Corrosion susceptibility and allergy potential of austenitic stainless steels

被引:0
作者
Reclaru L. [1 ]
Ardelean L.C. [2 ]
机构
[1] Scientific Independent Consultant Biomaterials and Medical Devices, 103 Paul-Vouga, Marin-Neuchâtel
[2] Department of Technology of Materials and Devices in Dental Medicine, 'Victor Babes' University of Medicine and Pharmacy Timisoara, 2 Eftimie Murgu sq, Timisoara
来源
Ardelean, Lavinia Cosmina (lavinia_ardelean@umft.ro) | 1600年 / MDPI AG卷 / 13期
关键词
Austenitic steels; Contact with skin; Crevice corrosion; Galvanic couplings; General (uniform) corrosion; Intergranular corrosion; Medical devices; Nickel release; Pitting corrosion; Watchmaking;
D O I
10.3390/MA13184187
中图分类号
学科分类号
摘要
Although called stainless steels, austenitic steels are sensitive to localized corrosion, namely pitting, crevice, and intergranular form. Seventeen grades of steel were tested for localized corrosion. Steels were also tested in general corrosion and in galvanic couplings (steels-precious alloys) used in watchmaking applications. The evaluations have been carried out in accordance with the ASTM standards which specifically concern the forms of corrosion namely, general (B117-97, salt fog test), pitting (G48-11, FeCl3), crevice (F746-87) and intergranular (A262-15, Strauss chemical test and G108-94, Electrochemical potentiodynamic reactivation test). All tests revealed sensitivity to corrosion. We have noticed that the transverse face is clearly more sensitive than the longitudinal face, in the direction of rolling process. The same conclusion has been drawn from the tests of nickel release. It should be pointed out that, despite the fact that the grade of steel is in conformity with the classification standards, the behavior is very different from one manufacturer to another, due to parameters dependent on the production process, such as casting volume, alloying additions, and deoxidizing agents. The quantities of nickel released are related to the operations involved in the manufacturing process. Heat treatments reduce the quantities of nickel released. The surface state has little influence on the release. The hardening procedures increase the quantities of nickel released. The quantities of released nickel are influenced by the inclusionary state and the existence of the secondary phases in the steel structure. Another aspect is related to the strong dispersion of results concerning nickel release and corrosion behavior of raw materials. © 2020 by the authors.
引用
收藏
相关论文
共 50 条
[31]   Effect of biofilm in the corrosion of austenitic stainless steels in wastewater treatment plants [J].
Bethencourt, M. ;
Garcia de Lomas, J. ;
Corzo, A. ;
Villahermosa, D. ;
Matres, V. .
REVISTA DE METALURGIA, 2010, 46 (01) :37-51
[32]   Pitting corrosion behaviour of austenitic stainless steels with Cu and Sn additions [J].
Pardo, A. ;
Merino, M. C. ;
Carboneras, M. ;
Coy, A. E. ;
Arrabal, R. .
CORROSION SCIENCE, 2007, 49 (02) :510-525
[33]   Localized Corrosion Resistance Of Welded Austenitic And Lean Duplex Stainless Steels [J].
Mikael Magnus Johansson ;
Elin Marianne Westin ;
James Oliver ;
Rachel F. A. Pettersson .
Welding in the World, 2011, 55 :19-27
[34]   Pitting Corrosion Resistance of Mn-Alloyed Austenitic Stainless Steels [J].
Pulkkinen, Heikki ;
Apajalahti, Helka ;
Papula, Suvi ;
Talonen, Juho ;
Hanninen, Hannu .
STEEL RESEARCH INTERNATIONAL, 2014, 85 (03) :324-335
[35]   Fundamentals for better use of stainless steels - Development history, characteristics and resistance to corrosion - IV: Corrosion tests for stainless steels [J].
Miyuki H. .
Zairyo/Journal of the Society of Materials Science, Japan, 2011, 60 (10) :950-956
[36]   Pitting corrosion studies on nitrogen-bearing austenitic stainless steels [J].
Mudali, UK ;
Dayal, RK ;
Gnanamoorthy, JB ;
Rodriguez, P .
MATERIALS TRANSACTIONS JIM, 1996, 37 (10) :1568-1573
[37]   Effect of laser surface melting on intergranular corrosion behaviour of aged austenitic and duplex stainless steels [J].
Kwok, C. T. ;
Lo, K. H. ;
Chan, W. K. ;
Cheng, F. T. ;
Man, H. C. .
CORROSION SCIENCE, 2011, 53 (04) :1581-1591
[38]   Swelling of austenitic stainless steels [J].
Dubuisson, P. .
REVUE DE METALLURGIE-CAHIERS D INFORMATIONS TECHNIQUES, 2011, 108 (01) :33-37
[39]   Intergranular corrosion of non-sensitized austenitic stainless steels in nitric acid [J].
Gwinner, B. ;
Auroy, M. ;
Bague, V. ;
Chaachoua, S. ;
Fieulaine, B. ;
Tran, Q. T. ;
Tricoit, S. .
REVUE DE METALLURGIE-CAHIERS D INFORMATIONS TECHNIQUES, 2010, 107 (10-11) :441-443
[40]   On the pitting corrosion resistance of nitrogen alloyed cold worked austenitic stainless steels [J].
Mudali, UK ;
Shankar, P ;
Ningshen, S ;
Dayal, RK ;
Khatak, HS ;
Raj, B .
CORROSION SCIENCE, 2002, 44 (10) :2183-2198