Effect of lime neutralization wastewater on the performance of alkali-activated slag/fly ash mortars

被引:0
作者
Zhou, Tao [1 ]
Li, Jin [1 ,2 ,3 ]
机构
[1] Anhui Univ Sci & Technol, Sch Civil Engn & Architecture, Huainan 232001, Peoples R China
[2] Anhui Univ Sci & Technol, State Key Lab Min Response & Disaster Prevent & Co, Huainan 232001, Anhui, Peoples R China
[3] Anhui Hongchang New Mat Co Ltd, Huaibei 35199, Anhui, Peoples R China
关键词
Alkali-activated slag/fly ash; Neutralization wastewater; Nanomechanical properties; Compressive strength; Pore structure; PHASE-CHANGE MATERIALS; CONCRETE; SHRINKAGE; SEAWATER; PASTES; CEMENT;
D O I
10.1617/s11527-024-02494-9
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
This paper was conducted to upcycle lime-neutralize etching wastewater (LNW), produced from the etching of cenospheres for producing perforated cenospheres, into alkali-activated slag/fly ash, considering the high contents of Ca2+ (Calcium ion), Cl- (Chloride ion), and OH- (Hydroxyl). The aim of this study is to limit the discharge of calcium-rich wastewater and minimize the pollution of water and soil resources. To this end, the effects of different LNW content on the fresh properties, hydration products, compressive strength, microstructure and nanomechanical properties of AASF were investigated. Results revealed that the addition of LNW extended the setting times and inhibited the early hydration of AASF due to the existence of Ca2+ and NH4+ (Ammonium) in LNW. In addition, the existence of Ca2+ in LNW reacts with NaOH to form Ca(OH)(2), which can work as an auxiliary activator for AASF. Consequently, the LNW-added AASF mortars exhibited denser pore structures and higher compressive strengths. By using 25-100% LNW, the compressive strengths of AASF mortars can be improved by 2.7-18.9% (3d), 4.8-19.5% (7d) and 5.6-19.7% (28d), respectively.
引用
收藏
页数:11
相关论文
共 35 条
[2]  
[Anonymous], 2019, Standard practice for making and curing concrete test specimens in the laboratory
[3]  
[Anonymous], 2014, ANN BOOK ASTM STAND, DOI DOI 10.1520/C0191-21
[4]  
[Anonymous], 2020, Standard Test Mrthod for Flow of Hydraulic Cement Mortar 1
[5]  
ASTM D, 1993, Standard Test Method for Precipitated Silica-Surface Area by Multipoint BET Nitrogen Adsorption 1
[6]   Effect of combined activator of Ca(OH)2 and Na2CO3 on workability and compressive strength of alkali-activated ferronickel slag system [J].
Bian, Zuwang ;
Jin, Guowang ;
Ji, Tao .
CEMENT & CONCRETE COMPOSITES, 2021, 123
[7]   Ultra-low thermal conductivity thermal barrier coatings from recycled fly-ash cenospheres [J].
Chavez-Valdez, A. ;
Arizmendi-Morquecho, A. ;
Vargas, G. ;
Almanza, J. M. ;
Alvarez-Quintana, J. .
ACTA MATERIALIA, 2011, 59 (06) :2556-2562
[8]   Pre-carbonation of calcium carbide slag for the preparation of eco-friendly mortars [J].
Chen, Peiyuan ;
Wang, Chunjie ;
Wang, Yonghui ;
Xie, Jiankai ;
Shen, Xin ;
Wang, Cheng ;
Wang, Jialai .
CONSTRUCTION AND BUILDING MATERIALS, 2023, 399
[9]   Perforated cenospheres: A reactive internal curing agent for alkali activated slag mortars [J].
Chen, Peiyuan ;
Wang, Jialai ;
Wang, Liang ;
Xu, Ying .
CEMENT & CONCRETE COMPOSITES, 2019, 104
[10]   Converting hollow fly ash into admixture carrier for concrete [J].
Chen, Peiyuan ;
Wang, Jialai ;
Liu, Fengjuan ;
Qian, Xin ;
Xu, Ying ;
Li, Jin .
CONSTRUCTION AND BUILDING MATERIALS, 2018, 159 :431-439