Comparative analysis of thermally evaporated nanoscale CdS thin film's structural, morphological, optical and nanomechanical properties

被引:1
|
作者
Gaur, Shailendra Kumar [1 ,2 ]
Chaudhary, Ashwani [3 ]
Murtaza, Qasim [1 ]
Mishra, R. S. [1 ]
机构
[1] Delhi Technol Univ, Dept Mech Engn, Main Bawana Rd, Delhi 110042, India
[2] Solid State Phys Lab, Delhi 110054, India
[3] Indian Inst Technol, Dept Mat Sci & Engn, Delhi 110016, India
关键词
CdS thin film; crystal structure; morphology; transmittance; band gap; nanoindentation; GRAIN-SIZE; MECHANICAL-PROPERTIES; ELECTRICAL-PROPERTIES; ELASTIC-MODULUS; NANOINDENTATION; DEFORMATION; CREEP; DEPENDENCE; BEHAVIOR; HARDNESS;
D O I
10.1016/j.molstruc.2024.140850
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
CdS nanoscale thin films were deposited on glass substrates at 1, 5 and 10 & Aring;/s deposition rates by thermal evaporation process. The structural, morphological, compositional, optical and nanomechanical properties of CdS thin films were analyzed by X-ray diffraction (XRD), atomic force microscopy (AFM), scanning electron microscopy (SEM), energy dispersive x-ray (EDX), UV-vis spectrophotometer and nanoindentation. XRD diffractogram indicate that the deposited CdS thin films have hexagonal structure with preferred orientation towards (002) plane and nearly stoichiometric composition. Various crystal structure parameters like lattice constant, crystallite size, defect density, dislocation density, lattice strain, number of crystallite per unit surface, stacking fault were determined. From XRD results, the calculated crystal structure parameters such as the crystallite size, microstrain and defect density were in the range of 20.4-14.7 nm, 7.74-10.62 and 2.3-4.52 x 1011 lines/cm2, at 1, 5and 10 & Aring;/s deposition rates, respectively .The AFM images indicated that the film's rms surface roughnesses were 2.73 nm, 2.94 nm and 3.18 nm at 1, 5and 10 & Aring;/s, respectively. The SEM images indicated that the films were uniform, continuous and defect free. The EDX examination revealed that at 1 & Aring;/s deposition rate the film was nearly stoichiometic. The optical band gaps were determined to be in the range of 2.37-2.43 eV. Nanoindentation tests evaluated the hardness, Young's modulus, creep behavior and strain rate of CdS films. Hardness evaluated to be 0.14-1.48 GPa, 0.15-2.46 GPa, and 0.21-2.55 GPa at 1,5 and 10 & Aring;/s deposition rate, respectively for 20-50 mu N load. The Young's modulus decreases 1-5 & Aring;/s deposition rate and becomes almost constant 5-10 & Aring;/s deposition rate at 70 mu N load. The characterization of CdS thin film recommend it as a favorable window layer in applications like photovoltaic, optoelectronic, thermoelectric and solar cells.
引用
收藏
页数:13
相关论文
共 50 条
  • [1] Nanomechanical characterization of thermally evaporated Cr thin films - FE analysis of the substrate effect
    Kataria, S.
    Goyal, Sunil
    Dash, S.
    Tyagi, A. K.
    THIN SOLID FILMS, 2010, 519 (01) : 312 - 318
  • [2] Effect of substrates temperature on structural and optical properties of thermally evaporated CdS nanocrystalline thin films
    Arif, Mohd
    Siddhartha
    Khan, Ziaul Raza
    Gupta, Vinay
    Singh, Arun
    INDIAN JOURNAL OF PURE & APPLIED PHYSICS, 2014, 52 (10) : 699 - 703
  • [3] Analysis of structural, morphological and nano-mechanical properties of vacuum evaporated nanoscale CdTe and ZnS films
    Gaur, Shailendra Kumar
    Murtaza, Qasim
    Mishra, R. S.
    OPTICAL MATERIALS, 2024, 154
  • [4] Structural, optical and nanomechanical properties of (111) oriented nanocrystalline ZnTe thin films
    Kiran, M. S. R. N.
    Kshirsagar, S.
    Krishna, M. G.
    Tewari, Surya P.
    EUROPEAN PHYSICAL JOURNAL-APPLIED PHYSICS, 2010, 51 (01)
  • [5] Optical and electrical properties of thermally evaporated Se90Sb10 thin film
    Abd-Elrahman, M., I
    Abu-Sehly, A. A.
    El-Sonbaty, Sherouk Sh
    Hafiz, M. M.
    MATERIALS SCIENCE AND ENGINEERING B-ADVANCED FUNCTIONAL SOLID-STATE MATERIALS, 2018, 232 : 8 - 14
  • [6] Effect of pH on the structural, optical and nanomechanical properties of CdS thin films grown by chemical bath deposition
    Yucel, Ersin
    Sahin, Osman
    CERAMICS INTERNATIONAL, 2016, 42 (05) : 6399 - 6407
  • [7] Effect of air annealing on structural, optical, morphological and electrical properties of thermally evaporated CdSe thin films
    Purohit, A.
    Chander, S.
    Nehra, S. P.
    Dhaka, M. S.
    PHYSICA E-LOW-DIMENSIONAL SYSTEMS & NANOSTRUCTURES, 2015, 69 : 342 - 348
  • [8] Correlation between the structural, morphological, optical, nanomechanical, and tribological properties of ZnO films by USPT with their photocatalytic activities
    Gonullu, Meryem Polat
    Cinici, Hanifi
    Cetinkaya, Cemil
    Tekeli, Suleyman
    Bostan, Bulent
    Cakil, Damla Dilara
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1010
  • [9] OPTICAL AND MORPHOLOGICAL INVESTIGATIONS OF THERMALLY VACUUM EVAPORATED ZnTe THIN FILMS
    Toma, O.
    Antohe, S.
    CHALCOGENIDE LETTERS, 2014, 11 (11): : 611 - 618
  • [10] Structural and optical properties of thermally evaporated BiSb2S3 thin films
    Kandaswamy, K.
    Selvin, P. Christopher
    Nalini, B.
    Abdulla, I. Mohamed
    Abhilash, K. P.
    ADVANCES IN NANOSCIENCE AND NANOTECHNOLOGY, 2013, 678 : 123 - +