Additive manufacturing of sustainable and heat-resistant Al-Fe-Mo-Si-Zr alloys

被引:0
|
作者
Sun, Zhongji [1 ]
Roscher, Moritz [2 ]
Paolantonio, Mario Claudio [2 ]
Soh, Verner [1 ]
Liu, Chang [3 ]
Tsai, Shao-Pu [4 ]
Ng, Chee Koon [1 ]
Tan, Cheng Cheh [1 ]
Wang, Pei [1 ]
Jaegle, Eric A. [5 ]
机构
[1] ASTAR, Inst Mat Res & Engn IMRE, 2 Fusionopolis Way,Innovis 08-03, Singapore 138634, Singapore
[2] Max Planck Inst Sustainable Mat GmbH, Dept Microstruct Phys & Alloy Design, Max Planck Str 1, D-40237 Dusseldorf, Germany
[3] Xi An Jiao Tong Univ, Ctr Alloy Innovat & Design CAID, State Key Lab Mech Behav Mat, Xian, Peoples R China
[4] Natl Taiwan Univ, Dept Mat Sci & Engn, Taipei 10617, Taiwan
[5] Univ Bundeswehr Munchen, Inst Mat Sci, D-85579 Neubiberg, Germany
关键词
Sustainability; Additive manufacturing; Supersaturated alloys; Metastable intermetallic compounds; And cracking; MECHANICAL-PROPERTIES; THERMAL-STABILITY; MICROSTRUCTURAL EVOLUTION; PROPERTY; STRENGTH; REMOVAL; STEEL; IRON;
D O I
10.1016/j.jallcom.2024.177118
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Improving the sustainability of metals and alloys is essential for slowing down global warming. The reason is that their extraction and production stand for about 40 % of all greenhouse gas emissions in the industrial sector. This motivates new alloy design and processing criteria such as the (1) preferred use of abundant and sustainable alloying elements and (2) improved material tolerance against impurity intrusion from recycling. In this context, additive manufacturing (AM) is attractive, through rapid solidification, capable of quenching impurities into a solid solution state, avoiding formation of large intermetallics and introduction of metastable phases. Here, by using this approach we show how iron, an important scrap-related contaminant in aluminum alloys, can be turned from a harmful into a valuable ingredient. Specifically, the addition of Mo and Si facilitates the formation of beneficial metastable body-centred cubic (BCC) Al12(Fe, Mo)3Si phase, instead of more stable but detrimental intermetallic variants commonly observed in Al-Fe alloys. The as-built microstructures have excellent thermal stability, tested up to 200 hours at 300 degrees C, because of low diffusivity of Fe and the formation of Zr shell. We find that for such supersaturated alloys, two issues are important, namely (a) the heterogeneous microstructures in the as-built condition, (b) the evolution of metastable precipitates during heating. We suggest that this type of approach help to guide sustainable alloy design via AM and other rapid solidification processes.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] Pressureless Sintering of Mo-Si-B Alloys with Fe Additive
    Ouyang, Gaoyuan
    Ray, Pratik K.
    Kramer, Matthew J.
    Akinc, Mufit
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (05) : 2417 - 2422
  • [22] Pressureless Sintering of Mo-Si-B Alloys with Fe Additive
    Gaoyuan Ouyang
    Pratik K. Ray
    Matthew J. Kramer
    Mufit Akinc
    Journal of Materials Engineering and Performance, 2017, 26 : 2417 - 2422
  • [23] Manufacturing of Ti–Al–Zr–Mo–V Alloy Components by Additive Methods
    V. M. Semenchuk
    A. V. Nikolaeva
    N. L. Savchenko
    A. P. Zykova
    A. V. Chumaevskii
    S. Yu. Nikonov
    E. A. Kolubaev
    Russian Physics Journal, 2024, 66 : 1180 - 1188
  • [24] ASSESTMENT OF THE Al-Ni-Mn-Fe-Si-Zr PHASE DIAGRAM FOR NEW GENERATION HEAT RESISTANT CASTING ALUMINUM ALLOYS
    Belov, N. A.
    Alabin, A. N.
    PROCEEDINGS OF THE 13TH INTERNATIONAL CONFERENCE ON ALUMINUM ALLOYS (ICAA13), 2012, : 123 - 128
  • [25] Synthesis and characterization of heat-resistant composites in the Mo-Si-C system
    Belikova, AF
    Gorshkov, VA
    Kobyakov, VP
    Komratov, GN
    Ponomarev, VI
    Yukhvid, VI
    INORGANIC MATERIALS, 1996, 32 (04) : 382 - 387
  • [26] Heat-resistant Al-0.2Sc-0.04Zr electrical conductor
    Zhou, W. W.
    Cai, B.
    Li, W. J.
    Liu, Z. X.
    Yang, S.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 552 : 353 - 358
  • [27] Structure and coarsening behavior of the strengthening phase in RS Al-Fe-Mo-Si-Zr-Ti alloys
    Dai, SL
    Yu, GF
    Yan, MG
    ADVANCED PERFORMANCE MATERIALS, 1995, 2 (03): : 289 - 298
  • [28] Highly heat-resistant powder Fe-Cr-Al alloy
    TsNIIchermet, Moscow, Russia
    Stal', 2002, (01): : 75 - 76
  • [29] Characterization of Al–Fe–V–Si heat-resistant aluminum alloy components fabricated by selective laser melting
    Shaobo Sun
    Lijing Zheng
    Yingying Liu
    Jinhui Liu
    Hu Zhang
    Journal of Materials Research, 2015, 30 : 1661 - 1669
  • [30] Welding of Highly Heat-Resistant Fe-Ni-Cr Alloys.
    Smoktun, Horst
    Berger, Guenther
    Kothe, Bodo
    Schweisstechnik (Berlin), 1973, 23 (03): : 102 - 105