共 19 条
[1]
Klyapitsyn V.A., Black V.A., Goliaev V.I., Butt welding of thin strips with a non-consumable electrode, Svarochnoe Proizvodstvo, (1970)
[2]
Kulikov F.R., Bulin A.I., Frolov N.G., Mechanised argon-shielded arc spot welding of SN-2 stainless steel and OT titanium alloy, Svarochnoe Proizvodstvo, pp. 16-19, (1964)
[3]
Suzdalev I.V., Berezovsky B.M., Prokhorov V.K., Effect of the welding conditions on the shape and dimensions of the crater of the weld pool and the thickness of the interlayer below the arc, Svarochnoe Proizvodstvo, pp. 35-36, (1988)
[4]
Erokin A.A., Bucaram V.A., Ishchenko Y., The effect of the geometry of the tungsten cathode on some characteristics of the welding arc and penetration of metal, Svarochnoe Proizvodstvo, pp. 17-19, (1971)
[5]
Selyanenkov V.N., Stepanov V.V., Sayfiev R.W., Dependence of the pressure of the welding arc on the parameters of the tungsten electrode, Svarochnoe Proizvodstvo, pp. 5-6, (1980)
[6]
Eroshenko L.E., Mechev V.S., Effect of melting of the tungsten electrode on the parameters of the arc discharge in argon, Avtomaticheskaia Svarka, pp. 71-72, (1975)
[7]
Vinogradov V.A., Guma V.V., Romanenkov E.I., The effect of the parameters of the welding conditions on the temperature of the arc in argon and the methods of measuring this temperature, Svarochnoe Proizvodstvo, pp. 13-15, (1976)
[8]
Mechev V.S., Eroshenko L.E., Effect of the tip angle of a non-consumable electrode on the parameters of the electric arc in argon-shielded welding, Svarochnoe Proizvodstvo, pp. 4-7, (1976)
[9]
Russo V.L., Suzdalev I.V., Yavno E.I., Effect of arc voltage and the tip angle geometry of the non-consumable electrode on the force effect of the arc, Svarochnoe Proizvodstvo, pp. 6-8, (1977)
[10]
Gvozdetskii V.S., Function of the distribution of the current density in the anode spot of the arc, Avtomaticheskaia Svarka, pp. 20-24, (1973)