Electrochemical behavior of Sn-9Zn-xCu solder alloy in 3.5 wt% NaCl solution at room temperature

被引:0
作者
Jaiswal, Dheeraj [1 ]
Kumar, Sharvan [1 ,2 ]
Behera, C.K. [1 ]
机构
[1] Department of Metallurgical Engineering, Indian Institute of Technology (BHU), Varanasi,221005, India
[2] Department of Metallurgical Engineering and Material Sciences, IIT Bombay, Maharashtra, India
来源
Materials Today Communications | 2022年 / 33卷
关键词
D O I
暂无
中图分类号
学科分类号
摘要
58
引用
收藏
相关论文
共 50 条
[21]   The electrochemical corrosion behavior of Pb-free Sn-8.5Zn-XCr solders in 3.5 wt.% NaCl solution [J].
Liu, Moumiao ;
Yang, Wenchao ;
Ma, Yueyuan ;
Tang, Chenghuang ;
Tang, Hongqun ;
Zhan, Yongzhong .
MATERIALS CHEMISTRY AND PHYSICS, 2015, 168 :27-34
[22]   Effect of bismuth and silver on the corrosion behavior of Sn-9Zn alloy in NaCl 3 wt.% solution [J].
Ahmido, A. ;
Sabbar, A. ;
Zouihri, H. ;
Dakhsi, K. ;
Guedira, F. ;
Serghini-Idrissi, M. ;
El Hajjaji, S. .
MATERIALS SCIENCE AND ENGINEERING B-ADVANCED FUNCTIONAL SOLID-STATE MATERIALS, 2011, 176 (13) :1032-1036
[23]   Electrochemical behavior of a lead-free Sn-Cu solder alloy in NaCl solution [J].
Osorio, Wislei R. ;
Freitas, Emmanuelle S. ;
Spinelli, Jose E. ;
Garcia, Amauri .
CORROSION SCIENCE, 2014, 80 :71-81
[24]   Electrochemical Migration Investigation on Lead-Free Sn-based Solder Alloys in 3.5 wt.% NaCl Solution [J].
Gharaibeh, Ali ;
Rigler, Daniel ;
Medgyes, Balint ;
Harsanyi, Gabor .
2022 45TH INTERNATIONAL SPRING SEMINAR ON ELECTRONICS TECHNOLOGY (ISSE), 2022,
[25]   Corrosion Behavior of New Cu-Sn-Fe-Ni Alloy in 3.5wt% NaCl Solution [J].
Xie, Wang ;
Qian, Lei ;
Yong, Liu .
RARE METAL MATERIALS AND ENGINEERING, 2023, 52 (11) :3893-3899
[26]   Microstructure and adhesion strength of Sn-9Zn-1.5Ag-xBi (x=0 wt% and 2 wt%)/Cu after electrochemical polarization in a 3.5 wt% NaCl solution [J].
Li, Wang-Long ;
Chen, Ying-Ru ;
Chang, Kuo-Ming ;
Liu, Chih-Yao ;
Hon, Min-Hsiung ;
Wang, Moo-Chin .
JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 461 (1-2) :160-165
[27]   Microstructure and adhesion strength of Sn-9Zn-1.5Ag-xBi (x = 0 wt% and 2 wt%)/Cu after electrochemical polarization in a 3.5 wt% NaCl solution [J].
Department of Mechanical Engineering, National Kaohsiung University of Applied Sciences, 415 Chien-Kung Road, Kaohsiung, 80782, Taiwan ;
不详 ;
不详 ;
不详 .
Journal of Alloys and Compounds, 2008, 461 (1-2) :160-165
[28]   Corrosion behavior of Mge5Al based magnesium alloy with 1 wt.% Sn, Mn and Zn additions in 3.5 wt.% NaCl solution [J].
Nguyen Dang Nam .
JOURNAL OF MAGNESIUM AND ALLOYS, 2014, 2 (02) :190-195
[29]   Electrochemical corrosion behaviour and corrosion mechanism of Sn-9Zn-xGe solder alloys in NaCl solution [J].
Pu, Cunji ;
Li, Caiju ;
Miao, Yingde ;
Lu, Qiong ;
Peng, Jubo ;
Xu, Zunyan ;
Zhang, Xin ;
Yi, Jianhong .
CORROSION SCIENCE, 2024, 228
[30]   Electrochemical Corrosion Behaviour of Sn-8Zn-3Bi-XCr Solder in 3.5% NaCl [J].
Hu, Jing ;
Hu, Anmin ;
Li, Ming ;
Mao, Dali .
2009 INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY & HIGH DENSITY PACKAGING (ICEPT-HDP 2009), 2009, :625-631