Mechanical properties of Halloysites-based and Halloysites-modified slag/fly ash-based geopolymers

被引:0
作者
Fan, Lidan [1 ]
Wu, Duoshen
Yu, Yongqiang [1 ]
Yang, Jie
Zhang, Jiyun
Li, Peitao
Guo, Jiaqi
机构
[1] Henan Polytech Univ, Sch Civil Engn, Jiaozuo 454003, Henan, Peoples R China
来源
JOURNAL OF BUILDING ENGINEERING | 2024年 / 98卷
基金
中国国家自然科学基金;
关键词
Halloysite; Calcination temperature; Thermally induced microstructural evolution; Geopolymer; Chemical bonding; Mechanical property; COMPRESSIVE STRENGTH; CURING TEMPERATURE; MOLAR RATIO; NANOTUBES; MICROSTRUCTURE; DURABILITY; METAKAOLIN; MORPHOLOGY; MORTAR; WATER;
D O I
10.1016/j.jobe.2024.111427
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Halloysite is an affordable natural mineral clay with a nanotubular structure and surface reactivity, giving it strong industrialization potential. This study investigated how the calcination temperature (0 degrees C-850 degrees C) affected the properties of halloysite and geopolymers derived from calcined halloysite, then as a modified material, the performances of a slag/fly-ash geopolymer with halloysite calcined at different temperatures were compared. Finally, the effects of halloysite curing temperature (20 degrees C-80 degrees C) and mass content (0.25%-1.5 %) on the mechanical properties and microstructure of the slag/fly-ash geopolymer were studied. The results show that the calcination temperature of 750 degrees C was optimal for stimulating the halloysite's activity, leading to the highest compressive strength of 42.7 MPa of the halloysite-based geopolymer. Uncalcined halloysite was the most suitable reinforcement for slag/fly-ash geopolymer because it retains relatively intact tubular structure, and its chemical bonding at the interface with geopolymers ensured good reinforcing properties. The bridging effect derived from tubular structure of halloysite led to a more noticeable enhancement of flexural strength. To prevent agglomeration from too much tubular halloysite, 1.0 % content was found to be optimal. The compressive and flexural strengths reached 62.5 MPa and 3.83 MPa, respectively, which were 9.84 % and 35.8 % higher than that without halloysite. Furthermore, with increasing curing temperature, the strength of the halloysite-modified geopolymer reached its peak at 60 degrees C. For 1.0 % halloysite modified geopolymer, the compressive strength was 87.0 MPa and the flexural strength was 4.56 MPa, respectively, which were 39.2 % and 19.1 % higher than that at the curing temperature of 20 degrees C.
引用
收藏
页数:15
相关论文
共 50 条
  • [21] Effects of relative humidity on the properties of fly ash-based geopolymers
    Oderji, Sajjad Yousefi
    Chen, Bing
    Jaffar, Syed Taseer Abbas
    CONSTRUCTION AND BUILDING MATERIALS, 2017, 153 : 268 - 273
  • [22] Understanding the generation and evolution of hydrophobicity of silane modified fly ash/slag based geopolymers
    She, Yuanshan
    Chen, Yuxuan
    Li, Linjun
    Xue, Longjian
    Yu, Qingliang
    CEMENT & CONCRETE COMPOSITES, 2023, 142
  • [23] Understanding the impact of synthesis parameters on the pore structure properties of fly ash-based geopolymers
    Xu, Wenrui
    Tang, Zhuo
    Xie, Youjun
    Long, Guangcheng
    Kai, Mingfeng
    Zhang, Zhaorui
    Bu, Mengxin
    Zaland, Saifurahman
    CONSTRUCTION AND BUILDING MATERIALS, 2024, 411
  • [24] Dielectric properties for characterization of fly ash-based geopolymer binders
    Malkawi, Ahmad B.
    Al-Mattarneh, Hashem
    Achara, Bitrus Emmanuel
    Mohammed, Bashar S.
    Nuruddin, Muhd Fadhil
    CONSTRUCTION AND BUILDING MATERIALS, 2018, 189 : 19 - 32
  • [25] Efflorescence and subflorescence induced microstructural and mechanical evolution in fly ash-based geopolymers
    Zhang, Zuhua
    Provis, John L.
    Ma, Xue
    Reid, Andrew
    Wang, Hao
    CEMENT & CONCRETE COMPOSITES, 2018, 92 : 165 - 177
  • [26] The influence of Pb addition on the properties of fly ash-based geopolymers
    Nikolic, Violeta
    Komljenovic, Miroslav
    Dzunuzovic, Natasa
    Miladinovic, Zoran
    JOURNAL OF HAZARDOUS MATERIALS, 2018, 350 : 98 - 107
  • [27] The effect of activators on the fly ash-based geopolymers
    Hou Yunfen
    Wang Dongmin
    ECOLOGICAL ENVIRONMENT AND TECHNOLOGY OF CONCRETE, 2011, 477 : 85 - +
  • [28] Influence of slag on mechanical and durability properties of fly ash-based geopolymer concrete
    Bellum, Ramamohana Reddy
    Muniraj, Karthikeyan
    Madduru, Rama Chand
    JOURNAL OF THE KOREAN CERAMIC SOCIETY, 2020, 57 (05) : 530 - 545
  • [29] Influence of slag on mechanical and durability properties of fly ash-based geopolymer concrete
    Ramamohana Reddy Bellum
    Karthikeyan Muniraj
    Sri Rama Chand Madduru
    Journal of the Korean Ceramic Society, 2020, 57 : 530 - 545
  • [30] High-Temperature Performance of Low-Calcium Fly Ash-Based Geopolymers
    Hanumananaik, Mude
    Reddy, Mittapalli Sanath Kumar
    Subramaniam, Kolluru V. L.
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2022, 34 (05)