Electroless nickel plating process and properties of alumina ceramics

被引:0
|
作者
Zheng, Xiao-Hui [1 ]
Shan, Dong-Dong [1 ]
Song, Hao [1 ]
Ye, Xiong [1 ]
Wu, Di [1 ]
Tan, Jun [1 ]
机构
[1] Department of Equipment Maintenance and Remanufacturing, Academy of Armored Force Engineering, Beijing,100072, China
来源
Surface Technology | 2017年 / 46卷 / 10期
关键词
Nickel sulfates - Surface roughness - Nickel coatings - Scanning electron microscopy - Adhesion - Aluminum oxide - Microhardness - Morphology - Nickel - Thermal shock - Microstructure - Nickel plating - Surface morphology - Sodium compounds - Phosphorus compounds - Field emission microscopes;
D O I
10.16490/j.cnki.issn.1001-3660.2017.10.018
中图分类号
学科分类号
摘要
The work aims to study the effects of plating time on surface morphology, microstructure, microhardness, surface roughness and adhesion of electroless nickel plating on alumina. Plating bath composition and process parameters were as follows: NiSO4-6H2O 25 g/L, NaH2PO2H2O 22 g/L, Na3C6H5O7 · 2H2O 64 g/L, (NH4)SO4 62 g/L, pH=5.0~6.0, heating in water bath to 90 °C and plating time 1-4 h. Surface morphology of the coatings was observed by using NovaNanoSEM50 field emission scanning electron microscopy (SEM), hardness by TH765 automatic microhardness tester, surface roughness by OLS4000 3D measurement instrument and adhesion strength by thermal shock test and in indentation method. Provided with plating time of 1-4 h, the coatings exhibited good metallic glossiness and looked silvery white after 1 h, the coating was more delicate after 4 h, but the surface gloss was poor. As the deposition time prolonged, the smoother surface of nickel plating on A1203 was, the higher its microhardness would be; the electroless coatings were free from blistering, flaking or with separation from alumina matrix. Provided with the plating time of 1~4 h, unchanged temperature and pH, as the plating time prolongs, the thickness of coatings changes slightly, the coating grains are finer, microhardness increases obviously and surface roughness reduces. Also, the coating exhibits good adhesion to substrate. © 2017, Chongqing Wujiu Periodicals Press. All right reserved.
引用
收藏
页码:128 / 134
相关论文
共 50 条
  • [21] Investigation of electrochemical nature of induction process of electroless nickel plating
    Hu, Maopu
    Wang, Baojue
    Shen, Zhuoshen
    Pan, Jinxing
    Shen, Rongfu
    Huang, Zixun
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 1998, 8 (04): : 673 - 677
  • [22] Electroless nickel plating on alumina ceramic activated by metallic nickel as electrocatalyst for oxygen evolution reaction
    Zhang, Pingping
    Lv, Zunhang
    Liu, Xuguang
    Xie, Guangwen
    Zhang, Baoquan
    CATALYSIS COMMUNICATIONS, 2021, 149
  • [23] LOW TEMPERATURE AUTOCATALYTIC (ELECTROLESS) NICKEL PLATING PROCESS.
    John, S.
    Shanmugham, N.V.
    Shenoi, B.A.
    Metal Finishing, 1982, 80 (04) : 47 - 52
  • [24] Bath and deposit monitoring system for electroless nickel plating process
    Tenno, Robert
    Kantola, Kalle
    PROCEEDINGS OF THE 9TH WSEAS INTERNATIONAL CONFERENCE ON AUTOMATIC CONTROL, MODELING & SIMULATION, 2007, : 58 - +
  • [25] EFFECT OF ULTRAVIOLET IRRADIATION ON ELECTROLESS PLATING PROCESS OF NICKEL.
    Nakamichi, Ichiro
    Ishikawa, Yutaka
    Hirose, Yoichi
    Japanese Journal of Applied Physics, Part 2: Letters, 1987, 26 (04): : 228 - 230
  • [26] Pure nickel coating on a mesoporous alumina membrane: Preparation by electroless plating and characterization
    Haag, Stephane
    Burgard, Michel
    Ernst, Barbara
    SURFACE & COATINGS TECHNOLOGY, 2006, 201 (06): : 2166 - 2173
  • [27] ELECTROLESS NICKEL PLATING ON SILICON
    IWASA, H
    YOKOZAWA, M
    TERAMOTO, I
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1968, 115 (05) : 485 - &
  • [28] Electroless Nickel Plating – A Review
    C. A. Loto
    Silicon, 2016, 8 : 177 - 186
  • [29] CHEMICAL (ELECTROLESS) NICKEL PLATING
    ALBERTH, W
    GALVANOTECHNIK, 1979, 70 (06): : 502 - 505
  • [30] Electroless nickel plating of diamond
    Tong, Kui
    Xu, Enxia
    Xin, Rongsheng
    Pan, Yuehong
    Cailiao Baohu/Materials Protection, 2000, 33 (02): : 19 - 20