Comprehensive extraction of V, Ni and Mo from black shale via selective leaching oxidation process

被引:0
|
作者
Li, Kailin [1 ,2 ,3 ,4 ]
Huang, Jing [1 ,2 ,3 ,4 ]
Zhang, Yimin [1 ,2 ,3 ,4 ]
Hu, Pengcheng [1 ,2 ,3 ,4 ]
Li, Sheng [1 ,2 ,3 ,4 ]
Xiang, Shuwen [1 ,2 ,3 ,4 ]
机构
[1] Wuhan Univ Sci & Technol, Sch Resource & Environm Engn, Wuhan 430081, Hubei Province, Peoples R China
[2] State Environm Protect Key Lab Mineral Met Resourc, Wuhan 430081, Hubei Province, Peoples R China
[3] Collaborat Innovat Ctr Strateg Vanadium Resources, Wuhan 430081, Hubei Province, Peoples R China
[4] Hubei Prov Engn Technol Res Ctr High Efficient Cle, Wuhan 430081, Hubei Province, Peoples R China
来源
JOURNAL OF ENVIRONMENTAL CHEMICAL ENGINEERING | 2024年 / 12卷 / 06期
关键词
Black shale; Vanadium; Nickel; Molybdenum; Stepwise leaching oxidation; STONE COAL; VANADIUM; NICKEL;
D O I
10.1016/j.jece.2024.114581
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Black shale is one of the most representative sources of vanadium, nickel and molybdenum in China. Due to the poor endowment of minerals in black shale, V, Ni, Mo and other metals complex co-associated endowment state, extraction is difficult and long-term unused, resulting in a significant waste of resources. In this paper, it is shown that V, Ni and Mo can be obtained from black shale by a stepwise oxidation leaching process. In a first leaching process, V and Ni are effectively leached simultaneously. Mo is left in the residue. The leaching efficiency of V, Ni and Mo was 86.81 %, 89.19 % and 5.80 % respectively under the leaching conditions of 35 wt% H2SO4, 4 wt% CaF2, 1.2:1 liquid to solid ratio (L/kg), 95 degrees C and 8 h. The residue was then leached twice. The leaching efficiency of molybdenum was 91.10 % under the leaching conditions of 25 wt% H2SO4, 8 wt% NaClO3, 1.5:1 liquid to solid ratio (L/kg), 45 degrees C and 7 h. V2O5 products have been successfully prepared, the purity of V2O5 reaches 98.34 %. A stepwise oxidation leaching method has been proposed to separate the vanadium, nickel and molybdenum in the leaching process. Vanadium, nickel and molybdenum can be effectively extracted from the black shale by the stepwise oxidation leaching process to maximize the utilization of the resources.
引用
收藏
页数:15
相关论文
共 50 条
  • [1] Acid Leaching Extraction of Mo, V, and Ni Compounds from the Semicoking Product of Tar Hydroconversion Residue
    Kadiev, Kh. M.
    Visaliev, M. Ya.
    Zekel', L. A.
    Shpirt, M. Ya.
    SOLID FUEL CHEMISTRY, 2018, 52 (06) : 392 - 395
  • [2] Acid Leaching Extraction of Mo, V, and Ni Compounds from the Semicoking Product of Tar Hydroconversion Residue
    Kh. M. Kadiev
    M. Ya. Visaliev
    L. A. Zekel’
    M. Ya. Shpirt
    Solid Fuel Chemistry, 2018, 52 : 392 - 395
  • [3] Comprehensive recovery of Ca, V, Zn, and Si from black shale using a novel hydrochloric acid selective leaching-decarburization process
    Liu, Hong
    Zhang, Yi-min
    Hu, Peng-cheng
    Liu, Tao
    Huang, Jing
    SEPARATION AND PURIFICATION TECHNOLOGY, 2023, 304
  • [4] Vanadium extraction from black shale: Enhanced leaching due to fluoride addition
    Zheng, Qiushi
    Zhang, Yimin
    Liu, Tao
    Huang, Jing
    Xue, Nannan
    HYDROMETALLURGY, 2019, 187 : 141 - 148
  • [5] Green and selective recovery process of Mo, V, and Ni from spent hydrodesulfurization catalysts via novel ionic liquids and deep eutectic solvents technology
    Abbas, Zaheer
    Jung, Simon MoonGeun
    DYES AND PIGMENTS, 2024, 346
  • [6] Extraction of vanadium from black shale using pressure acid leaching
    Li, Minting
    Wei, Chang
    Fan, Gang
    Li, Cunxiong
    Deng, Zhigan
    Li, Xingbin
    HYDROMETALLURGY, 2009, 98 (3-4) : 308 - 313
  • [7] Organic acid-mediated leaching kinetics study and selective extraction of Mo, V, and Ni from spent catalysts
    Gao, Jing
    Lu, Wenchao
    Li, Yujiang
    Wu, Tao
    WASTE MANAGEMENT, 2024, 187 : 198 - 206
  • [8] Leaching Mo and Ni by Direct Oxygen Pressure from Black Shale with any other only water
    Deng Zhi-gan
    Wei Chang
    Li Xing-bin
    Li Cun-xiong
    Fan Gang
    PROCEEDINGS OF THE 2015 4TH INTERNATIONAL CONFERENCE ON SUSTAINABLE ENERGY AND ENVIRONMENTAL ENGINEERING, 2016, 53 : 527 - 532
  • [9] The role of CaO in the extraction of Ni and Mo from carbonaceous shale by calcification roasting, sulphation roasting and water leaching
    Wang, Xue-Wen
    Peng, Jun
    Wang, Ming-Yu
    Ye, Pu-Hong
    Xiao, Yuan
    INTERNATIONAL JOURNAL OF MINERAL PROCESSING, 2011, 100 (3-4) : 130 - 135
  • [10] Selective extraction of Mo from a Ni-Mo ore using pressure alkaline leaching
    Wang, Mingshuang
    Wei, Chang
    Fan, Gang
    Li, Minting
    Deng, Zhigan
    Wang, Sifu
    HYDROMETALLURGY, 2015, 153 : 6 - 11