Flow stress of die-cast AZ91D magnesium alloy under hot compression deformation

被引:0
|
作者
You, Guoqiang [1 ,2 ]
Zuo, Xudong [1 ]
Tan, Xia [1 ]
Wang, Xiangjie [1 ]
Long, Siyuan [1 ,2 ]
机构
[1] Chongqing University, Chongqing 400045, China
[2] National Engineering Research Center for Magnesium Alloys, Chongqing 400044, China
关键词
Magnesium alloys - Dies - Strain rate - Compression testing - Hyperbolic functions - Constitutive equations - Plastic flow;
D O I
暂无
中图分类号
学科分类号
摘要
Hot compression tests of die-cast AZ91D magnesium alloy were performed on Gleeblle-1500D at strain rates ranging in 0.01~10 s-1 and deformation temperatures ranging in 250~450°C. The constitutive equation, Ε=1.41×1012 [sinh(0.014σ)]5.295exp (-159 449.509/RT), which is described by Zener-Hollomom parameters for hot compression deformation of die-cast AZ91D magnesium alloy was established. Compared to gravity cast AZ91D magnesium alloy, the deformation activation energy of die-cast AZ91D magnesium alloy, Q=159.45 kJ·mol-1, determined by hyperbolic sine function is lower. Copyright © 2013 Northwest Institute for Nonferrous Metal Research. Published by Elsevier BV. All rights reserved.
引用
收藏
页码:1844 / 1848
相关论文
共 50 条
  • [1] Flow Stress of Die-Cast AZ91D Magnesium Alloy under Hot Compression Deformation
    You Guoqiang
    Zuo Xudong
    Tan Xia
    Wang Xiangjie
    Long Siyuan
    RARE METAL MATERIALS AND ENGINEERING, 2013, 42 (09) : 1844 - 1848
  • [2] Laser welding of die-cast AZ91D magnesium alloy
    Wahba, M.
    Mizutani, M.
    Kawahito, Y.
    Katayama, S.
    MATERIALS & DESIGN, 2012, 33 : 569 - 576
  • [3] Microstructure and cyclic deformation behaviour of the magnesium die-cast alloy AZ91D hp
    Ebel-Wolf, B
    Walther, F
    Eifler, D
    MATERIALPRUFUNG, 2005, 47 (7-8): : 462 - 467
  • [4] Fatigue crack propagation in die-cast AZ91D magnesium alloy
    Shibusawa, T
    Kobayashi, Y
    Ishikawa, K
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1997, 61 (04) : 298 - 302
  • [5] Fatigue crack propagation in die-cast AZ91D magnesium alloy
    Toyo Univ, Saitama, Japan
    Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals, 1997, 61 (04): : 298 - 302
  • [6] Barium phosphate conversion coating on die-cast AZ91D magnesium alloy
    Liu Feng
    Shan Da-yong
    Han En-hou
    Liu Chang-sheng
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2008, 18 : S344 - S348
  • [7] Processing Technology and Mechanical Properties of Die-Cast Magnesium Alloy AZ91D
    刘艳改
    刘文辉
    熊守美
    柳百成
    王罡
    MATSUMOTO Yoshihide
    MURAKAMI Masayuki
    TsinghuaScienceandTechnology, 2004, (05) : 612 - 616
  • [8] Barium phosphate conversion coating on die-cast AZ91D magnesium alloy
    刘锋
    单大勇
    韩恩厚
    刘常升
    Transactions of Nonferrous Metals Society of China, 2008, 18(S1) (S1) : 344 - 348
  • [9] Processing technology and mechanical properties of die-cast magnesium alloy AZ91D
    Liu, Yan'gai
    Liu, Wenhui
    Xiong, Shoumei
    Liu, Baicheng
    Wang, Gang
    Matsumoto, Yoshihide
    Murakami, Masayuki
    Tsinghua Science and Technology, 2004, 9 (05) : 612 - 616
  • [10] Fatigue crack growth behaviour of a die-cast magnesium alloy AZ91D
    Venkateswaran, P
    Raman, SGS
    Pathak, SD
    Miyashita, Y
    Mutoh, Y
    MATERIALS LETTERS, 2004, 58 (20) : 2525 - 2529