Study on the material flow behavior, microstructure evolution and strengthening mechanism of arc-assisted friction stir weld of Ti6321 alloy

被引:1
|
作者
Sun, Guangda [1 ,2 ]
Zhou, Li [1 ,2 ]
Li, Yuxuan [2 ]
Yan, Zhongxian [2 ]
Song, Xiaoguo [1 ,2 ]
Gao, Fuyang [3 ]
Liu, Xiangqian [3 ]
Liao, Zhiqian [3 ]
机构
[1] Harbin Inst Technol, State Key Lab Precis Welding & Joining Mat & Struc, Harbin 150001, Peoples R China
[2] Harbin Inst Technol Weihai, Shandong Prov Key Lab Special Welding Technol, Weihai 264209, Peoples R China
[3] Luoyang Ship Mat Res Inst, Luoyang 471000, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2024年 / 918卷
关键词
Ti6321; alloy; Arc assisted friction stir welding; Defect suppression; Microstructural evolution; Failure mechanism; TITANIUM-ALLOY; ALPHA-TITANIUM; JOINT; TRANSFORMATION; DEFORMATION; STRESS; PHASE; ZONE;
D O I
10.1016/j.msea.2024.147455
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, 6 mm thick Ti6321 alloy plates were butt welded using conventional friction stir welding (FSW) and arc-assisted friction stir welding (AAFSW). The defect formation and suppression, microstructure evolution, and plastic deformation and failure mechanisms of the joints were systematically studied. The results showed that a defect-free joint could be achieved with a significant reduction of 50 % in both axial and forward forces for AAFSW. The formation of the bottom defect was attributed to the non-convergence of vertical flow components and the circumferential flow along the pin. The applied arc enhances the material flow along the thickness direction, thereby promoting the transformation of the microstructure at the bottom of the stir zone (SZ) from a bimodal structure to a fully lamellar structure. Texture analysis reveals a shift from B and Y2 to C1 components with increased heat input and strain. Plastic deformation in the SZ is primarily dominated by slip, accompanied by twinning deformation in both joints. And the mechanism involving dislocation decomposition and stacking fault formation leading to dynamic phase transformations has been further confirmed. The AAFSW joint exhibits a more uniform hardness distribution and higher joint efficiency (96 %) with an average ultimate tensile strength (UTS) of 771 MPa and an elongation of 7.8 %. The joint failure mechanism is influenced by microhardness and uncoordinated plastic deformation arising from dislocation slip and twinning effects along the thickness. These insights confirm that AAFSW is a new choice for achieving efficient and high-quality connections in medium- thick Ti alloys.
引用
收藏
页数:19
相关论文
共 13 条
  • [1] Microstructure evolution of friction stir welding of Ti6321 titanium alloy based on the weld temperature below microstructure transformation temperature
    Gao, Fuyang
    Guo, Yufan
    Yu, Wei
    Jiang, Peng
    Liao, Zhiqian
    MATERIALS CHARACTERIZATION, 2021, 177
  • [2] Mechanism Study on Microstructure and Properties of Ti6321 Alloy Welding by Transverse Magnetic Field
    Ding, Laifa
    Zhang, Zheng
    Zeng, Zhibin
    Qin, Binhao
    Vladyslav, Khaskin
    Chen, Lijia
    Zhang, Yupeng
    Wang, Haiyan
    METALS AND MATERIALS INTERNATIONAL, 2025,
  • [3] Additive friction stir deposition of Al-Ce alloy:Microstructure evolution, strengthening and fracture mechanism
    Hu, Jinbing
    He, Wenjie
    Wan, Yuting
    Qi, Liang
    Chen, Jiqiang
    Guo, Xunzhong
    Ye, Jieyun
    Zhao, Hongjin
    Liang, Xiaoxia
    Lv, Wancheng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1017
  • [4] Recrystallization behavior and strengthening mechanism of friction stir welded T-joint of Ti80 titanium alloy
    Su, Yu
    Yang, Xiawei
    Zhao, Wenwei
    Gao, Fuyang
    Ma, Shitong
    Meng, Tingxi
    Yin, Shuo
    Li, Wenya
    MATERIALS CHARACTERIZATION, 2024, 216
  • [5] Microstructure evolution and strengthening mechanism of friction stir welded joint of 20 mm-thick AZ31 magnesium alloy
    Liu, Qiang
    Wang, Wen
    Peng, Pai
    Zhang, Ting
    Han, Peng
    Guan, Xiao-hu
    Wang, Zhi
    Qiao, Ke
    Cai, Jun
    Wang, Kuai-she
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2023, 33 (11) : 3295 - 3308
  • [6] Study on the materials flow, microstructure and mechanical properties of ultrasonic vibration-assisted friction stir weld of 1500 MPa martensitic steel
    Zhu, Shuhao
    Wang, Naiqian
    Li, Shuai
    Huang, Guan
    Ge, Shang
    Du, Peihua
    Zhang, Li
    Sun, Yufeng
    Guan, Shaokang
    MATERIALS CHARACTERIZATION, 2023, 206
  • [7] Investigation of material flow, microstructure evolution, and texture development in dissimilar friction stir welding of Al6061 to Ti6Al4V
    Sundar, Saravana A.
    Kumar, Adepu
    Mugada, Krishna Kishore
    MATERIALS TODAY COMMUNICATIONS, 2022, 33
  • [9] Numerical simulation of effect of rotational tool with screw on material flow behavior of friction stir welding of Ti6Al4V alloy
    Ji, Shude
    Zou, Aili
    Yue, Yumei
    Luan, Guohong
    Jin, Yanye
    Li, Fu
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2012, 25 (05) : 365 - 373
  • [10] Study of microstructure evolution and mechanical properties in friction stir based additive multi-layer manufacturing of Al 6061 alloy: Effect of feedstock material form and heat treatment
    Chaudhary, Bhavesh
    Jain, Neelesh Kumar
    Murugesan, Jayaprakash
    Sathiaraj, Dan
    MATERIALS TODAY COMMUNICATIONS, 2023, 34