Regulation active components distribution of NiMo/Al2O3 catalysts for hydrodesulfurization

被引:0
作者
Wang, Jia [1 ]
Li, Wencui [1 ]
Wu, Fan [1 ]
Gao, Xinqian [1 ]
Lu, Anhui [1 ]
机构
[1] State Key Laboratory of Fine Chemicals, School of Chemical Engineering, Dalian University of Technology, Liaoning, Dalian
来源
Huagong Jinzhan/Chemical Industry and Engineering Progress | 2024年 / 43卷 / 08期
关键词
adsorption; alumina; eggshell catalyst; hydrodesulfurization; surface property;
D O I
10.16085/j.issn.1000-6613.2023-1131
中图分类号
学科分类号
摘要
Residue hydrogenation is a diffusion-limited reaction. When the active components are distributed in the outer region of pellet catalysts, namely eggshell distribution, the diffusion resistance of reactants in catalyst particles can be effectively reduced to achieve the best catalytic activity. The adsorption strength of active metals on alumina support was regulated by adjusting the surface properties. Multiple techniques, including X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), molybdenum equilibrium adsorption, and contact angle, were employed to determine the surface properties of the supports. It was found that the support with more basic hydroxyl group would have stronger adsorption on the active metals, slowing down the diffusion rate of the active components during impregnation. The distribution of active components could be adjusted through the regulation of adsorption and diffusion rates. Dibenzothiophene was chosen as a model compound for the evaluation of the desulfurization performance. The results showed that the eggshell catalyst exhibited an apparent desulfurization rate of 79.3%, with a specific activity 1.2 times higher than the uniform catalyst. It might be attributed to the weaker metal-support interactions on the eggshell catalyst, which facilitates a higher sulfurization degree and the formation of the Ni-Mo-S type Ⅱ active phase during the sulfurizing process. Moreover, eggshell catalyst could remarkably reduce the internal diffusion resistance owing to a short diffusion path of the reactants, thus greatly improving the utilization efficiency of the active components. © 2024 Chemical Industry Press Co., Ltd.. All rights reserved.
引用
收藏
页码:4393 / 4402
页数:9
相关论文
共 38 条
  • [1] LI Chunnian, Residue processing technology, (2002)
  • [2] ZHANG Chunguang, TAN Qingfeng, ZHANG Tianqi, Et al., Synthesis of residue-hydrotreating catalysts by hydrotalcite method, Chemical Industry and Engineering Progress, 37, 11, pp. 4303-4307, (2018)
  • [3] HAN Kunpeng, DAI Lishun, NIE Hong, Research progress on deactivation of fixed bed residue hydrogenating catalysts at the initial stage of operation, Chemical Industry and Engineering Progress, 36, S1, pp. 211-220, (2017)
  • [4] DIK P P, DANILOVA I G, GOLUBEV I S, Et al., Hydrocracking of vacuum gas oil over NiMo/zeolite-Al<sub>2</sub>O<sub>3</sub>: Influence of zeolite properties, Fuel, 237, pp. 178-190, (2019)
  • [5] CUI Qingyan, MA Xiaoliang, NAKANO Koji, Et al., Hydrotreating reactivities of atmospheric residues and correlation with their composition and properties, Energy & Fuels, 32, 6, pp. 6726-6736, (2018)
  • [6] ZHAO Rifeng, Progress and application of hydrocracking and residue hydrogenation technology, (2022)
  • [7] PENG Chong, ZENG Ronghui, WU Ziming, Et al., Development and application of high-efficiency hydrocracking catalyst stacking technology, Petroleum Refinery Engineering, 46, 3, pp. 49-51, (2016)
  • [8] SHAO Zhicai, SHENG Jian'an, DENG Zhonghuo, Et al., Development and application of high sulfur residue hydrotreating technology for producing low sulfur heavy marine fuel components, Petroleum Processing and Petrochemicals, 54, 4, pp. 24-28, (2023)
  • [9] ZHU Huihong, MAO Zhiwei, LIU Bin, Et al., Regulating catalyst morphology to boost the stability of Ni-Mo/Al<sub>2</sub>O<sub>3</sub> catalyst for ebullated-bed residue hydrotreating, Green Energy & Environment, 6, 2, pp. 283-290, (2021)
  • [10] CHEN W, NIE H, LONG X, Et al., Role of pore structure on the activity and stability of sulfide catalyst, Catalysis Today, 377, pp. 69-81, (2021)