One-step fabrication of wear resistant and friction-reducing Al2O3/MoS2 nanocomposite coatings on 2A50 aluminum alloy by plasma electrolytic oxidation with MoS2 nanoparticle additive

被引:1
|
作者
Zhang, Min [1 ]
Ma, Xining [1 ,2 ]
Zhang, Siyang [1 ]
Hou, Liyan [1 ]
Kim, Kwang Ho [2 ]
机构
[1] Liaoning Normal Univ, Sch Phys & Elect Technol, Dalian 116029, Peoples R China
[2] Pusan Natl Univ, Sch Mat Sci & Engn, Busan 609735, South Korea
基金
中国国家自然科学基金;
关键词
Plasma electrolytic oxidation; Molybdenum disulfide; Wear resistance; Nanocomposite coating; MECHANICAL-PROPERTIES; CORROSION BEHAVIOR; CERAMIC COATINGS; PEO COATINGS; MICROSTRUCTURE; COMPOSITES; PROPERTY;
D O I
10.1016/j.surfcoat.2025.131796
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Wear resistant and friction-reducing Al2O3/MoS2 nanocomposite coatings were fabricated in-situ on 2A50 aluminum alloy substrate using one-step plasma electrolytic oxidation in silicate electrolyte solution with MoS2 nanoparticle addition. The effect of MoS2 incorporation on microstructure and wear resistance of the obtained ceramic coatings was investigated by regulating the concentration of MoS2 nanoparticle. Phase structure, microstructure, composition and wear resistance of the ceramic coatings were characterized by XRD, SEM, EDS, profilometer and ball-on-disc friction and wear tester. The results show that the anodic voltage of micro-arc discharge stage increased with the increasing of MoS2 concentration and the prepared ceramic coatings were mainly composed of alpha-Al2O3, gamma-Al2O3, MoS2, and mullite phases. The EDS mapping results show Mo and S elements were evenly distributed in the ceramic coatings indicating the formation of Al2O3/MoS2 nanocomposite coatings. Friction performance evaluation shows that the ceramic coatings obtained at the MoS2 nanoparticle concentration of 4 g/L exhibit the best wear resistance and antifriction property. During the friction and wear test, the protective lubricant film formed between ceramic layer and grinding parts is the largest and the average friction coefficient is the lowest, as low as 0.1. The wear rate was the lowest (about 5.28 x 10-4 cm3 center dot N-1 center dot m- 1). It can be concluded that MoS2 can play a good antifriction and lubrication effect in ceramic layer, optimize the microstructure of ceramic layer, and improve the wear resistance of ceramic layer.
引用
收藏
页数:9
相关论文
共 50 条
  • [21] Microstructure and mechanical properties of A356/Al2O3/MoS2 hybrid nanocomposites
    Kumar, K. Ajay
    Mallikarjuna, C.
    MATERIALS TODAY-PROCEEDINGS, 2022, 54 : 415 - 420
  • [22] Effect of Al 2 O 3 nanoparticles additions on wear resistance of plasma electrolytic oxidation coatings on TC4 alloys
    Shi, Lei
    Jiang, Chaoping
    Zhao, Ruoyi
    Si, Tongkang
    Li, Yao
    Qian, Weifeng
    Gao, Guangrui
    Chen, Yongnan
    CERAMICS INTERNATIONAL, 2024, 50 (11) : 18484 - 18496
  • [23] Photocatalytic activity of Al2O3:Eu2+and Al2O3:Ce3+coatings formed by plasma electrolytic oxidation of aluminum
    Stojadinovic, Stevan
    Radic, Nenad
    JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 2025, 203
  • [24] Sliding wear of spark plasma sintered CrFeCoNiCu high entropy alloy coatings with MoS2 and WC additions
    Ji, Xiulin
    Zhao, Jianhua
    Wang, Hui
    Luo, Chanyuan
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2018, 96 (5-8) : 1685 - 1691
  • [25] Promotion of highly loaded MoS2/Al2O3 hydrodesulfurization catalysts prepared in aqueous solution
    Bezverkhyy, I
    Afanasiev, P
    Lacroix, M
    JOURNAL OF CATALYSIS, 2005, 230 (01) : 133 - 139
  • [26] Evaluation on tribological design coatings of Al2O3, Ni-P-PTFE and MoS2 on aluminium alloy 7075 under oil lubrication
    Liew, K. W.
    Chia, S. Y.
    Kok, C. K.
    Low, K. O.
    MATERIALS & DESIGN, 2013, 48 : 77 - 84
  • [27] Highly active (CO)MoS2/Al2O3 hydrodesulfurization catalysts prepared in aqueous solution
    Bezverkhyy, I
    Afanasiev, P
    Geantet, C
    Lacroix, M
    JOURNAL OF CATALYSIS, 2001, 204 (02) : 495 - 497
  • [28] The formation of tungsten doped Al2O3/ZnO coatings on aluminum by plasma electrolytic oxidation and their application in photocatalysis
    Stojadinovic, Stevan
    Vasilic, Rastko
    Radic, Nenad
    Tadic, Nenad
    Stefanov, Plamen
    Grbic, Bosko
    APPLIED SURFACE SCIENCE, 2016, 377 : 37 - 43
  • [29] Eu2+ photoluminescence in Al2O3 coatings obtained by plasma electrolytic oxidation
    Stojadinovic, Stevan
    Vasilic, Rastko
    JOURNAL OF LUMINESCENCE, 2018, 199 : 240 - 244
  • [30] Improved wear and corrosion resistance of MoS2/MgO/MgAl2O4 composite layer in-situ prepared by one-step micro-arc oxidation
    Sun, Song
    Shang, Jian
    MATERIALS TODAY COMMUNICATIONS, 2024, 40