Corrosion behavior of arc welded joints of chassis parts and an approach to improve its corrosion resistance

被引:0
作者
Yamamoto S. [1 ]
Suzuki S. [1 ]
Ando S. [1 ]
Ikeda R. [1 ]
Kataoka T. [1 ,2 ]
机构
[1] JFE Steel Corporation, Japan
[2] JFE Techno-Research Corporation, Japan
来源
Yosetsu Gakkai Ronbunshu/Quarterly Journal of the Japan Welding Society | 2018年 / 36卷 / 01期
关键词
Arc weld; Corrosion resistance; Film; Lap-fillet Weld; Rust; Slag;
D O I
10.2207/qjjws.36.77
中图分类号
学科分类号
摘要
Reducing auto body weight by use of high strength steel is an important issue. Although it is necessary to increase the strength of steel sheets for underbody parts, use of high strength steel sheets has not progressed sufficiently due to the problems of fatigue and corrosion. Corrosion of underbody parts mainly occurs in arc welded joints, but the detailed corrosion mechanism had not yet been clarified. The author investigated the corrosion behavior in arc weld by laboratory corrosion tests using Ar-20%CO2 gas shielded arc weld, and clarified the corrosion mechanism. Based on that work, Ar-5%CO2 gas shielded arc weld was applied as an approach to improve corrosion resistance. The corrosion behavior of arc welded joints was classified into three phases. In the 1st phase, rust occurred at the slag portion as a paint defect on the weld bead and toe. In the 2nd phase, under-film corrosion occurred from the weld toe. In the 3rd phase, perforation corrosion progressed at the film peeling portion near the weld toe. When Ar-5%CO2 gas shielded arc weld was applied as an improvement technique, slag generation was suppressed and as a result, corrosion resistance was improved. © 2018 Japan Welding Society. All Rights Reserved.
引用
收藏
页码:77 / 85
页数:8
相关论文
共 12 条
  • [1] Kataoka T., Ikeda R., Ueda S., Nakazawa T., Preprints of The National Meeting of JWS, 95, pp. 356-357, (2014)
  • [2] Nakazawa T., Koike M., Kogure T., Subaru Technical Review, 41, pp. 131-137, (2014)
  • [3] Takahashi M., Uchihara M., Sakoda A., Ueki M., Niisato F., Transactions of Society of Automotive Engineers of Japan, 28, 2, pp. 143-148, (1997)
  • [4] Takahashi M., Uchihara M., Sakoda A., Ueki M., Niisato F., SAE Technical Paper Series, No. 971008, pp. 187-193, (1997)
  • [5] Yamamoto S., Suzuki S., Ando S., Ikeda R., Kataoka T., Ueda S., Nakazawa T., Preprints of The National Meeting of JWS, No. 336, pp. 304-305, (2015)
  • [6] SAE International Surface Vehicle Standard: SAE J2334 “Cosmetic Corrosion Lab Test, (1998)
  • [7] Townsend H.E., Galvatech’98, pp. 659-666, (1998)
  • [8] Matsushima I., Journal of The Japan Welding Society, 60, 8, pp. 627-631, (1991)
  • [9] Matsushima I., Journal of The Japan Welding Society, 61, 2, pp. 76-81, (1992)
  • [10] Uchihara M., Takahashi M., Sakoda A., Taka T., Transactions of Society of Automotive Engineers of Japan, 28, 2, pp. 149-154, (1997)