Precipitates in X70 pipeline steel

被引:0
|
作者
Materials Science and Engineering School, University of Science and Technology Beijing, Beijing 100083, China [1 ]
不详 [2 ]
机构
来源
Beijing Keji Daxue Xuebao | 2006年 / 3卷 / 253-258期
关键词
Electron diffraction - Strength of materials - Titanium compounds - Transmission electron microscopy;
D O I
暂无
中图分类号
学科分类号
摘要
The precipitates in X70 acicular ferrite pipeline steel were investigated by transmission electron microscope. There are two typical precipitates in X70 pipeline steel. One is cubic shaped compound precipitates Ti(Nb)NC with the size of 50 nm-1 μm, in which TiN plays the main role and the ratio of Ti/Nb reaches 5-12. The other is spherical shaped Nb(Ti)C with the size less than 20 nm, in which NbC is the main phase with the ratio of Nb/Ti within 1-6.37. The spherical shaped precipitates exist in multi-grains proved by electron diffraction. The cubic shaped precipitates formed above 1150°C, and varied scarcely during the process afterwards. The spherical (ellipsoidal) shaped precipitates emerged almost totally in the range of 900°C to 1100°C, and kept coherent or semi-coherent relationship with the matrix. The precipitate of V was not obviously observed reminding the weak effect of V in steel. The results from the high-temperature ductility and strength curves show that the precipitation started at 1050°C and the amount of the precipitates reach the highest within the temperature range of 900°C-50°C in the condition of no deformation.
引用
收藏
相关论文
共 50 条
  • [21] The charpy notch impact test of X70 pipeline steel
    Yang, Z
    Guo, WL
    Dong, H
    Lu, MX
    Zhao, XW
    Luo, JH
    ACTA METALLURGICA SINICA, 2003, 39 (02) : 159 - 163
  • [22] Dynamic recrystallization kinetics model of X70 pipeline steel
    Xu, Yaowen
    Tang, Di
    Song, Yong
    Pan, Xiaogang
    MATERIALS & DESIGN, 2012, 39 : 168 - 174
  • [23] Microstructure and grain boundary microanalysis of X70 pipeline steel
    J. Wang
    A. Atrens
    Journal of Materials Science, 2003, 38 : 323 - 330
  • [24] Cracking Failure Analysis of X70 Pipeline Steel Weld
    Wang, Bin
    Zhang, Senfeng
    Zhou, Cui
    Liu, Nan
    Wang, Liang
    Tian, Xiaoyu
    ADVANCES IN ENERGY AND ENVIRONMENTAL MATERIALS, 2018, : 371 - 386
  • [25] A CCT Diagram for an Offshore Pipeline Steel of X70 Type
    Onsoien, M. I.
    M'Hamdi, M.
    Mo, A.
    WELDING JOURNAL, 2009, 88 (01) : 1S - 6S
  • [26] Continuous cooling transformation behavior of X70 pipeline steel
    Yang, Hongmei
    MATERIAL DESIGN, PROCESSING AND APPLICATIONS, PARTS 1-4, 2013, 690-693 : 2205 - 2209
  • [27] Electronic band structure of passive film on X70 pipeline steel
    Zeng, YM
    Luo, JL
    ELECTROCHIMICA ACTA, 2003, 48 (23) : 3551 - 3562
  • [28] Tension fracture behaviors of welded joints in X70 steel pipeline
    Kong, Dejun
    Wu, Yongzhong
    Long, Dan
    Zhou, Chaozheng
    THEORETICAL AND APPLIED MECHANICS LETTERS, 2011, 1 (03)
  • [29] Evaluation of the fracture toughness of X70 pipeline steel with ferritebainite microstructure
    Liu Ligang
    Xiao Hong
    Li Qiang
    Liu Yu
    Li Peishuai
    Yang Zhiqiang
    Yu Hui
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 688 : 388 - 395
  • [30] Development of High Deformation X70 Pipeline Steel Plates in NISCO
    Liu Zhao-xia
    Li Xiao-ling
    Chen Yuan-shu
    Song Shi-jia
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2011, 18 : 915 - 919