Comparative study of tool wear mechanisms in drilling ZrO2 ceramics using various tool types

被引:0
|
作者
Liu, Yin [1 ,2 ]
Lv, Shicong [1 ,2 ]
Sun, Xingwei [1 ,2 ]
Yang, Heran [1 ,2 ]
Dong, Zhixu [1 ,2 ]
Mu, Shibo [1 ,2 ]
Zhang, Weifeng [1 ,2 ]
Gong, Yadong [3 ]
机构
[1] Shenyang Univ Technol, Sch Mech Engn, 111 Shenliao West Rd,Shenyang Econ & Technol Dev D, Shenyang 110870, Peoples R China
[2] Shenyang Univ Technol, Liaoning Prov Key Lab Complex Surface NC Mfg Techn, 111 Shenliao West Rd,Shenyang Econ & Technol Dev D, Shenyang 110870, Peoples R China
[3] Northeastern Univ, Sch Mech Engn & Automat, 3-11,Wenhua Rd, Shenyang 110819, Liaoning, Peoples R China
基金
中国国家自然科学基金;
关键词
ZrO2; ceramics; Material removal mechanism; Tool wear; Hole quality; EDM METHOD; MICRO-EDM; LASER; TEMPERATURE; COMPOSITES; ELECTRODES;
D O I
10.1007/s40430-024-05220-2
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
ZrO2 ceramics are commonly known as 'hard and brittle' materials due to their exceptional properties, such as high hardness, heat resistance, chemical stability, and low thermal conductivity. However, the hole processing technique for ZrO2 ceramics often results in significant tool wear and compromises the quality of the holes. This study investigates the removal mechanism of ZrO2 ceramic materials by using carbide tools, diamond-coated carbide tools, and micro-sintered tools. It also analyzes the impact of processing parameters on the wear mechanism of different tools and the quality of hole processing in ZrO2 ceramics. The findings revealed that at high spindle speed (8000 r/min) and low feed rate (1 mm/min), the diamond coating on the rake surface of the diamond-coated carbide tool tends to peel off, leading to the formation of sharp edges on the flank surface. This phenomenon results in a reduction in thrust forces. Moreover, it is observed that as the number of hole machining operations increases, the peeling of the diamond coating on the tool flank becomes more severe. The increase in feed rate causes the diamond coating peeling area on the rake face of the tool to expand toward the chisel edge and even reach the thinned edge area near the chisel edge. When the feed rate of carbide tools increases, the wear degree of the chisel edge gradually increases, while the wear degree of the main cutting edge corner position gradually decreases. At low spindle speeds, the main cutting edge breaks and the cutter head is also damaged and deformed. The main wear mechanisms of micro-sintered tools involve shedding, fragmentation, wear, and adhesion of diamond abrasive grains. The bottom surface of the tool tends to accumulate a significant amount of flaky adhesion, which dulls the tool and increases thrust force. In contrast to carbide tools, diamond-coated carbide tools offer improved hole exit quality. However, micro-sintered tools often exhibit large volumes of flaking at the hole exits, resulting in shell-like stripes on the peeled surface.
引用
收藏
页数:24
相关论文
共 50 条
  • [1] Tool wear in drilling of machinable ceramics ZrO2/CePO4
    Yu, Ai-Bing
    Ma, Lian-Jie
    Liu, Jia-Chen
    Du, Hai-Yan
    Yu, Si-Yuan
    Tianjin Daxue Xuebao (Ziran Kexue yu Gongcheng Jishu Ban)/Journal of Tianjin University Science and Technology, 2005, 38 (08): : 669 - 673
  • [2] A study on the tool wear of PCD micro end mills in ductile milling of ZrO2 ceramics
    Rong Bian
    Ning He
    Wenzheng Ding
    Shuqing Liu
    The International Journal of Advanced Manufacturing Technology, 2017, 92 : 2197 - 2206
  • [3] A study on the tool wear of PCD micro end mills in ductile milling of ZrO2 ceramics
    Bian, Rong
    He, Ning
    Ding, Wenzheng
    Liu, Shuqing
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2017, 92 (5-8): : 2197 - 2206
  • [4] TOOL WEAR MECHANISMS IN ULTRASONIC DRILLING
    ADITHAN, M
    VENKATESH, VC
    WEAR, 1975, 34 (03) : 449 - 453
  • [5] COMPARATIVE STUDY OF MATERIAL DAMAGE AND TOOL WEAR MECHANISMS DURING DRILLING OF CFRP/ TI STACK
    Mathiyazhagan, Vijayathithan
    Meena, Anil
    PROCEEDINGS OF THE ASME INTERNATIONAL MECHANICAL ENGINEERING CONGRESS AND EXPOSITION, 2019, VOL 2A, 2019,
  • [6] Tool Wear Characters in Micro-milling of Fully Sintered ZrO2 Ceramics by Diamond Coated End Mills
    Bian, Rong
    Ferraris, Eleonora
    Qian, Jun
    Reynaerts, Dominiek
    Li, Liang
    He, Ning
    HIGH SPEED MACHINING V, 2012, 723 : 365 - +
  • [7] Study on tool wear monitoring with wavelets in drilling
    Xi'an Dianzi Keji Daxue Xuebao, 2 (204-206, 210):
  • [8] EFFECT OF SULFUR-CONTENT IN STEEL ON THE WEAR OF ZRO2 CUTTING-TOOL
    KATAYAMA, S
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1987, 73 (05): : S579 - S579
  • [9] EFFECT OF SULFUR-CONTENT IN STEEL ON THE WEAR OF ZRO2 CUTTING-TOOL
    KATAYAMA, S
    IMAI, T
    SUZUKI, N
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1987, 27 (09) : B236 - B236
  • [10] Study on the diamond tool drilling of engineering ceramics
    Zhang, QH
    Zhang, JH
    Sun, DM
    Wang, GD
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2002, 122 (2-3) : 232 - 236