Consolidation and properties of tungsten carbide target with low cobalt content by hot-press sintering

被引:0
作者
Shao, G.Q. [1 ]
Xiong, Z. [1 ]
Wang, T.G. [1 ]
Shi, X.L. [1 ]
Duan, X.L. [1 ]
机构
[1] State Key Laboratory of Advanced Technology for Materials Synthesis and Processing, Wuhan University of Technology
关键词
Hot-press sintering; In-situ reaction; Target; Tungsten carbide;
D O I
10.4028/0-87849-451-0.98
中图分类号
学科分类号
摘要
Tungsten carbide (WC) targets with low cobalt (Co) content (0.1 - 0.2 wt.%) were prepared by hot-press sintering at 1700°C for 60 minutes in argon, from element starting powders of tungsten, cobalt and carbon. Results show that the as-fabricated targets yield relatively high relative density above 99% and high HRA above 92. WC with low Co content is formed easily than pure WC The hot-press sintering process, while element starting powders are used, is an in-situ reaction technique for accelerating the WC's diffusion rate to obtain a dense sintered body.
引用
收藏
页码:98 / 102
页数:4
相关论文
共 18 条
  • [1] Lassner E., Schubert W.-D., Tungsten - Properties, Chemistry, Technology of the Element, Alloys, and Chemical Compounds, (2000)
  • [2] Upadhyaya G.S., Cemented Tungsten Carbides - Production, Properties, and Testing, (1998)
  • [3] Engqvist H., Botton G.A., Axen N., Hogmark S., J. Am. Ceram. Soc, 83, (2000)
  • [4] Ledoux M.J., Pham C.H., Guille J., Dunlop H., J. Catal, 134, (1992)
  • [5] Koc R., Kodambaka S.K., J. Eur. Ceram. Soc, 20, (2000)
  • [6] Strondl C., Carvalho N.M., De Hosson J.T.M., Krug T.G., Surf. Coat. Technol, 200, (2005)
  • [7] Strondl C., Carvalho N.M., De Hosson J.T.M., van der Kolk G.J., Surf. Coat. Technol, 162, (2003)
  • [8] Rincon C., Romero J., Esteve J., Martinez E., Lousa A., Surf. Coat. Technol, 163-164, (2003)
  • [9] Omori M., Mater. Sci. Eng. A, 287, (2000)
  • [10] Cha S.I., Hong S.H., Mater. Sci. Eng. A, 356, (2003)