Bending Strength of en AC-44200-Al2O3 Composites at Elevated Temperatures

被引:4
|
作者
Kurzawa A. [1 ]
Kaczmar J.W. [1 ]
机构
[1] Politechnika Wrocławska, Faculty of Mechanical Engineering, Department of Foundry Engineering, Plastics and Automation, Smoluchowskiego 25, Wrocław
来源
Kurzawa, A. (adam.kurzawa@pwr.edu.pl) | 1600年 / De Gruyter Open Ltd卷 / 17期
关键词
Aluminium alloy composite materials; Aluminium oxide particles; Bending strength;
D O I
10.1515/afe-2017-0019
中图分类号
学科分类号
摘要
The paper presents results of bend tests at elevated temperatures of aluminium alloy EN AC-44200 (AlSi12) based composite materials reinforced with aluminium oxide particles. The examined materials were manufactured by squeeze casting. Preforms made of Al2O3 particles, with volumetric fraction 10, 20, 30 and 40 vol.% of particles joined with sodium silicate bridges were used as reinforcement. The preforms were characterised by open porosity ensuring proper infiltration with the EN AC-44200 (AlSi12) liquid alloy. The largest bending strength was found for the materials containing 40 vol.% of reinforcing ceramic particles, tested at ambient temperature. At increased test temperature, bending strength Rg of composites decreased in average by 30 to 50 MPa per 100°C of temperature increase. Temperature increase did not significantly affect cracking of the materials. Cracks propagated mainly along the interfaces particle/matrix, with no effect of the particles falling-out from fracture surfaces. Direction of cracking can be affected by a small number of agglomerations of particles or of non-reacted binder. In the composites, the particles strongly restrict plastic deformation of the alloy, which leads to creation of brittle fractures. At elevated temperatures, however mainly at 200 and 300°C, larger numbers of broken, fragmented particles was observed in the vicinity of cracks. Fragmentation of particles occurred mainly at tensioned side of the bended specimens, in the materials with smaller fraction of Al2O3 reinforcement, i.e. 10 and 20 vol.%. © 2017 by A. Kurzawa.
引用
收藏
页码:103 / 108
页数:5
相关论文
共 42 条
  • [1] Cracked-Healing and Elevated Temperature Bending Strength of Al2O3 Composite Ceramics by an Amount of Y2O3
    Nam, K. W.
    Kim, H. S.
    Son, C. S.
    Kim, S. K.
    Ahn, S. H.
    TRANSACTIONS OF THE KOREAN SOCIETY OF MECHANICAL ENGINEERS A, 2007, 31 (11) : 1108 - 1114
  • [2] Bending strength recovery and crack healing behavior of Al2O3/SiC nanocomposites at different annealing temperatures
    Zhai, HZ
    Li, JB
    Huang, XD
    HIGH-PERFORMANCE CERAMICS 2001, PROCEEDINGS, 2002, 224-2 : 325 - 329
  • [3] Evaluating Bending Strength of Plasma Sprayed Al2O3 Coatings
    Zhijian Yin
    Shunyan Tao
    Xiaming Zhou
    Chuanxian Ding
    Journal of Thermal Spray Technology, 2009, 18 : 292 - 296
  • [4] Evaluating Bending Strength of Plasma Sprayed Al2O3 Coatings
    Yin, Zhijian
    Tao, Shunyan
    Zhou, Xiaming
    Ding, Chuanxian
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2009, 18 (02) : 292 - 296
  • [5] BENDING STRENGTH AND MICROSTRUCTURE OF AL2O3-Y2O3-MGO AND AL2O3-Y2O3-ZRO2-MGO COMPOSITE CERAMICS
    TAKEUCHI, S
    NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1992, 100 (04): : 608 - 612
  • [6] Effect of residual stress on the bending strength of ground Al2O3/TiCN ceramics
    Yang, HT
    Gao, L
    Yuan, RZ
    Kim, KR
    Jung, JY
    MATERIALS CHEMISTRY AND PHYSICS, 2003, 80 (01) : 305 - 308
  • [7] Effect of the addition ZrO2-Al2O3 on nanocrystalline hydroxyapatite bending strength and fracture toughness
    Mobasherpour, I.
    Hashjin, M. Solati
    Toosi, S. S. Razavi
    Kamachali, R. Darvishi
    CERAMICS INTERNATIONAL, 2009, 35 (04) : 1569 - 1574
  • [8] Preliminary study of the crack healing and strength recovery of Al2O3-matrix composites
    Jun, L
    Zheng, ZX
    Ding, HF
    Jin, ZH
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2004, 27 (02) : 89 - 97
  • [9] Bending strength of Al2O3 ceramics for textiles machinery and elastic wave characteristics by wavelet analysis
    Nam, K. W.
    Ahn, B. G.
    Kim, M. K.
    Son, C. S.
    Kim, J. W.
    Ahn, S. H.
    PROGRESSES IN FRACTURE AND STRENGTH OF MATERIALS AND STRUCTURES, 1-4, 2007, 353-358 : 345 - +
  • [10] Effect of rheological properties of the suspension on the mechanical strength of Al2O3-ZrO2 composites prepared by gelcasting
    Liu, XL
    Huang, Y
    Yang, JL
    CERAMICS INTERNATIONAL, 2002, 28 (02) : 159 - 164