键词
selected laser melting; magnesium alloys; micro-arc oxidation; wetting angle; corrosion resistance; CORROSION-RESISTANCE; SURFACE-MORPHOLOGY; MICROSTRUCTURE; PERFORMANCE; MECHANISM; IMPLANTS;
D O I
10.3390/ma17204988
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this study, we utilized Selective Laser Melting (SLM) technology to fabricate a magnesium alloy, and subsequently subject it to micro-arc oxidation treatment. We analyzed and compared the microstructure, elemental distribution, wetting angle, and corrosion resistance of the SLM magnesium alloy both before and after the micro-arc oxidation process. The findings indicate that the SLM magnesium alloy exhibits surface porosity defects ranging from 2% to 3.2%, which significantly influence the morphology and functionality of the resulting film layer formed during the micro-arc oxidation process. These defects manifest as pores on the surface, leading to an uneven distribution of micropores with varying sizes across the layer. The surface roughness of the 3D-printed magnesium alloy exhibits a high roughness value of 180 nanometers. The phosphorus (P) content is lower within the film layer compared to the surface, suggesting that the Mg3(PO4)2 phase predominantly resides on the surface, whereas the interior is primarily composed of MgO. The micro-arc oxidation process enhances the hydrophilicity and corrosion resistance of the SLM magnesium alloy, thereby potentially endowing it with bioactivity. Additionally, the increased surface roughness post-treatment promotes cell proliferation. However, certain inherent defects present in the SLM magnesium alloy samples negatively impact the improvement of their corrosion resistance.
引用
收藏
页数:14
相关论文
共 27 条
[1]   Biodegradable magnesium alloys for orthopaedic applications: A review on corrosion, biocompatibility and surface modifications [J].
Agarwal, Sankalp ;
Curtin, James ;
Duffy, Brendan ;
Jaiswal, Swarna .
MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2016, 68 :948-963
[2]   Bioactivity enhancement by Sr doped Zn-Ca-P coatings on biomedical magnesium alloy [J].
Amaravathy, P. ;
Kumar, T. S. Sampath .
JOURNAL OF MAGNESIUM AND ALLOYS, 2019, 7 (04) :584-596
[3]   Effect of gas protection on form and microstructure of wire arc additive manufactured WE43 magnesium alloy [J].
Chen, Fukang ;
Cai, Xiaoyu ;
Dong, Bolun ;
Lin, Sanbao .
MATERIALS LETTERS, 2024, 367
[4]   Corrosion performance of plasma electrolytic oxidized AZ31 magnesium alloy in silicate solutions with different additives [J].
Chen, Huan ;
Lv, GuoHua ;
Zhang, GuLing ;
Pang, Hua ;
Wang, XingQuan ;
Lee, HeonJu ;
Yang, SiZe .
SURFACE & COATINGS TECHNOLOGY, 2010, 205 :S32-S35
[5]   In vitro degradation and antibacterial property of a copper-containing micro-arc oxidation coating on Mg-2Zn-1Gd-0.5Zr alloy [J].
Chen, Junxiu ;
Zhang, Yi ;
Ibrahim, Muhammad ;
Etim, Iniobong P. ;
Tan, Lili ;
Yang, Ke .
COLLOIDS AND SURFACES B-BIOINTERFACES, 2019, 179 :77-86
[6]   Mechanical and corrosion properties of full liquid phase sintered WE43 magnesium alloy specimens fabricated via binder jetting additive manufacturing [J].
Cho, Dae Hyun ;
Dean, David ;
Luo, Alan A. .
JOURNAL OF MAGNESIUM AND ALLOYS, 2024, 12 (07) :2711-2724
[7]   Plasma electrolytic oxidation of magnesium and its alloys: Mechanism, properties and applications [J].
Darband, Gh. Barati ;
Aliofkhazraei, M. ;
Hamghalam, P. ;
Valizade, N. .
JOURNAL OF MAGNESIUM AND ALLOYS, 2017, 5 (01) :74-132
[8]   Bilayer micro-arc oxidation-poly (glycerol sebacate) coating on AZ91 for improved corrosion resistance and biological activity [J].
Ghafarzadeh, Mohsen ;
Kharaziha, Mahshid ;
Atapour, Masoud .
PROGRESS IN ORGANIC COATINGS, 2021, 161
[9]   The role of anions in the formation and corrosion resistance of the plasma electrolytic oxidation coatings [J].
Ghasemi, A. ;
Raja, V. S. ;
Blawert, C. ;
Dietzel, W. ;
Kainer, K. U. .
SURFACE & COATINGS TECHNOLOGY, 2010, 204 (9-10) :1469-1478
[10]   Tough Bonding, On-Demand Debonding, and Facile Rebonding between Hydrogels and Diverse Metal Surfaces [J].
Li, Weichang ;
Liu, Xiaobo ;
Deng, Zhishuang ;
Chen, Yutong ;
Yu, Qianqian ;
Tang, Wen ;
Sun, Tao Lin ;
Zhang, Yu Shrike ;
Yue, Kan .
ADVANCED MATERIALS, 2019, 31 (48)