Tri-reforming of methane to syngas over Ni/Al2O3 - Thermal distribution in the catalyst bed

被引:40
作者
The Key Laboratory of Green Process and Engineering, Institute of Process Engineering, Chinese Academy of Sciences, Beijing, 100080, China [1 ]
不详 [2 ]
机构
[1] The Key Laboratory of Green Process and Engineering, Institute of Process Engineering, Chinese Academy of Sciences, Beijing
[2] Graduate School, the Chinese Academy of Sciences, Beijing
来源
Ranliao Huaxue Xuebao | 2007年 / 1卷 / 72-78期
基金
中国国家自然科学基金;
关键词
methane; Ni/Al[!sub]2[!/sub]O[!sub]3[!/sub] catalyst; thermal distributing; tri-reforming;
D O I
10.1016/S1872-5813(07)60012-7
中图分类号
学科分类号
摘要
Thermal distribution in catalyst bed was investigated for the fixed-bed tri-reforming of methane over Ni/Al2O3 under atmospheric pressure, 750 - 950°C, and space velocity (SV) of 2000 - 20000 h-1. The effects of the furnace temperature (tf), the space velocity, and the feed stock composition on the thermal distribution were examined. The results indicated that the temperature gradient of the catalyst bed in methane tri-reforming is smaller than that in methane partial oxidation. The temperature near the inlet of the catalyst bed (tmax) is 80°C higher than tf when the feed composition n(CH4)/n(CO2)/n(H2O)/n(O2) = 50/12.5/12.5/25 (by mol) and the space velocity SV = 20000 h-1, whereas the temperature near the outlet of the catalyst bed is close to tf. The temperature difference between the inlet and the furnace Δtmax = tmax - tf) increases with the space velocity Δtmax = 30°C at 2000 h-1, Δtmax = 80°C at 20000 h-1). No distinct hot spot is observed near the catalyst bed inlet when there is no oxygen in feed. Under specific condition, the lowest temperature in the catalyst bed (tmin) is about 30 - 40°C lower than tf. According to the thermal distribution, the catalyst bed can then be divided into three zones: oxygen adequate zone, oxygen inadequate zone, and oxygen absent zone. Methane reforming proceeds in the first and second zones, while methane combustion proceeds only in the first zone and partial oxidation of methane proceeds only in the second zone. © 2007 Institute of Coal Chemistry, Chinese Academy of Sciences.
引用
收藏
页码:72 / 78
页数:6
相关论文
共 17 条
[1]  
Song C., Tri-reforming: A new process for reducing CO<sub>2</sub> emissions, Chemical Innovation, 31, 1, pp. 21-26, (2001)
[2]  
Song C., Pan W., Tri-reforming of methane: A novel concept for catalytic production of industrially useful synthesis gas with desired H<sub>2</sub>/CO ratios, Catal Today, 98, 4, pp. 463-484, (2004)
[3]  
Lee S., Cho W., Ju W., Cho B., Lee Y., Baek Y., Tri-reforming of CH<sub>4</sub> using CO<sub>2</sub> for production of synthesis gas to dimethyl ether, Catal Today, 87, 1 -4, pp. 133-137, (2003)
[4]  
Tomishige K., Syngas production from methane reforming with CO<sub>2</sub>/H<sub>2</sub>O and O<sub>2</sub> over NiO-MgO solid solution catalyst in fluidized bed reactors, Catal Today, 89, 4, pp. 405-418, (2004)
[5]  
Xu D., Li W., Chen Y., Xu H., Study on the combined catalytic partial oxidation and CO<sub>2</sub>-H<sub>2</sub>O reforming of coal-bed methane to syngas, Journal of China Coal Society, 29, 4, pp. 468-471, (2004)
[6]  
Xu D., Li W., Ge Q., Xu H., Study on the conversion of drained coal-bed methane to syngas: The effect of solid solution formation on the performance of NiO/MgO catalyst, Journal of Fuel Chemistry and Technology, 32, 5, pp. 579-583, (2004)
[7]  
Heitnes K., Lingberg S., Rokstad O., Holmen A., Catalytic partial oxidation of methane to synthesis gas, Catal Today, 24, 3, pp. 211-216, (1995)
[8]  
Groote A., Froment G., Simulation of the catalytic partial oxidation of methane to synthesis gas, Appl Catal A, 138, 2, pp. 245-264, (1996)
[9]  
Sile F., Fornasari G., Trifiro F., Vaccari A., Partial oxidation of methane: Effect of reaction parameters and catalyst composition on the thermal profile and heat distribution, Catal Today, 64, 1 -2, pp. 21-30, (2001)
[10]  
Cai W., Li H., Zhang Y., Preparation of nanofibrous γ-Al<sub>2</sub>O<sub>3</sub> particles with large pore volume from H<sub>2</sub>O<sub>2</sub> and sodium aluminate solutions, Journal of Chemical Industry and Engineering (China), 1155, 12, pp. 1976-1981, (2004)