Effect of Processing Route on Microstructure and Mechanical Properties of an Al-12Si Alloy

被引:0
作者
Alsolami, Abdulrahman [1 ]
Zaman, Adnan [1 ]
Alshabouna, Fahad [2 ,3 ]
Kurdi, Abdulaziz [2 ,3 ]
Degnah, Ahmed [2 ]
Alfihed, Salman [1 ]
Tabbakh, Thamer [1 ]
Basak, Animesh Kumar [4 ]
机构
[1] King Abdulaziz City Sci & Technol, Microelect & Semicond Inst, POB 6086, Riyadh 11442, Saudi Arabia
[2] King Abdulaziz City Sci & Technol, Adv Mat Technol Inst, POB 6086, Riyadh 11442, Saudi Arabia
[3] King Abdulaziz City Sci & Technol, Ctr Excellence Adv Mat & Mfg, POB 6086, Riyadh 11442, Saudi Arabia
[4] Univ Adelaide, Adelaide Microscopy, Adelaide, SA 5005, Australia
关键词
powder laser bed fusion; microstructure; micro-pillar compression; Al-12Si (wt. %) alloy; TENSILE PROPERTIES; RESIDUAL-STRESS; HEAT-TREATMENT; SCAN STRATEGY; POWDER REUSE; BEHAVIOR; HARDNESS;
D O I
10.3390/ma17194780
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Two different microstructures of an Al-12Si (wt. %) alloy were produced, respectively, via a powder laser bed fusion (P-LBF) additive manufacturing and casting. Compared to casting, additive manufacturing of Al-based alloy requires extra care to minimize oxidation tendency. The role of the microstructure on the mechanical properties of Al-12Si (wt. %) alloy was investigated by in situ compression of the micro-pillars. The microstructure of additively manufactured specimens exhibited a sub-cellular (similar to 700 nm) nature in the presence of melt-pool arrangements and grain boundaries. On the other hand, the microstructure of the cast alloy contains typical needle-like eutectic structures. This striking difference in microstructure had obvious effects on the plastic flow of the materials under compression. The yield and ultimate compressive strength of the additively manufactured alloy were 23.69-27.94 MPa and 75.43-81.21 MPa, respectively. The cast alloy exhibited similar yield strength (31.46 MPa); however, its ultimate compressive strength (34.95 MPa) was only half that of the additively manufactured alloy. The deformation mechanism, as unrevealed by SEM investigation on the surface as well as on the cross-section of the distorted micro-pillars, confirms the presence of ductile and quasi-ductile facture of the matrix and the Si needle, respectively, in the case of the cast alloy. In contrast, the additively manufactured alloy exhibits predominantly ductile fractures.
引用
收藏
页数:13
相关论文
共 50 条
[31]   Microstructure Characteristics and Mechanical Properties of Al-12Si Coatings on AZ31 Magnesium Alloy Produced by Cold Spray Technique [J].
Hao, Yi ;
Wang, Ji-qiang ;
Cui, Xin-yu ;
Wu, Jie ;
Li, Tie-fan ;
Xiong, Tian-ying .
JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2016, 25 (05) :1020-1028
[32]   Effect of Heat Treatment on the Microstructure and Mechanical Properties of a Composite Made of Al-Si-Cu-Mg Aluminum Alloy Reinforced with SiC Particles [J].
Li, Xin ;
Yan, Hong ;
Wang, Zhi-Wei ;
Li, Ning ;
Liu, Jian-Long ;
Nie, Qiao .
METALS, 2019, 9 (11)
[33]   Microstructure Characteristics and Mechanical Properties of Al-12Si Coatings on AZ31 Magnesium Alloy Produced by Cold Spray Technique [J].
Yi Hao ;
Ji-qiang Wang ;
Xin-yu Cui ;
Jie Wu ;
Tie-fan Li ;
Tian-ying Xiong .
Journal of Thermal Spray Technology, 2016, 25 :1020-1028
[34]   A Statistical Assessment of Casting Quality-Tribological Properties of Eutectic Al-12Si Alloy: Effect of Mg [J].
Uludag, Muhammet .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (11) :7526-7543
[35]   Microstructure and mechanical properties of foundry Al-Si-Cu-Hf alloy [J].
Xing, Yuan ;
Jia, Zhihong ;
Li, Jiehua ;
Ding, Lipeng ;
Huang, Huilan ;
Liu, Qing .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 722 :197-205
[36]   Effect of Solidification Cooling Rate on Mechanical Properties and Microstructure of Al-Si-Mn-Mg Alloy [J].
Lee, Eunkyung ;
Mishra, Brajendra .
MATERIALS TRANSACTIONS, 2017, 58 (11) :1624-1627
[37]   Effect of Friction Stir Processing on the Microstructure, Damping Capacity, and Mechanical Properties of Al-Si Alloy [J].
H. J. Jiang ;
C. Y. Liu ;
Z. X. Yang ;
Y. P. Li ;
H. F. Huang ;
F. C. Qin .
Journal of Materials Engineering and Performance, 2019, 28 :1173-1179
[38]   The fatigue fracture characteristics of the bond zone of aluminum matrix composites (Al-12Si/ABOw) with Al-12Si alloys [J].
Chen, Guozheng ;
Zhang, Weizheng ;
Iizuka, Tateoki .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 755 :181-189
[39]   Influence of rheo-diecasting processing parameters on microstructure and mechanical properties of hypereutectic Al-30% Si alloy [J].
Zheng, Zhi-kai ;
Ji, Yong-jian ;
Mao, Wei-min ;
Yue, Rui ;
Liu, Zhi-yong .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2017, 27 (06) :1264-1272
[40]   Experimental investigation on microstructure and mechanical properties of direct squeeze cast Al-13%Si alloy [J].
Souissi, S. ;
Ben Amar, M. ;
Bradai, C. .
STRENGTH OF MATERIALS, 2012, 44 (03) :337-345