Corrosion analysis of 316L and T91 steels exposed to liquid lead-bismuth eutectic using X-ray CT

被引:0
作者
Huang, Yuji [1 ]
Peng, Sirui [1 ]
Zhang, Zhihan [1 ]
Shi, Jiajian [1 ]
Yuan, Rui [1 ,4 ]
Zhou, Zhou [2 ]
Ji, Yuchun [3 ]
Lin, Jiming [4 ]
Chen, Yingxue [4 ]
Zhang, Feifei [4 ]
Meng, Fanqiang [1 ]
机构
[1] Sun Yat Sen Univ, Sino French Inst Nucl Engn & Technol, Zhuhai 519082, Peoples R China
[2] Sun Yat Sen Univ, Sch Phys, Guangzhou 510275, Peoples R China
[3] Guilin Univ Technol, Coll Mat Sci & Engn, Guilin 541006, Peoples R China
[4] China Nucl Power Technol Res Inst, Shenzhen 518026, Peoples R China
来源
MATERIALS TODAY COMMUNICATIONS | 2024年 / 41卷
基金
中国国家自然科学基金;
关键词
Liquid Lead-bismuth Eutectic; X-ray computed tomography; Dissolution corrosion; Oxidation corrosion; T91 Ferritic/Martensitic steel; 316L Austenitic steel; DISSOLUTION CORROSION; OXIDATION MECHANISM; FE-9CR-1MO STEEL; STAINLESS-STEELS; OXIDE SCALE; LBE; TOMOGRAPHY; OXYGEN; TEMPERATURES; CONCRETE;
D O I
10.1016/j.mtcomm.2024.110985
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Acquiring three-dimensional (3D) corrosion data is crucial for monitoring the corrosion behaviors of stainless steels within liquid metals. In the present study, 316 L and T91 steels subjected to liquid Lead-Bismuth Eutectic (LBE) corrosion were characterized using X-ray computed tomography (CT) for the first time. CT results show that LBE residing within the grain boundaries would consistently dissolves the surrounding ferrite structure of 316 L upon extended exposure to LBE. This sustained dissolution corrosion eventually results in the formation of grain-shaped pits on the surface. Moreover, the non-uniform dissolution corrosion pattern in T91 originates from the degradation of the local oxide film caused by the continuous LBE attacks. This process eventually leads to the formation of the dissolved corrosion pits with large dimensions. Additionally, the needle-shaped 316 L and T91 samples exhibit corrosion behaviors in LBE that are consistent with those observed in bulk samples.
引用
收藏
页数:10
相关论文
共 37 条
[1]   Three dimensional imaging of reinforcement corrosion using micro-computed tomography: Literature review [J].
Alhusain, Mustafa ;
Al-Mayah, Adil .
CONSTRUCTION AND BUILDING MATERIALS, 2021, 284
[2]   Early stages of dissolution corrosion in 316L and DIN 1.4970 austenitic stainless steels with and without anticorrosion coatings in static liquid lead-bismuth eutectic (LBE) at 500 °C [J].
Charalampopoulou, Evangelia ;
Lambrinou, Konstantina ;
Van der Donck, Tom ;
Paladino, Boris ;
Di Fonzo, Fabio ;
Azina, Clio ;
Eklund, Per ;
Mraz, Stanislav ;
Schneider, Jochen M. ;
Schryvers, Dominique ;
Delville, Remi .
MATERIALS CHARACTERIZATION, 2021, 178
[3]   Oxide scale formation on 316L and FeCrAl steels exposed to oxygen controlled static LBE at temperatures up to 800 °C [J].
Cionea, C. ;
Abad, M. D. ;
Aussat, Y. ;
Frazer, D. ;
Gubser, A. J. ;
Hosemann, P. .
SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2016, 144 :235-246
[4]   Monitoring reinforcement corrosion and corrosion-induced cracking by X-ray microcomputed tomography method [J].
Dong, Biqin ;
Fang, Guohao ;
Liu, Yuqing ;
Dong, Peng ;
Zhang, Jianchao ;
Xing, Feng ;
Hong, Shuxian .
CEMENT AND CONCRETE RESEARCH, 2017, 100 :311-321
[5]   Influence of oxide scale on the wettability of LBE on T91 steel [J].
Du, Xiaochao ;
Niu, Fenglei ;
Zhu, Huiping ;
Ma, Tengfei ;
Zhao, Yungan ;
Xiong, Wei ;
Zhang, Hongpeng .
FUSION ENGINEERING AND DESIGN, 2017, 125 :378-383
[6]   Corrosion behaviour of steels in lead-bismuth at 823 K [J].
Gnecco, F ;
Ricci, E ;
Bottino, C ;
Passerone, A .
JOURNAL OF NUCLEAR MATERIALS, 2004, 335 (02) :185-188
[7]   Intergranular precipitation-enhanced wetting and phase transformation in an Al0.4CoCrFeNi high-entropy alloy exposed to lead-bismuth eutectic [J].
Gong, Xing ;
Auger, Thierry ;
Zhu, Wenjian ;
Lei, Huasheng ;
Xiang, Congying ;
Yu, Zhiyang ;
Short, Michael P. ;
Wang, Pei ;
Yin, Yuan .
CORROSION SCIENCE, 2022, 196
[8]   X-ray computed tomography for medical imaging [J].
Hiriyannaiah, HP .
IEEE SIGNAL PROCESSING MAGAZINE, 1997, 14 (02) :42-59
[9]   Nano-indentation measurement of oxide layers formed in LBE on F/M steels [J].
Hosemann, P. ;
Swadener, J. G. ;
Welch, J. ;
Li, N. .
JOURNAL OF NUCLEAR MATERIALS, 2008, 377 (01) :201-205
[10]   Effect of deformation twinning on dissolution corrosion of 316L stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °C [J].
Klok, Oksana ;
Lambrinou, Konstantina ;
Gavrilov, Serguei ;
Stergar, Erich ;
Lim, Jun ;
Van der Donck, Tom ;
Van Renterghem, Wouter ;
De Graeve, Iris .
JOURNAL OF NUCLEAR MATERIALS, 2018, 510 :556-567