Experimental research on the hydration heat temperature field of hollow concrete piers

被引:0
|
作者
Peng, Jun [1 ]
Tang, Chunping [2 ]
Zhang, Liangliang [3 ]
Saeed, Ayad Thabit [4 ]
机构
[1] Chongqing Vocational Institute of Engineering, Chongqing, China
[2] Chongqing Technology and Business Institute, Chongqing, China
[3] College of Civil Engineering, Chongqing University, Chongqing, China
[4] T.Y.Lin International Engineering Consulting Co., Ltd, Chongqing, China
来源
关键词
Measuring points were observed continuously to reveal the hydration heat temperature distribution of hollow concrete bridge pier. The results showed that as the thickness of the pier increased; the central temperature of the pier increased significantly due to hydration and the heat was difficult to be dissipated. The hydration temperature accounted for up to 70% of the maximum temperature rise during 20 h and reached the maximum temperature at 24 h after pouring the concrete. There was a jump value between the central temperature and surface temperature in a short period after removing the framework. The jumping was the most dangerous moment for the cracking of pier surfaces. Therefore; the formwork removal time has to be determined prudently and corresponding measures have to be conducted to reduce the possibility of pier surface cracking. © Peng et al; Licensee Bentham Open;
D O I
10.2174/1874836801408010482
中图分类号
学科分类号
摘要
引用
收藏
页码:482 / 487
相关论文
共 50 条
  • [1] Analysis of the temperature field of hydration heat in a hollow and high concrete pier
    Tang, Chunping (tcp501@163.com), 1600, Universidad Central de Venezuela (55):
  • [2] Experimental Research on Hydration Heat Temperature of Concrete Box Girder in Low-Temperature Environment
    Sun, Wei-gang
    Liu, Lai-jun
    Wu, Qun-hu
    Feng, Jian-ping
    MECHANICAL ENGINEERING, MATERIALS SCIENCE AND CIVIL ENGINEERING II, 2014, 470 : 1045 - +
  • [3] Experimental and finite element investigations on hydration heat and early cracks in massive concrete piers
    Sheng, Xingwang
    Xiao, Shimiao
    Zheng, Weiqi
    Sun, Huanzhong
    Yang, Ying
    Ma, Kunlin
    CASE STUDIES IN CONSTRUCTION MATERIALS, 2023, 18
  • [4] Experimental and finite element investigations on the temperature field of a massive bridge pier caused by the hydration heat of concrete
    Huang, Yonghui
    Liu, Guoxing
    Huang, Shiping
    Rao, Rui
    Hu, Changfu
    CONSTRUCTION AND BUILDING MATERIALS, 2018, 192 : 240 - 252
  • [5] Temperature field calculation and influencing factors analysis for concrete hollow piers under solar radiation
    Fu, B. (fobofobo@163.com), 1600, Binary Information Press, Flat F 8th Floor, Block 3, Tanner Garden, 18 Tanner Road, Hong Kong (10):
  • [6] Experimental study on effective stiffness of reinforced concrete hollow piers
    Wei, Wang
    Shao, Changjiang
    Xiao, Zhenghao
    Qi, Qiming
    Hu, Chenxu
    Xiao, Laichuan
    Wang, Meng
    Tumu Gongcheng Xuebao/China Civil Engineering Journal, 2019, 52 (10): : 101 - 110
  • [7] Analytical Solution for the Temperature Field of the Hydration Heat in a Mass Concrete Wall
    Li Z.
    Luo Q.
    Han Q.
    Zhang J.
    Sun J.
    Tianjin Daxue Xuebao (Ziran Kexue yu Gongcheng Jishu Ban)/Journal of Tianjin University Science and Technology, 2023, 56 (08): : 878 - 885
  • [8] Research on shear strength of rectangular hollow reinforced concrete piers
    Zhang, Xizhi
    Li, Xingqian
    Zhang, Shaohua
    Ding, Yongjun
    Meng, Xiangliang
    Wang, Lei
    Harbin Gongcheng Daxue Xuebao/Journal of Harbin Engineering University, 2022, 43 (02): : 203 - 211
  • [9] Comparative study on seismic performance of concrete-filled double skin tubular piers and hollow concrete piers: Experimental and analytical
    Li, Zhong-Xian
    Du, Chunyu
    Liu, Dong
    Liang, Xiao
    Zhao, Bo
    STRUCTURES, 2023, 49 : 1078 - 1092
  • [10] Time dependent effect on hydration heat temperature and stress field for concrete box girder
    School of Highway, Chang'an University, Xi'an 710064, China
    Chang'an Daxue Xuebao, 2008, 4 (51-56):