The Effect of Solution Treatment Temperature on Hardness, Microstructure, and Corrosion Resistance of Ti-6Al-4V ELI

被引:0
|
作者
Azahra, Siti Amalina [1 ]
Damisih [1 ]
Kozin, Muhammad [1 ]
Fitriani, Diah Ayu [1 ]
Puranto, Prabowo [1 ]
Jujur, Nyoman [1 ]
Prajitno, Djoko Hadi [2 ]
Ulfah, Ika Maria [1 ]
Hanafi, Razie [3 ]
Saudi, Aghni Ulma [3 ]
Suwondo, Kusuma Putri [1 ]
Marchel, Prima [4 ]
Kamil, Muhammad Prisla [1 ]
机构
[1] Research Center for Advanced Materials, National Research and Innovation Agency (BRIN), Puspiptek Area, 224 Building, Banten, South Tangerang
[2] Research Center for Radiation Process Technology, National Research and Innovation Agency (BRIN), Puspiptek Area, 11 Building, Banten, South Tangerang
[3] School of Materials Science & Engineering, University of New South Wales, Sydney
[4] Deparment of Metallurgical Engineering, Sultan Ageng Tirtayasa University, Jl. Jendral Soedirman KM. 3 Cilegon, Banten
关键词
corrosion resistance; hardness; heat treatment; microstructure; Ti-6Al-4V ELI;
D O I
10.4028/p-7ES1Pj
中图分类号
学科分类号
摘要
Ti-6Al-4V ELI (Ti64 ELI) has been widely used as metal-based biomedical implants as it has ductility and fracture toughness that surpasses the commercial Ti-6Al-4V. Casting process is one of the most cost-effective ways to produce near-net-shape Ti64 ELI implants. Nevertheless, previous study has found that grain coarsening occurred in an as-cast Ti64 ELI, which lowered its mechanical properties. To improve the properties, in this work, the samples were heat-treated in three different temperatures that varied above and below β-transus temperature for 30 minutes and then waterquenched. Following the solution treatment, each sample was artificially aged in 500 °C for four hours and left cooled inside the furnace. Hardness Vickers, microstructure, and XRD analyses were conducted to determine the effect of solution treatment regarding to its phase and properties. The result of microstructure observation showed transformation in different temperatures. The highest result of hardness value was obtained in the solution treatment variation of 1050 °C, which was 474 HVN. The XRD pattern showed that the intensity of the α/α’ phase of temperatures 850 °C, 950 °C, and 1050 °C were 92.84%, 72.65%, and 86.78%, respectively, with the intensity of the β phase were 7.16%, 27.35%, and 13.22%. The corrosion resistance performance was measured by the potentiodynamic polarization method using Ringer’s solution with pH±7,4 and the best corrosion resistance result was 0.093 mmpy in variation 950 °C as β phase was predominantly appeared in this temperature. © 2024 Trans Tech Publications Ltd, Switzerland.
引用
收藏
页码:3 / 11
页数:8
相关论文
共 50 条
  • [1] Impact of Cryogenic Treatment on Mechanical Behavior and Microstructure of Ti-6Al-4V ELI Biomaterial
    Singla, Anil Kumar
    Singh, Jagtar
    Sharma, Vishal S.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (10) : 5931 - 5945
  • [2] Impact of Cryogenic Treatment on Mechanical Behavior and Microstructure of Ti-6Al-4V ELI Biomaterial
    Anil Kumar Singla
    Jagtar Singh
    Vishal S. Sharma
    Journal of Materials Engineering and Performance, 2019, 28 : 5931 - 5945
  • [3] Effect of heat treatment on mechanical properties of Ti-6Al-4V ELI alloy
    Venkatesh, B. D.
    Chen, D. L.
    Bhole, S. D.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 506 (1-2): : 117 - 124
  • [4] Effect of Heat Treatment on Microstructure and Mechanical Properties of Ti-6Al-4V ELI Alloy Plate
    Lei Wenguang
    Mao Xiaonan
    Yu Lanlan
    Lin Hai
    TI-2011: PROCEEDINGS OF THE 12TH WORLD CONFERENCE ON TITANIUM, VOL II, 2012, : 1038 - 1041
  • [5] Characteristics Microstructure and Microhardness of Cast Ti-6Al-4V ELI for Biomedical Application Submitted to Solution Treatment
    Damisih
    Jujur, I. Nyoman
    Sah, Joni
    Agustanhakri
    Prajitno, Djoko Hadi
    METALLURGY AND ADVANCED MATERIAL TECHNOLOGY FOR SUSTAINABLE DEVELOPMENT, 2018, 1964
  • [6] Effect of Plastic Deformation and Acidic Solution on the Corrosion Behavior of Ti-6Al-4V ELI Titanium Alloy
    Zheng, Xuyong
    Xu, Chen
    Cai, Yi
    Zhang, Binbin
    METALS, 2023, 13 (10)
  • [7] Effect of Cooling Rate on Microstructure and Hardness during Solution Treatment and Aging Process of Ti-6Al-4V Alloy for Aerospace Components
    Seo, Seongji
    Choi, Hojoon
    Lee, Geeyoung
    Lee, Kee-Ahn
    Han, Jeongho
    Jung, Minsu
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2021, 30 (05) : 3406 - 3415
  • [8] Effect of Cooling Rate on Microstructure and Hardness during Solution Treatment and Aging Process of Ti-6Al-4V Alloy for Aerospace Components
    Seongji Seo
    Hojoon Choi
    Geeyoung Lee
    Kee-Ahn Lee
    Jeongho Han
    Minsu Jung
    Journal of Materials Engineering and Performance, 2021, 30 : 3406 - 3415
  • [9] The Study on Corrosion Resistance of Ti-6Al-4V ELI Alloy with Varying Surface Roughness in Hydrofluoric Acid Solution
    Wang, Han
    Cheng, Quanshi
    Chang, Zhuo
    Wang, Kedi
    Gao, Xuemin
    Fan, Xueling
    METALS, 2024, 14 (03)
  • [10] Effect of heat treatment on the corrosion resistance behavior of selective laser melted Ti6Al4V ELI
    Yan, Xingchen
    Shi, Chunbao
    Liu, Taikai
    Ye, Yun
    Chang, Cheng
    Ma, Wenyou
    Deng, Chunming
    Yin, Shuo
    Liao, Hanlin
    Liu, Min
    SURFACE & COATINGS TECHNOLOGY, 2020, 396