High temperature tensile behaviors of extruded and rolled AZ31 Mg alloy

被引:6
作者
Qiao J. [1 ]
Wang Y. [1 ]
Shi G.-D. [1 ]
机构
[1] College of Materials Science and Engineering, University of Science and Technology Liaoning
来源
Transactions of Nonferrous Metals Society of China (English Edition) | 2010年 / 20卷 / SUPPL. 2期
基金
中国国家自然科学基金;
关键词
AZ31 Mg alloy; solute-drag creep; stress exponent; superplasticity; tensile ductility;
D O I
10.1016/S1003-6326(10)60534-1
中图分类号
学科分类号
摘要
High temperature tensile ductilities and deformation mechanisms of an extruded and rolled AZ31 Mg alloy were investigated. Elongation-to-failure tests were conducted under constant T-head velocity and constant temperatures ranging from 300 °C to 450 °C. Strain-rate-change tests were conducted under varying strain rate from 5×10-5 s-1 to 2×10-2 s-1 and constant temperature from 300 °C to 450 °C. Experimental results show that the maximum elongation of the AZ31 alloy with an average grain size of about 19 μm is 117% at strain rate of 10-3 s-1 and temperature of 450 °C. Stress exponent and activation energy were characterized to clarify the deformation mechanisms. The enhanced ductility is dominated by solute drag dislocation creep, and the major failure mechanism is cavity growth and interlinkage. © 2010 The Nonferrous Metals Society of China.
引用
收藏
页码:s540 / s544
页数:4
相关论文
共 16 条
[1]  
K Y.U., Rui S.T., Song J.M., X L.I.W., Guo L., Effects of grain refinement on mechanical properties and microstructures of AZ31 alloy [J], Transaction of Nonferrous Metals Society China, 18, Z1, pp. 39-43, (2008)
[2]  
Mukherjee A.K., An examination of the constitutive equation for elevated temperature plasticity [J], Materials Science and Engineering A, 322, 1-2, pp. 1-22, (2002)
[3]  
Ito T., Saeki J., Otsuka M., Superplastic-like behavior in coarse grained Mg-Al solid solutions [J], J Japan Inst Metals, 67, 2, pp. 85-92, (2003)
[4]  
Zhang Y.-shu, Zeng Z.-peng, Jin Q.-lin, Hot forming behavior and microstructure evolution of magnesium alloy AZ31D [J], Metal Heat Proceessing, 32, 7, pp. 22-26, (2007)
[5]  
Valle J.A.D., Ruano O.A., Separate contributions of texture and grain size on the creep mechanisms in a fine-grained magnesium alloy [J], Acta Materialia, 55, 2, pp. 455-466, (2007)
[6]  
Cao J., Zhang F.-quan, Xia W.-jun, D.-Fa F.U., Chen Z.-hua, Y.-Wu W.U., Superplasticity in a rolled AZ31 magnesium alloy by multi-stage deformation [J], Light Metal, 2, pp. 58-61, (2005)
[7]  
Del V.J., Perez-Prado M.T., Ruano O.A., Deformation mechanisms responsible for the high ductility in a Mg AZ31 alloy analyzed by electron backscattered diffraction [J], Metallurgical and Materials Transactions A, 36, 6, pp. 1427-1438, (2005)
[8]  
Zhang S.-chang, Zhu M., Zhao G., Chen C.-jun, Effect of zinc content on high temperature creep property of AZ31 magnesium alloy [J], The Chinese Journal of Nonferrous Metals, 18, 7, pp. 1205-1210, (2008)
[9]  
Somekawa H., Hirai K., Watanabe H., Takigawa Y., Higashi K., Dislocation creep behavior in Mg-Al-Zn alloys [J], Materials Science and Engineering A, 407, 1-2, pp. 53-61, (2005)
[10]  
Watanabe H., Tsutsui H., Mukai T., Kohzu M., Tanabe S., Higashi K., Deformation mechanism in a coarse-grained Mg-Al-Zn alloy at elevated temperatures [J], International Journal of Plasticity, 17, 3, pp. 387-397, (2001)