Aluminum incorporation into 4H-SiC layers during epitaxial growth in a hot-wall CVD system

被引:0
|
作者
Wagner, G. [1 ]
Leitenberger, W. [1 ]
Irmscher, K. [1 ]
Schmid, F. [2 ]
Laube, M. [2 ]
Pensl, G. [2 ]
机构
[1] Institute of Crystal Growth, Max-Born-Str. 2, DE-12489 Berlin, Germany
[2] Institute of Applied Physics, University of Erlangen-Nürnberg, DE-91058 Erlangen, Germany
关键词
Aluminum - Carrier concentration - Chemical vapor deposition - Concentration (process) - Epilayers - Silicon carbide;
D O I
10.4028/www.scientific.net/msf.389-393.207
中图分类号
学科分类号
摘要
Experimental results are presented for aluminium incorporation in Si-face 4H-SiC epilayers grown in a hot-wall reactor by chemical vapour deposition (CVD). Epitaxial growth was performed using silane and propane as process gases, and trimethylaluminium (TMA) as the doping source. The incorporation of aluminium has been studied in the concentration range from 3×10 14 cm-3 to 2×1018 cm-3. In addition, the influence of growth rate on the carrier concentration in the epilayers is studied. © 2002 Trans Tech Publications.
引用
收藏
页码:207 / 210
相关论文
共 50 条
  • [41] Hot-wall CVD growth of 4H-SiC using Si2Cl6+C 3H8+H2 system
    Miyanagi, Toshiyuki
    Nishino, Shigehiro
    Materials Science Forum, 2002, 389-393 (01) : 199 - 202
  • [42] EPITAXIAL-GROWTH OF SILICON BY CVD IN A HOT-WALL FURNACE
    BLOEM, J
    OEI, YS
    DEMOOR, HHC
    HANSSEN, JHL
    GILING, LJ
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1985, 132 (08) : 1973 - 1980
  • [43] Highly uniform epitaxial SiC-layers grown in a hot-wall CVD reactor with mechanical rotation
    Schöner, A
    Konstantinov, A
    Karlsson, S
    Berge, R
    SILICON CARBIDE AND RELATED MATERIALS 2001, PTS 1 AND 2, PROCEEDINGS, 2002, 389-3 : 187 - 190
  • [44] Growth characteristics of SiC in a hot-wall CVD reactor with rotation
    Zhang, J.
    Forsberg, U.
    Isacson, M.
    Ellison, A.
    Henry, A.
    Kordina, O.
    Janzén, E.
    Materials Science Forum, 2002, 389-393 (01) : 191 - 194
  • [45] Growth characteristics of SiC in a hot-wall CVD reactor with rotation
    Zhang, J
    Forsberg, U
    Isacson, M
    Ellison, A
    Henry, A
    Kordina, O
    Janzén, E
    SILICON CARBIDE AND RELATED MATERIALS 2001, PTS 1 AND 2, PROCEEDINGS, 2002, 389-3 : 191 - 194
  • [46] Growth characteristics of SiC in a hot-wall CVD reactor with rotation
    Zhang, J
    Forsberg, U
    Isacson, M
    Ellison, A
    Henry, A
    Kordina, O
    Janzén, E
    JOURNAL OF CRYSTAL GROWTH, 2002, 241 (04) : 431 - 438
  • [47] Effects of C/Si ratio in fast epitaxial growth of 4H-SIC(0001) by vertical hot-wall chemical vapor deposition
    Fujiwara, H
    Danno, K
    Kimoto, T
    Tojo, T
    Matsunami, H
    JOURNAL OF CRYSTAL GROWTH, 2005, 281 (2-4) : 370 - 376
  • [48] High-voltage (>2.5kV) 4H-SiC Schottky rectifiers processed on hot-wall CVD and high-temperature CVD layers
    Kimoto, T
    Wahab, Q
    Ellison, A
    Forsberg, U
    Tuominen, M
    Yakimova, R
    Henry, A
    Janzen, E
    SILICON CARBIDE, III-NITRIDES AND RELATED MATERIALS, PTS 1 AND 2, 1998, 264-2 : 921 - 924
  • [49] Gettering effect with Al implanted into 4H-SiC CVD epitaxial layers
    Kalinina, E
    Kholujanov, G
    Sitnikova, A
    Kossov, V
    Yafaev, R
    Pensl, G
    Reshanov, S
    Hallén, A
    Konstantinov, A
    SILICON CARBIDE AND RELATED MATERIALS - 2002, 2002, 433-4 : 637 - 640
  • [50] Influence of ion implantation on the quality of 4H-SiC CVD epitaxial layers
    Kalinina, E
    Kholujanov, G
    Solov'ev, V
    Strel'chuk, A
    Kossov, V
    Yafaev, R
    Kovarskii
    Shchukarev, A
    Obyden, S
    Saparin, G
    Ivannikov, P
    Hallén, A
    Konstantinov, A
    APPLIED SURFACE SCIENCE, 2001, 184 (1-4) : 323 - 329