Experimental study on spheroidal morphology of palladium coated copper wire with different palladium layer thickness

被引:0
|
作者
An, Bin [1 ]
Zhou, Hongliang [1 ,2 ]
Cao, Jun [1 ,2 ]
Ming, Pingmei [1 ,2 ]
Xia, Jie [1 ]
Yao, Jingguang [1 ]
Persic, John [1 ,3 ]
Zhang, Yuemin [1 ,2 ]
机构
[1] Henan Polytech Univ, Sch Mech & Power Engn, Jiaozuo 454003, Peoples R China
[2] Henan Polytech Univ, Henan Int Joint Lab Adv Elect Packaging Mat Precis, Jiaozuo 454003, Peoples R China
[3] Microbonds Inc, 7495 Birchmount Rd, Markham, ON L3R 5G2, Canada
来源
APL MATERIALS | 2024年 / 12卷 / 10期
基金
中国国家自然科学基金;
关键词
CORROSION BEHAVIOR; CU; RELIABILITY; MECHANISM; AL;
D O I
10.1063/5.0232025
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Palladium (Pd) coated copper (PCC) wire is an emerging bonding wire that has been widely researched. In this paper, the effects of electronic flame-off (EFO) current and EFO time on the free air ball (FAB) morphology of four PCC wires with Pd layer thicknesses of 60, 80, 100, and 120 nm, respectively, are first investigated. The larger the EFO current or the longer the EFO time, the larger the FAB diameter. The EFO time or EFO current setting is either too high or too low to form a FAB with good morphology. Taking the ratio of FAB diameter to wire diameter as 2 as the standard, the EFO current of 48 mA and the EFO time of 700 mu s are selected as the optimal EFO parameter combination. Under this parameter combination, the symmetry, roundness, and surface smoothness of the FAB of the four PCC wires are all at a better level. It is found that the FAB surface Pd coverage of PCC wire with 120 nm Pd layer thickness is higher through the corrosion test. The Pd transfer law on the FAB at different EFO times under optimal EFO current is also studied. The results show that with the prolongation of the EFO time, the Pd on the FAB surface is gradually transferred from the neck to the middle and lower parts. This study can provide technical reference for the selection of Pd layer thickness and EFO parameters of PCC wire. (c) 2024 Author(s).
引用
收藏
页数:13
相关论文
共 50 条
  • [21] Leadframes' AuAg plating thickness influences to stitch bonding of palladium coated copper wires
    Tey, Sock Chien
    Lau, Kok-Tee
    Abd. Manaf, Mohd Edderozey
    2015 16TH INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY, 2015,
  • [22] Ultra Low Loop Wire Bonding of 20 μm Palladium Coated Copper Wire for Very Thin Packages
    Hwa, Loh Kian
    Jeng, Loh Lee
    Har, Liew Siew
    Erfe, Eric
    2014 IEEE 36TH INTERNATIONAL ELECTRONICS MANUFACTURING TECHNOLOGY CONFERENCE (IEMT), 2015,
  • [23] Investigation of Palladium Coverage on Bonded Balls of Palladium-Coated Copper Wires
    Koh, Wei
    Lee, Teck-Kheng
    Ng, Hun-Shen
    Goh, Kay-Soon
    Ho, Hong-Meng
    2011 12TH INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY AND HIGH DENSITY PACKAGING (ICEPT-HDP), 2011, : 188 - 194
  • [24] Characterization of a Wire Bonding Process with the Added Challenges from Palladium-coated Copper Wires
    Chang, A. C. K.
    Lim, A. B. Y.
    Lee, C. X.
    Milton, B.
    Clauberg, H.
    Yauw, O.
    Chylak, B.
    2012 35TH IEEE/CPMT INTERNATIONAL ELECTRONICS MANUFACTURING TECHNOLOGY SYMPOSIUM (IEMT), 2012,
  • [25] Behavior of palladium and its impact on intermetallic growth in palladium-coated Cu wire bonding
    Xu, Hui
    Qin, Hry
    Clauberg, Horst
    Chylak, Bob
    Acoff, Viola L.
    ACTA MATERIALIA, 2013, 61 (01) : 79 - 88
  • [26] Investigation of Palladium Coverage on Free Air Balls of Palladium-Coated Copper Wires
    Pu, Haonan
    Lo, Tawei
    Wang, Techun
    Wang, Jiaji
    2012 13TH INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY & HIGH DENSITY PACKAGING (ICEPT-HDP 2012), 2012, : 1110 - 1113
  • [27] Development of Palladium-based Oxygen Scavenger: Optimization of Substrate and Palladium Layer Thickness
    Yildirim, Selcuk
    Roecker, Bettina
    Rueegg, Nadine
    Lohwasser, Wolfgang
    PACKAGING TECHNOLOGY AND SCIENCE, 2015, 28 (08) : 710 - 718
  • [28] Adsorption of 125I on palladium coated silver wire
    He, Jiaheng
    Song, Hu
    Jian, Yuan
    Jiang, Lin
    Zhong, Wenbin
    Li, Xinliang
    Ma, Zongping
    Liu, Guoping
    JOURNAL OF RADIOANALYTICAL AND NUCLEAR CHEMISTRY, 2011, 290 (02) : 469 - 473
  • [29] Adsorption of 125I on palladium coated silver wire
    Jiaheng He
    Hu Song
    Yuan Jian
    Lin Jiang
    Wenbin Zhong
    Xinliang Li
    Zongping Ma
    Guoping Liu
    Journal of Radioanalytical and Nuclear Chemistry, 2011, 290 : 469 - 473
  • [30] Palladium Coated Copper Wire Wedge Integrity To Withstand Extended High Temperature Storage Stress Test
    Chia, Lee Cher
    Guan, Tan Kim
    Lam, Cha Chan
    Hoe, Mak Chee
    Yen, Gwee Hoon
    2016 IEEE 37TH INTERNATIONAL ELECTRONICS MANUFACTURING TECHNOLOGY (IEMT) & 18TH ELECTRONICS MATERIALS AND PACKAGING (EMAP) CONFERENCE, 2016,