Enhanced Air Stability and High Li-Ion Conductivity of Li6.988P2.994Nb0.2S10.934O0.6 Glass-Ceramic Electrolyte for All-Solid-State Lithium-Sulfur Batteries

被引:0
|
作者
Ahmad, Niaz [1 ]
Zhou, Lei [1 ]
Faheem, Muhammad [1 ]
Tufail, Muhammad Khurram [1 ]
Yang, Le [1 ]
Chen, Renjie [2 ]
Zhou, Yaodan [1 ]
Yang, Wen [1 ]
机构
[1] Key Lab. of Cluster Sci. of Min. of Educ. Beijing Key Lab. of Photoelectronic/Electrophotonic Conversion Mat., School of Chemistry and Chemical Engineering, Beijing Institute of Technology, 5# Zhongguancun Road, Haidian District, Beijing,100081, China
[2] School of Material Science and Engineering, Beijing Institute of Technology, Beijing,100081, China
来源
ACS Applied Materials and Interfaces | 2020年 / 12卷 / 19期
关键词
The development of novel sulfide solid-state electrolytes with high Li-ion conductivity; excellent air-stability; and a stable electrode-electrolyte interface is needed for the commercialization of all-solid-state cells. Currently; an ideal solid electrolyte; which can integrate the solid-state batteries; has not been developed. Herein; the Nb and O codoping strategy is excogitated to improve the chemical and electrochemical performance of sulfide electrolytes. The interactive effect of Nb and O in the novel Li6.988P2.994Nb0.2S10.934O0.6 glass-ceramic electrolyte results in a superior Li+ conductivity of 2.82 mS cm-1 and remarkable air-stability and electrochemical stability against the Li metal compared to the Li7P3S11 counterpart at 25 °C. Solid-state 31P MAS-NMR revealed that doping of LiNbO3 (0 ≤ x ≤ 1) not only enhances the degree of crystallization but also produces P2OS64- units with bridging oxygen atoms in the Li6.988P2.994Nb0.2S10.934O0.6 glass-ceramic electrolyte and hence boosts the conductive deportment of glass-ceramics. Impressively; the developed electrolyte exhibits a stable full voltage window of up to 5 V versus Li/Li+. Furthermore; electrochemical impedance spectroscopy analysis shows that the interface resistance of the Li2S/Li6.988P2.994Nb0.2S10.934O0.6/Li-In cell is lower than that of the cell with Li7P3S11 electrolyte. Besides; the battery of the Li6.988P2.994Nb0.2S10.934O0.6 electrolyte delivers initial discharge capacities of 472.7 and 530.9 mAh g-1 after 50 cycles with 98.88% capacity retention from the second cycle. The Coulombic efficiency of the cell remains at ∼100% after 50 cycles. Thus; the proposed codoped strategy produced a sulfide electrolyte; which addressed the challenging issues of chemical/electrochemical stabilities and showed promising industrial prospects for next-generation all-solid-state batteries. Copyright © 2020 American Chemical Society;
D O I
暂无
中图分类号
学科分类号
摘要
引用
收藏
页码:21548 / 21558
相关论文
共 50 条
  • [1] Enhanced Air Stability and High Li-Ion Conductivity of Li6.988P2.994Nb0.2S10.934O0.6 Glass-Ceramic Electrolyte for All-Solid-State Lithium-Sulfur Batteries
    Ahmad, Niaz
    Zhou, Lei
    Faheem, Muhammad
    Tufail, Muhammad Khurram
    Yang, Le
    Chen, Renjie
    Zhou, Yaodan
    Yang, Wen
    ACS APPLIED MATERIALS & INTERFACES, 2020, 12 (19) : 21548 - 21558
  • [2] Metal-phosphide-doped Li7P3S11 glass-ceramic electrolyte with high ionic conductivity for all-solid-state lithium-sulfur batteries
    Ge, Qi
    Zhou, Lei
    Lian, Yi-meng
    Zhang, Xiaoling
    Chen, Renjie
    Yang, Wen
    ELECTROCHEMISTRY COMMUNICATIONS, 2018, 97 : 100 - 104
  • [3] Synthesis and Electrochemical Characterization of a Glass-Ceramic Li7P2S8I Solid Electrolyte for All-Solid-State Li-Ion Batteries
    Choi, Seon-Joo
    Lee, Sang-Hun
    Ha, Yoon-Cheol
    Yu, Ji-Hyun
    Doh, Chil-Hoon
    Lee, Youjin
    Park, Jun-Woo
    Lee, Sang-Min
    Shin, Heon-Cheol
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2018, 165 (05) : A957 - A962
  • [4] Slurry-Processed Glass-Ceramic LI2S-P2S5-LiI Electrolyte for All-Solid-State Li-Ion Batteries
    Choi, S. J.
    Lee, S. H.
    Yu, J. H.
    Doh, C. H.
    Ha, Y. C.
    BATTERY ELECTROLYTES, 2017, 77 (01): : 65 - 70
  • [5] Lithium Argyrodite Sulfide Electrolytes with High Ionic Conductivity and Air Stability for All-Solid-State Li-Ion Batteries
    Lee, Yongheum
    Jeong, Jiwon
    Lee, Ho Jun
    Kim, Mingony
    Han, Daseul
    Kim, Hyoungchul
    Yuk, Jong Min
    Nam, Kyung-Wan
    Chung, Kyung Yoon
    Jung, Hun-Gi
    Yu, Seungho
    ACS ENERGY LETTERS, 2022, 7 (01): : 171 - 179
  • [6] Tailored Li2S-P2S5 glass-ceramic electrolyte by MoS2 doping, possessing high ionic conductivity for all-solid-state lithium-sulfur batteries
    Xu, Ruo-chen
    Xia, Xin-hui
    Wang, Xiu-li
    Xia, Yan
    Tu, Jiang-ping
    JOURNAL OF MATERIALS CHEMISTRY A, 2017, 5 (06) : 2829 - 2834
  • [7] Recent Progress in All-Solid-State Lithium-Sulfur Batteries Using High Li-Ion Conductive Solid Electrolytes
    Umeshbabu, Ediga
    Zheng, Bizhu
    Yang, Yong
    ELECTROCHEMICAL ENERGY REVIEWS, 2019, 2 (02) : 199 - 230
  • [8] Oxygenated Li3PS4 electrolyte with improved conductivity and air stability for all-solid-state Li-ion batteries
    Narsimulu, D.
    Subramanian, Yuvaraj
    Rajagopal, Rajesh
    Ryu, Kwang-Sun
    ELECTROCHIMICA ACTA, 2025, 511
  • [9] Enhanced Li-Ion Conductivity and Air Stability of Sb-Substituted Li4GeS4 toward All-Solid-State Li-Ion Batteries
    Roh, Jihun
    Lyoo, Jeyne
    Hong, Seung-Tae
    ACS APPLIED ENERGY MATERIALS, 2023, 6 (10) : 5446 - 5455
  • [10] Congener Substitution Reinforced Li7P2.9Sb0.1S10.75O0.25 Glass-Ceramic Electrolytes for All-Solid-State Lithium-Sulfur Batteries
    Zhao, Bo-Sheng
    Wang, Lu
    Chen, Peng
    Liu, Sheng
    Li, Guo-Ran
    Xu, Ning
    Wu, Meng-Tao
    Gao, Xue-Ping
    ACS APPLIED MATERIALS & INTERFACES, 2021, 13 (29) : 34477 - 34485