Creep strength evaluation of a long-term used boiler weldment part on 2.25Cr-1Mo steel by using miniature specimens

被引:0
|
作者
Kakikoshi T. [1 ]
Ogata T. [1 ]
机构
[1] Faculty of Engineering, Chiba Inst. of Tech., Tsudanuma, Narashino
来源
| 1600年 / Society of Materials Science Japan卷 / 69期
关键词
2.25Cr-1Mo steel welded joint; Creep damage; Creep strength; Finite element analysis; Long-term operation; Miniature specimen;
D O I
10.2472/jsms.69.408
中图分类号
学科分类号
摘要
Creep damage gradually progress during operation especially at weldment parts of 2.25Cr-1Mo steel boiler pipes. In creep damage assessment of the weldment parts based on stress analysis by a finite element method, creep deformation property of constituent materials in the welded joint has to be obtained. Additionally, it is desired to develop a creep damage assessment method by using a miniature specimen. In this study, in order to clarify influence of a long-term operation on creep strength property, creep tests were performed in inert gas condition using miniature specimens with 1mm diameter taken from each portion of constituent materials of a welded joint in a long-term used boiler header. Although minimum creep strain rates of a base metal and a fine grain are similar to those in a new welded joint, those of a weld metal and a coarse grain are much higher than those in the new welded joint indicating significant reduction of creep strength in the weld metal and the coarse grain occurred during the long-term operation. Creep rupture times of the miniature welded joint specimens are almost equal to those of the standard welded joint specimens. Therefor creep rupture time of the standard welded joint specimen may be predicted by a creep test result of the miniature welded joint specimen. From creep test results of the miniature welded joint specimen taken from creep damaged standard welded joint specimen, it was demonstrated that creep damage greater than medium level can be evaluated by using the miniature welded joint creep specimen. © 2020 The Society of Materials Science, Japan
引用
收藏
页码:408 / 415
页数:7
相关论文
共 18 条
  • [1] Effect of initial microstructure on long-term creep strength properties of 2.25Cr-1Mo steel
    Kushima, H
    Kimura, K
    Abe, F
    Yagi, K
    Irie, H
    Maruyama, K
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1999, 85 (11): : 848 - 855
  • [2] TOUGHNESS AND CREEP STRENGTH OF MODIFIED 2.25CR-1MO STEEL WELD METAL
    ICHIKAWA, K
    HORII, Y
    SUEDA, A
    KOBAYASHI, J
    WELDING JOURNAL, 1995, 74 (07) : S230 - S238
  • [3] Evaluation of creep strength property of long-term used Mod.9Cr-1Mo welded joint
    Ogata T.
    Watanabe A.
    2018, Society of Materials Science Japan (67) : 632 - 638
  • [4] INFLUENCE OF STRESS AND STRAIN ON THE CREEP DAMAGE OF A 2.25CR-1MO STEEL
    ENDO, T
    TAI, K
    MASUYAMA, F
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1994, 80 (05): : 412 - 417
  • [5] Influence of specimen geometry on creep strength of long-term used Mod.9Cr-1Mo steel welded joint
    Yamazaki H.
    Ogata T.
    Zairyo/Journal of the Society of Materials Science, Japan, 2019, 68 (02): : 91 - 98
  • [6] Effect of Multiaxial State of Stress on Creep Rupture Behaviour of 2.25Cr-1Mo Steel
    Goyal, Sunil
    Laha, K.
    Vijayanand, V. D.
    Selvi, S. Panneer
    Mathew, M. D.
    6TH INTERNATIONAL CONFERENCE ON CREEP, FATIGUE AND CREEP-FATIGUE INTERACTION, 2013, 55 : 510 - 516
  • [7] CREEP-BEHAVIOR ANALYSIS OF A SERVICE-EXPOSED 2.25CR-1MO STEEL
    SHI, JZ
    TAI, KC
    ENDO, T
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1995, 81 (08): : 839 - 844
  • [8] Evaluation of creep strength property of Mod.9Cr-1Mo welded joint by using a miniature specimen
    Ogata T.
    Chiwaki K.
    2017, Society of Materials Science Japan (66) : 93 - 100
  • [9] Influence of Coarsening Microstructure in Weld Metal on Creep Strength of a Long-Term Used Mod.9Cr-1Mo Welded Joint
    Ikegami H.
    Ogata T.
    Zairyo/Journal of the Society of Materials Science, Japan, 2024, 73 (04) : 321 - 327
  • [10] STRAIN-MEASUREMENT BY INTRA-GRANULAR DISTORTION ANALYSIS IN CREEP OF 2.25CR-1MO STEEL
    YOSHIZAWA, H
    NAKASHIRO, M
    KIHARA, S
    NAKAGAWA, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1995, 81 (02): : 141 - 146