Additively manufactured fine-grained Al-Fe-Cu-Sc-Zr alloy with resistance to brittleness under high temperature

被引:0
作者
Shi, Qianyu [1 ]
Chen, Jibing [1 ]
Chen, Junsheng [1 ]
Wang, Yueting [2 ,3 ]
Xia, Xizhen [2 ,3 ]
Li, Ruidi [2 ,3 ]
机构
[1] Wuhan Polytech Univ, Sch Mech Engn, Wuhan 430023, Hubei, Peoples R China
[2] Cent South Univ, Powder Met Res Inst, Changsha 410083, Hunan, Peoples R China
[3] Cent South Univ, State Key Lab Powder Met, Changsha 410083, Hunan, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2024年 / 33卷
基金
中国国家自然科学基金;
关键词
Additive manufacturing; Laser powder bed fusion; Aluminum alloy; Anti-brittleness; High temperature; MECHANICAL-PROPERTIES; MICROSTRUCTURAL EVOLUTION; DEFORMATION-BEHAVIOR; LASER; SOLIDIFICATION; DEPENDENCE;
D O I
10.1016/j.jmrt.2024.11.104
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Existing additively manufactured aluminum alloys exhibit a sharp decrease in yield strength at moderate temperatures (200 degrees C-400 degrees C), failing to meet the high-temperature resistance required in the complex service environments of aerospace applications. In this paper, an Al-2.5Fe-2Cu-0.6Sc-0.3Zr alloy material was designed and formed by laser powder bed fusion (L-PBF) technology. The optimal composition ratio was obtained by comparing the formed structures and properties, and then the phase composition, microstructure, precipitation distribution and mechanical properties were characterized and analyzed at high temperature. The result shows that the alloy's primary precipitate phases are Al6Fe (Al23CuFe4) and L12-Al3(Sc, Zr) at nano scale. Adding Zr and Sc, the thermal stability of Al6Fe is enhanced, delaying its transformation to the 0-Al13Fe4 phase and refining the particle size. The Al23CuFe4 phase, stabilized thermodynamically by substituting of Cu for Al atoms in the orthorhombic structure (oC28), also contributes to the stabilization of the Al6Fe phase. Moreover, This aluminum alloy obtained a yield strength of 449 MPa at room temperature and a yield strength of 142 MPa at 300 degrees C. In addition, it also shows excellent brittleness resistance under high temperature, which is better than most L-PBF aluminum alloys reported so far. These findings offer valuable insights for the future development of aluminumbased alloys with heat-resistant performance, and promising strategies for addressing particle coarsening under high temperature and intermediate-temperature brittleness.
引用
收藏
页码:7310 / 7324
页数:15
相关论文
共 50 条
  • [21] Significantly enhanced the ductility of the fine-grained Al-Zn-Mg-Cu alloy by strain-induced precipitation
    Lang, Yujing
    Zhou, Guxin
    Hou, Longgang
    Zhang, Jishan
    Zhuang, Linzhong
    MATERIALS & DESIGN, 2015, 88 : 625 - 631
  • [22] High temperature performance of additively manufactured Al 2024 alloy: Constitutive modelling, dynamic recrystallization evolution and kinetics
    Gairola, Saurabh
    Singh, Gaurav
    Jayaganthan, R.
    Ajay, Joe
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 25 : 3425 - 3443
  • [23] Study on Microstructure and High-Temperature Mechanical Properties of Al-Mg-Sc-Zr Alloy Processed by LPBF
    Ren, Zhihao
    Zhang, Hao
    Shu, Xuedao
    Xu, Haijie
    Chen, Siyuan
    Ding, Yaoyao
    Liang, Liwen
    Qiu, Zixiang
    Yang, Yang
    Zheng, Yongjian
    METALS, 2024, 14 (08)
  • [24] A novel two-step method to prepare fine-grained SiC/Al-Mg-Sc-Zr nanocomposite: Processing, microstructure and mechanical properties
    Huang, Guoqiang
    Wu, Jie
    Hou, Wentao
    Shah, Luqman Hakim Ahmad
    Midawi, Abdelbaset R. H.
    Cao, Fujun
    Gerlich, Adrian
    Shen, Yifu
    Meng, Fanqiang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 823
  • [25] Preparation and properties of Al2O3 dispersed fine-grained W-Cu alloy
    Zhang, He
    Liu, Jun-Ru
    Li, Zhi-Bo
    Deng, Xiao-Chun
    Zhang, Guo-Hua
    Chou, Kuo-Chih
    ADVANCED POWDER TECHNOLOGY, 2022, 33 (03)
  • [26] High temperature stability of fine grained 7075Al alloy containing nanosized SiC particles
    Mohseni, H.
    Keirs, S.
    Chan, S. L. I.
    Ferry, M.
    MATERIALS SCIENCE AND TECHNOLOGY, 2010, 26 (05) : 597 - 603
  • [27] Additively manufactured Al-Ce-Ni-Mn alloy with improved elevated-temperature fatigue resistance*
    Michi, Richard A.
    Simpson, Joseph J.
    Bahl, Sumit
    Campbell, Quinn
    Brackman, Paul
    Plotkowski, Alex
    Dehoff, Ryan R.
    Haynes, J. A.
    Wang, Qigui
    Shyam, Amit
    ADDITIVE MANUFACTURING, 2023, 66
  • [28] Microstructure, metallurgical defects and hardness of Al-Cu-Mg-Li-Zr alloy additively manufactured by selective laser melting
    Xu, Rong
    Li, Ruidi
    Yuan, Tiechui
    Niu, Pengda
    Wang, Minbo
    Lin, Zehuan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 835
  • [29] Superplastic behavior of fine-grained Ti-10V-2Fe-3Al alloy fabricated by friction stir processing
    Wang, Kai
    Zhang, Wenjing
    Ogura, Takuya
    Morisada, Yoshiaki
    Zhao, Xinqing
    Fujii, Hidetoshi
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2025, 206 : 26 - 36
  • [30] High-temperature strength sustained by nano-sized eutectic structure of Al-Fe alloy manufactured by laser powder bed fusion
    Wang, Wenyuan
    Takata, Naoki
    Suzuki, Asuka
    Kobashi, Makoto
    Kato, Masaki
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 838