Comparative Performance of ATH and SiO2 Doped Silicone Rubber Microcomposites Exposed to Mineral Oil

被引:0
|
作者
Mishra, Palash [1 ]
Sarathi, R. [2 ]
Phung, Toan [3 ]
Mondal, Mithun [4 ]
Paul, Moutusi [1 ]
Vangapandu, Dhanunjaya Naidu [1 ]
机构
[1] Natl Inst Technol Warangal, Dept Elect Engn, Hanumakonda 506004, Telangana, India
[2] Indian Inst Technol, Dept Elect Engn, Chennai 600036, Tamil Nadu, India
[3] Univ New South Wales, Sch Elect Engn & Telecommun, Sydney, NSW 2052, Australia
[4] Birla Inst Technol & Sci Pilani, Dept Elect & Elect Engn, Hyderabad Campus, Hyderabad 500078, Telangana, India
关键词
Aging; bushings; inclined plane tracking and erosion test (IPT-E); microcomposites; mineral oil; silicone rubber (SR) coatings; EROSION RESISTANCE; SURFACE-CHARGE; FILLERS; SUPPRESSION; DEGRADATION; COMPOSITES; TRACKING;
D O I
10.1109/TDEI.2024.3355356
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Alumina-tri-hydrate (ATH) and Silica (SiO2) microfillers are widely used to enhance the pollution performance of room temperature vulcanized (RTV) silicone rubber (SR) coatings which are now increasingly being used in porcelain-based bushings of oil-immersed transformers to enhance their operational safety. However, exposure of SR to transformer oil is detrimental and is underexplored. Therefore, the current work involves experimental investigations on relative electrical, thermal, and mechanical performances of undoped and 50% by weight of ATH and SiO2 doped SR microcomposites thermally aged in transformer mineral oil at 80 degrees C for 200 h. Test specimens incurred significant physical changes such as swelling and weight gain post aging. The presence of black patches, voids, and dents on the specimen indicating morphological deterioration, along with an increase in surface roughness and decrease in hardness was noted through scanning electron microscopy (SEM), 3-D microscopy, and shore hardness investigations. Tracking and erosion resistance of the test specimens evaluated as per IEC 60587 inclined plane tracking and erosion test (IPT-E) demonstrated that neither of the micro fillers could prevent tracking and erosion in aged specimens. IPT-E results were supported by surface potential decay measurements, confirming that ATH-doped SR microcomposites exhibited the maximum tracking and erosion resistance. Thermal properties of the test specimens, investigated via thermogravimetric and differential thermal analysis (DTA), revealed higher thermal stability of ATH-doped specimens compared to mSiO(2)-doped and unfilled specimens. In conclusion, post-aging in mineral oil, micro-ATH-doped RTV SR outperformed the SiO2-doped and undoped specimens, making it more suitable for transformer bushing applications.
引用
收藏
页码:3150 / 3158
页数:9
相关论文
共 50 条
  • [21] Electrified Droplet on Corona-charged Surface of Silicone Rubber/SiO2 Nanocomposite
    Du, B. X.
    Li, Jie
    IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2012, 19 (06) : 2073 - 2080
  • [22] Effects of Platinum Catalyst on the Dielectric Properties of Addition Cure Silicone Rubber/SiO2 Nanocomposites
    Xu, Chi
    Yan, Nianping
    Yang, Chanjian
    Wang, Xilin
    Jia, Zhidong
    IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2021, 28 (01) : 142 - 149
  • [23] Surface Charge Decay of Direct-fluorinated RTV Silicone Rubber/SiO2 Nanocomposites
    Li, Zhonglei
    Du, B. X.
    Xu, Hang
    Du, Huanhuan
    Gao, Yu
    PROCEEDINGS OF 2014 INTERNATIONAL SYMPOSIUM ON ELECTRICAL INSULATING MATERIALS (ISEIM 2014), 2014, : 477 - 480
  • [24] Tracking and Erosion Resistance Performance Investigation on Nano-sized SiO2 Filled Silicone Rubber for Outdoor Insulation Applications
    Loganathan, N.
    Muniraj, C.
    Chandrasekar, S.
    IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2014, 21 (05) : 2172 - 2180
  • [25] Performance Evaluation of Thermally-Aged RTV Silicone Rubber/TiO2 Nanocomposites in Mineral Oil for Transformer Bushings
    Vangapandu, Dhanunjaya Naidu
    Paul, Moutusi
    Mishra, Palash
    Sarathi, R.
    Paramane, Ashish
    Nazir, M. Tariq
    IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2023, 30 (04) : 1493 - 1501
  • [26] AC Breakdown Voltage and Viscosity of Mineral Oil based SiO2 Nanofluids
    Jin, H.
    Andritsch, T.
    Morshuis, P. H. F.
    Smit, J. J.
    2012 ANNUAL REPORT CONFERENCE ON ELECTRICAL INSULATION AND DIELECTRIC PHENOMENA (CEIDP), 2012, : 902 - 905
  • [27] Performance evaluation of thermally aged ATH and BN co-doped silicone rubber nano-micro composites for power cable applications
    Vangapandu, Dhanunjaya Naidu
    Paul, Moutusi
    Mishra, Palash
    Sarathi, Ramanujam
    Kornhuber, Stefan
    Thapliyal, Shivraman
    POLYMER ENGINEERING AND SCIENCE, 2022, 62 (11): : 3868 - 3879
  • [28] Coupling effects of gamma irradiation and moisture on the properties of SiO2 and TiO2 filled silicone rubber
    Qin, Zi-Ming
    Wang, Pu-Cheng
    Chen, Hong-Bing
    RADIATION PHYSICS AND CHEMISTRY, 2022, 197
  • [29] Fabrication of SiO2 microlenses on silicone rubber using a vacuum-ultraviolet F2 laser
    Takao, H
    Okoshi, M
    Miyagami, H
    Inoue, N
    IEEE JOURNAL OF SELECTED TOPICS IN QUANTUM ELECTRONICS, 2004, 10 (06) : 1426 - 1429
  • [30] Thermal distribution analysis and suppression mechanism of carbonized tracking and erosion in silicone rubber/SiO2 nanocomposites
    Nazir, M. Tariq
    Phung, B. T.
    Yu, Shihu
    Li, Shengtao
    Xie, Dongri
    Zhang, Yuanyuan