A novel approach to enhance formability in Ti-6Al-4V alloy: Experimental investigations and microstructural analysis of pulsating tensile test

被引:0
作者
Korkmaz, Habip Gokay [1 ,2 ]
Yapan, Yusuf Furkan [3 ]
Toros, Serkan [1 ]
Turkoz, Mevlut [2 ]
机构
[1] Nigde Omer Halisdemir Univ, Dept Mech Engn, TR-51100 Nigde, Turkiye
[2] Konya Tech Univ, Dept Mech Engn, TR-42250 Konya, Turkiye
[3] Yildiz Tech Univ, Dept Mech Engn, TR-34349 Istanbul, Turkiye
关键词
Pulsating loading; Ti-6Al-4V; Stress relaxation test; Loading-unloading test; Tensile test; STRESS-RELAXATION; DUCTILITY IMPROVEMENT; TITANIUM; 304-STAINLESS-STEEL; BEHAVIOR;
D O I
10.1016/j.cirpj.2024.09.008
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ti-6Al-4V alloy, widely utilized in aerospace, medical industries, and specialized applications, boasts exceptional properties. However, its limited formability poses challenges in manufacturing processes. The pulsating loading method emerges as a promising solution to enhance formability in such materials. This study delves into the impact of stress relaxation and loading-unloading tests on the formability of Ti-6Al-4V alloy, conducting tensile tests on sheets of two different thicknesses: 0.5 mm and 2.65 mm. Investigating parameters such as pulse starting strain, relaxation time, and strain increment in stress relaxation experiments, as well as unloading ratio and strain increment in loading-unloading experiments, enabled a comprehensive comparison of the two pulsating loading methods across different sheet thicknesses. Results indicate a notable increase in material formability, up to approximately 20 % for the 2.65 mm thickness and up to 50 % for the 0.5 mm thickness compared to monotonic loading. Stress relaxation time emerged as the most influential parameter for both thicknesses. Additionally, XRD analysis was employed to elucidate the microstructural reasons behind the observed formability enhancement, while SEM imaging provided insights into the fracture surface morphology. This systematic approach sheds light on the microstructural mechanisms underlying the effect of pulsating loading on material behavior.
引用
收藏
页码:98 / 107
页数:10
相关论文
共 50 条
[21]   Formability improvement in Ti-6Al-4 V sheet at room temperature by pulsating hydraulic bulging: experimental and numerical investigations [J].
Ozturk, Osman ;
Korkmaz, Habip G. ;
Atas, Gurkan ;
Aydin, Mevlut ;
Turkoz, Mevlut ;
Toros, Serkan ;
Dilmec, Murat ;
Livatyali, Haydar ;
Kotan, Hasan ;
Halkaci, H. Selcuk .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2023, 124 (7-8) :2903-2918
[22]   Microstructural characterization of Ti-6Al-4V alloy subjected to the duplex SMAT/plasma nitriding [J].
Pi, Y. ;
Faure, J. ;
Agoda-Tandjawa, G. ;
Andreazza, C. ;
Potiron, S. ;
Levesque, A. ;
Demangel, C. ;
Retraint, D. ;
Benhayoune, H. .
MICROSCOPY RESEARCH AND TECHNIQUE, 2013, 76 (09) :897-903
[23]   Understanding the microstructural evolution of cold sprayed Ti-6Al-4V coatings on Ti-6Al-4V substrates [J].
Lek, Jun Yan ;
Bhowmik, Ayan ;
Tan, Adrian Wei-Yee ;
Sun, Wen ;
Song, Xu ;
Zhai, Wei ;
Buenconsejo, Pio J. ;
Li, Feng ;
Liu, Erjia ;
Lam, Yeng Ming ;
Boothroyd, Chris B. .
APPLIED SURFACE SCIENCE, 2018, 459 :492-504
[24]   Finite element analysis of spring back in Ti-6Al-4V alloy [J].
Wahed, M. A. ;
Gadi, V. S. R. ;
Gupta, A. K. ;
Supradeepan, K. ;
Singh, S. K. ;
Kotkunde, N. R. .
MATERIALS TODAY-PROCEEDINGS, 2019, 18 :2693-2699
[25]   Characterization of the deformation texture after tensile test and cold rolling of a Ti-6Al-4V sheet alloy [J].
Mehdi, B. ;
Azzeddine, H. ;
Badji, R. ;
Ji, V. ;
Alili, B. ;
Bradai, D. .
17TH INTERNATIONAL CONFERENCE ON TEXTURES OF MATERIALS (ICOTOM 17), 2015, 82
[26]   Experimental and numerical investigation of the damage state of Ti-6Al-4V alloy sheet in the tensile test, hydraulic bulging, and hydroforming processes [J].
Yapan, Yusuf Furkan ;
Korkmaz, Habip Gokay ;
Toros, Serkan ;
Turkoz, Mevlut .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2024, 132 (9-10) :4585-4605
[27]   Mechanical and microstructural variations in ECAP of Ti-6Al-4V alloy with equiaxed microstructure [J].
Arabi, Hamid ;
Ketabchi, Mostafa ;
Alhosseini, S. H. N. .
RARE METALS, 2022, 41 (08) :2732-2738
[28]   Microstructure-Tensile Properties Correlation for the Ti-6Al-4V Titanium Alloy [J].
Shi, Xiaohui ;
Zeng, Weidong ;
Sun, Yu ;
Han, Yuanfei ;
Zhao, Yongqing ;
Guo, Ping .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (04) :1754-1762
[29]   Strong and Ductile Ti-6Al-4V Alloy Produced by Hot Pressing of Ti-6Al-4V Swarf [J].
Yang, F. ;
Pi, Z. Q. ;
Zhao, Q. Y. ;
Raynova, S. ;
Liu, Q. ;
Sharp, K. ;
Brandt, M. ;
Bolzoni, L. ;
Qian, M. .
JOM, 2019, 71 (03) :1056-1061
[30]   Experimental Studies on Duplex Turning of Titanium Alloy (Ti-6Al-4V) [J].
Kumar, Sunil ;
Yadav, Ravindra Nath ;
Kumar, Raghuvir .
2017 INTERNATIONAL CONFERENCE ON ADVANCES IN MECHANICAL, INDUSTRIAL, AUTOMATION AND MANAGEMENT SYSTEMS (AMIAMS) - PROCEEDINGS, 2017, :337-341