Effect of Aging Time on Stress Corrosion Cracking of Super Duplex Stainless Steel UNS S32750

被引:0
|
作者
de Jesus, Ihana Gabriela Conceicao [1 ]
Santos, Iris Sterfanie [1 ]
Nascimento, Brenno Lima [1 ]
Monteiro, Michael Douglas Santos [2 ,3 ]
Sussuchi, Eliana Midori [2 ,3 ]
Griza, Sandro [1 ]
机构
[1] Univ Fed Sergipe, Postgrad Program Mat Sci & Engn, Sao Cristovao, SE, Brazil
[2] Univ Fed Sergipe, Postgrad Program Chem, Sao Cristovao, SE, Brazil
[3] Univ Fed Sergipe, Corros & Nanotechnol Lab, NUPEG, Sao Cristovao, SE, Brazil
关键词
Super-duplex stainless steel; Thermal aging; Stress corrosion cracking; 475; DEGREES-C; PITTING CORROSION; EMBRITTLEMENT; DECOMPOSITION; BEHAVIOR; ALLOY; PHASE;
D O I
10.1007/s11668-024-02070-x
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Super duplex stainless steels are dual-phase alloys containing ferrite and austenite, whose microstructure, corrosion behavior, and mechanical properties are influenced by aging heat treatment. While aging could enhance the mechanical strength of the alloy, the deleterious phases formed can reduce the stress corrosion cracking and general corrosion resistances of the steel if the aging temperature or time are unsuitably chosen. The present study evaluates the isothermal aging effect on the microhardness, electrochemical corrosion, and stress corrosion cracking behavior of the superduplex UNS S32750 alloy. The alloy samples were heat treated at 500 degrees C for 2, 4, 8, 24, 48, and 100 h and water cooled. Stress corrosion cracking test were carried out under seawater with partial pressure of CO2 equal 1 MPa, at 60 degrees C for 3 months. The corrosion potential and pitting potential were assessed by electrochemical tests. The results showed the gradual increase in the ferrite phase microhardness as the aging time increased. Aging at 48 and 100 h promoted susceptibility to stress corrosion cracking, evidenced by the increase amount of pitting on the stressed surface and microcracks emerging from the pitting. Furthermore, as the aging time increased, the pitting potential decreased.
引用
收藏
页码:2821 / 2830
页数:10
相关论文
共 50 条
  • [41] Altered microstructure characteristics and enhanced corrosion resistance of UNS S32750 duplex stainless steel via ultrasonic surface rolling process
    Zhang, Jiantao
    Zhu, Yuanzhi
    Xi, Xiaoying
    Xiao, Zhiyu
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2022, 309
  • [42] Wear and Corrosion of UNS S32750 Steel Subjected to Nitriding and Cathodic Cage Deposition
    Silva, Lauriene G. L.
    Naeem, M.
    Costa, Thercio H. C.
    Liborio, Maxwell S.
    Bandeira, Rafael M.
    Ferreira, Natalia S.
    Rossino, Luciana S.
    Junior, Cesar A. A.
    Queiroz, Jose C. A.
    Neto, Joao F. M.
    Sousa, Romulo R. M.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (20) : 9011 - 9018
  • [43] Temperature dependence of precipitation mechanism of intragranular χ phase in super duplex stainless steel S32750
    Wu Min
    Li Guoping
    Wang Lixin
    Hou Lifeng
    Wei Yinghui
    MATERIALS LETTERS, 2021, 287
  • [44] Heat Input Effect on Dissimilar Super Duplex Stainless Steel (UNS S32750) and Nitronic Steel (N 50) Gas Tungsten Arc Weld: Mechanism, Microstructure, and Mechanical Properties
    Maurya, Anup Kumar
    Chhibber, Rahul
    Pandey, Chandan
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (12) : 5283 - 5316
  • [45] Effect of machined surface integrity on the stress corrosion cracking behaviour of super duplex stainless steel
    Rajaguru, J.
    Arunachalam, N.
    ENGINEERING FAILURE ANALYSIS, 2021, 125
  • [46] Characterization of weld strength and toughness in the multi-pass welding of Inconel 625 and Super-duplex stainless steel UNS S32750
    Ramkumar, K. Devendranath
    Oza, Smitkumar
    Periwal, Saurabh
    Arivazhagan, N.
    Sridhar, R.
    Narayanan, S.
    CIENCIA & TECNOLOGIA DOS MATERIAIS, 2015, 27 (01): : 41 - 52
  • [47] Influence of the grain size on deleterious phase precipitation in superduplex stainless steel UNS S32750
    Pardal, J. M.
    Tauares, S. S. M.
    Fonseca, M. Cindra
    de Souza, J. A.
    Corte, R. R. A.
    de Abreu, H. F. G.
    MATERIALS CHARACTERIZATION, 2009, 60 (03) : 165 - 172
  • [48] Hydrogen influence on fracture toughness of the weld metal in super duplex stainless steel (UNS S32750) welded with two different heat input
    Lage, M. A.
    Assis, K. S.
    Mattos, O. R.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2015, 40 (47) : 17000 - 17008
  • [49] Effect of Post-Weld Heat Treatment on the Corrosion Behavior of Resistance Spot Welded Super Duplex Stainless UNS S 32750
    Shin, Byung-hyun
    Park, Sanghyup
    Park, Junghyun
    Kim, Dohyung
    Hwang, Myoungwon
    Chung, Wonsub
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2019, 14 (03): : 2430 - 2441
  • [50] Evaluation of aged duplex stainless steel UNS S32750 susceptibility to intergranular corrosion by optimized double loop electrochemical potentiokinetic reactivation method
    Hong, Jufeng
    Han, Dong
    Tan, Hua
    Li, Jin
    Jiang, Yiming