Corrosion Behavior of Steam Injection Pipeline in CO2/O2/SO2 Environment

被引:0
|
作者
Zou, Qing [1 ]
Liao, Ke-Xi [1 ]
Liu, Xin-Yu [2 ]
He, Guo-Xi [1 ]
Leng, Ji-Hui [1 ]
Zhao, Shuai [1 ]
Peng, Mu-Lin [1 ]
机构
[1] School of Oil and Gas Engineering, Southwest Petroleum University, Chengdu,610000, China
[2] Sichuan Faithful Petroleum and Natural Gas Engineering Co., Ltd., Chengdu,610000, China
来源
Surface Technology | 2022年 / 51卷 / 07期
关键词
Corrosion protection - Corrosion rate - Corrosive effects - Hematite - High temperature corrosion - Localized corrosion - Oxygen - Passivation - Pipeline corrosion - Pipelines - Scanning electron microscopy - Steam - Steel corrosion - Tensile strength - Tensile testing - X ray diffraction;
D O I
暂无
中图分类号
学科分类号
摘要
In order to reveal the corrosion behavior and mechanical properties of 45# steel and 3Cr steel in the high temperature and pressure CO2/O2/SO2 system, and provide theoretical support for the safe operation of steam injection pipelines in Xinjiang Oilfield. Based on the on-site operating conditions of the steam injection pipeline, combined with high temperature autoclave, combined with scanning electron microscope, 3D microscope, X-ray diffractometer (XRD) and other means, weight loss test, product characterization and tensile test are carried out. With the increase of temperature (100-250 ℃), the corrosion rate of 45# steel and 3Cr steel shows a decreasing trend; with the increase of O2 content (0-3mol%), the corrosion of 45# steel and 3Cr steel rate first increases and then decreases, and the corrosion is inhibited when the O2 content is 2mol%-3mol%. The XRD test results show that the corrosion products of 45# steel in the CO2/O2/SO2 system mainly include FeSO4·H2O, FeCO3, Fe2O3, and the corrosion products of 3Cr steel mainly include Cr2O3, FeSO4·H2O, FeCO3, and Fe2O3. The 3D microscope results show that 45# there are obvious local corrosion defects on the surface of the steel substrate, and 3Cr steel does not appear local corrosion; the mechanical properties show that the tensile strength of 45# steel after corrosion is reduced by 1.36%, the elongation is reduced by 6.85%, and the tensile strength of 3Cr steel after corrosion Reduced by 0.39%, elongation reduced by 21.34%. In the high temperature and pressure CO2/O2/SO2 environment, SO2 dominates the corrosion process; the corrosion product film is dense at high temperature (100-250 ℃), which inhibits corrosion; O2 participates in the cathodic reaction, and in the low concentration of oxygen (0-2mol%), the corrosion product film is destroyed to promote corrosion. When high concentration oxygen (2mol%-3mol%), the steel matrix is passivated to inhibit corrosion; after corrosion, the mechanical properties of the steel are degraded, and corrosion has a greater impact on the elongation of the steel. The tensile strength is less affected. © 2022, Chongqing Wujiu Periodicals Press. All rights reserved.
引用
收藏
页码:225 / 235
相关论文
共 50 条
  • [21] NOx and SO2 emissions from O2/CO2 recycle coal combustion
    Croiset, E
    Thambimuthu, KV
    FUEL, 2001, 80 (14) : 2117 - 2121
  • [22] COLLISION-INDUCED EMISSION IN MN + O2, NO2, CO2, AND SO2
    LEVY, MR
    JOURNAL OF PHYSICAL CHEMISTRY, 1991, 95 (22): : 8500 - 8506
  • [23] Research on corrosion behavior of ground gathering pipeline under CO2/H2S/O2 system
    Huang Q.
    Surface Technology, 2021, 50 (04): : 351 - 360
  • [24] Effect of High-Concentration O2 on Corrosion Behavior of X70 Steel in Water-Containing Supercritical CO2 with SO2
    Xu, Minghe
    Zhang, Qian
    Wang, Zhe
    Liu, Jianmin
    Li, Zheng
    CORROSION, 2017, 73 (03) : 290 - 302
  • [25] Long term corrosion of X70 steel and iron in humid supercritical CO2 with SO2 and O2 impurities
    Xiang, Y.
    Wang, Z.
    Li, Z.
    Ni, W.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2013, 48 (05) : 395 - 398
  • [26] Effect of SO2, O2, NO2, and H2O Concentrations on Chemical Reactions and Corrosion of Carbon Steel in Dense Phase CO2
    Morland, Bjorn
    Truls, Norby
    Tjelta, Morten
    Svenningsen, Gaute
    CORROSION, 2019, 75 (11) : 1327 - 1338
  • [27] An investigation into the adverse effects of O2, SO2, and NOx on polyethyleneimine functional CO2 adsorbents
    Li, Kaimin
    Jiang, Jianguo
    SN APPLIED SCIENCES, 2021, 3 (03):
  • [28] An investigation into the adverse effects of O2, SO2, and NOx on polyethyleneimine functional CO2 adsorbents
    Kaimin Li
    Jianguo Jiang
    SN Applied Sciences, 2021, 3
  • [29] A novel material selection method and application in an aqueous environment containing CO2, H2S, O2 and SO2
    Liao, Kexi
    Leng, Jihui
    Yan, Yongbo
    He, Tengjiao
    Lv, Xidi
    Liu, Xin
    Qin, Min
    Zhao, Shuai
    Cheng, Y. Frank
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2024, 59 (01) : 27 - 38
  • [30] Reactivity of micas and cap-rock in wet supercritical CO2 with SO2 and O2 at CO2 storage conditions
    Pearce, Julie K.
    Dawson, Grant K. W.
    Law, Alison C. K.
    Biddle, Dean
    Golding, Suzanne D.
    APPLIED GEOCHEMISTRY, 2016, 72 : 59 - 76