Effect of long-term ageing by temperatures on mechanical behaviour of Fibre Reinforced Concretes

被引:0
|
作者
Caballero-Jorna, Marta [1 ]
Roig-Flores, Marta [2 ]
Serna, Pedro [1 ]
机构
[1] Univ Politecn Valencia, ICITECH Inst Concrete Sci & Technol, 4N Bldg,Camino Vera s-n, Valencia, Spain
[2] Univ Jaume 1, Dept Mech Engn & Construct, Ave Sos Baynat s-n, Castellon de La Plana 12071, Spain
来源
JOURNAL OF BUILDING ENGINEERING | 2024年 / 98卷
关键词
Aging; Durability; Fiber reinforced Concrete; Macrosynthetic fibers; Residual flexural strength; Temperature;
D O I
10.1016/j.jobe.2024.111197
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
This study examines the effect of ageing by operating temperatures on the mechanical properties of Fibre Reinforced Concretes (FRCs) when exposed during long-term periods (180 days of conditioning). There is little information in the literature about long-term mechanical performance of steel (SFRC), and especially, macro synthetic fibre reinforced concretes (MSFRCs), which may be affected due to this exposure. One type of steel fibre and three types of macro synthetic fibres were selected to reinforce an ordinary concrete in this work. An extensive experimental campaign (with a total of 260 specimens) which includes compression and flexural tests performed at temperatures, was carried out to investigate the influence of a range of temperature from-15 to 60 degrees C. Additionally, the interaction between cracking conditions (up to 0.5 mm) and temperature was analyzed for both type of FRC beams. The compression results obtained show higher strengths at low temperatures (25-30 %) and a decrease on the strengths at higher temperatures (15-20 %), but these variations are not crucial on the ageing of FRCs. Similar effects were detected for the strength at the peak load, and to a minor extent, for the residual flexural strengths, for all the FRCs. Specimens with a pre-existing crack (cracked condition) exposed to the studied temperature had the same results as uncracked specimens. Thus, both FRCs have the potential to obtain appropriate results for structural applications when exposed to the studied temperatures.
引用
收藏
页数:15
相关论文
共 50 条
  • [31] The Effect of Long-Term Ageing on the Degradation of the Microstructure the Inconel 740h Alloy
    Sroka, M.
    Zielinski, A.
    Sliwa, A.
    Nabialek, M.
    Kania-Pifczyk, Z.
    Vaskova, I
    ACTA PHYSICA POLONICA A, 2020, 137 (03) : 355 - 360
  • [32] Effect of seawater ageing with different temperatures and concentrations on static/dynamic mechanical properties of carbon fiber reinforced polymer composites
    Li, Hailin
    Zhang, Kaifu
    Fan, Xintian
    Cheng, Hui
    Xu, Guanhua
    Suo, Haoyuan
    COMPOSITES PART B-ENGINEERING, 2019, 173
  • [33] Hygrothermal ageing effects on failure behaviour of fibre-reinforced polymer composite materials under in-situ SEM testing
    Chowdhury, Indraneel R.
    Rao, Pavan S.
    O'Dowd, Noel P.
    Comer, Anthony J.
    COMPOSITES PART B-ENGINEERING, 2025, 294
  • [34] Effects of Hygrothermal Ageing on the Mechanical Properties of Glass-Fibre-Reinforced Polymer Pultruded Profiles
    Correia, Joao R.
    Cabral-Fonseca, Susana
    Carreiro, Ana
    Costa, Ricardo
    Rodrigues, Maria Paula
    Eusebio, Isabel
    Branco, Fernando
    STRUCTURAL ENGINEERING INTERNATIONAL, 2010, 20 (04) : 370 - 378
  • [35] Time-dependent and long-term mechanical properties of concretes incorporating different grades of coarse recycled concrete aggregates
    Gholampour, Aliakbar
    Ozbakkaloglu, Togay
    ENGINEERING STRUCTURES, 2018, 157 : 224 - 234
  • [36] Experimental Investigation on the Influence of Temperature Variations on Macro-synthetic Fibre Reinforced Concrete Short and Long Term Behaviour
    Del Prete, Clementina
    Buratti, Nicola
    Mazzotti, Claudio
    FIBRE REINFORCED CONCRETE: IMPROVEMENTS AND INNOVATIONS II, BEFIB 2021, 2022, 36 : 331 - 341
  • [37] EFFECT OF AGING OF PET FIBRE ON THE MECHANICAL PROPERTIES OF PET FIBRE REINFORCED CEMENT COMPOSITE
    Machovic, Vladimir
    Andertova, Jana
    Kopecky, Lubomir
    Cerny, Martin
    Borecka, Lenka
    Pribyl, Oldrich
    Kolar, Frantisek
    Svitilova, Jaroslava
    CERAMICS-SILIKATY, 2008, 52 (03) : 172 - 182
  • [38] The Effect of Long-Term Thermal Exposure at Elevated Temperatures on Microstructures and Mechanical Properties in Centrifugally Casted Iron-Base Alloy
    Lothongkum, Gobboon
    Thaweepornkhasemsukh, Natthasit
    Wangyao, Panyawat
    JOURNAL OF METALS MATERIALS AND MINERALS, 2006, 16 (02): : 25 - 31
  • [39] Eco-friendly fibre reinforced geopolymer concrete: A critical review on the microstructure and long-term durability properties
    Li, Weiwen
    Shumuye, Eskinder Desta
    Shiying, Tang
    Wang, Zike
    Zerfu, Kefiyalew
    CASE STUDIES IN CONSTRUCTION MATERIALS, 2022, 16
  • [40] Long-term tensile properties of natural fibre-reinforced polymer composites: Comparison of flax and glass fibres
    Hristozov, Dimo
    Wroblewski, Laura
    Sadeghian, Pedram
    COMPOSITES PART B-ENGINEERING, 2016, 95 : 82 - 95