Ni/WSi/Ti/Pt Ohmic contacts to n-SiC were investigated as a function of annealing temperatures up to 1000 °C. Annealing at temperatures between 950 and 1000 °C yielded excellent Ohmic behavior. At these temperatures the contact-SiC interface was smooth, defect free, and characterized by a narrow Ni2Si reaction region. The annealed contacts possessed atomically smooth surface morphologies and exhibited minimal contact expansion. The residual carbon, resultant from SiC decompositon and reaction with Ni to form Ni2Si, was constrained by reaction with the WSi and Ti layers forming carbide phases of W and Ti spatially distant from the metal semiconductor interface. Our results demonstrate that the Ni/WSi/Ti/Pt composite Ohmic contact maintains the desirable electrical properties associated with Ni contacts and possesses excellent interfacial, compositional, and surface properties which are required for reliable high power and high temperature device operation. © 2000 American Institute of Physics.
引用
收藏
相关论文
共 50 条
  • [31] Improved ohmic contact on n-type 4H-SiC
    Gao, Y
    Tang, Y
    Hoshi, M
    Chow, TP
    SOLID-STATE ELECTRONICS, 2000, 44 (10) : 1875 - 1878
  • [32] Accurate calculation of the specific contact resistance for Ni based Ohmic Contacts to the N-type SiC
    Guo, Hui
    Zhang, Yi-Men
    Zhang, Yu-Ming
    Tang, Xiao-Yan
    Feng, Qian
    Xi'an Dianzi Keji Daxue Xuebao/Journal of Xidian University, 2008, 35 (05): : 842 - 845
  • [33] Improved adhesion and interface ohmic contact on n-type 4H-SiC substrate by using Ni/Ti/Ni
    韩林超
    申华军
    刘可安
    王弋宇
    汤益丹
    白云
    许恒宇
    吴煜东
    刘新宇
    Journal of Semiconductors, 2014, 35 (07) : 19 - 22
  • [34] Improved adhesion and interface ohmic contact on n-type 4H-SiC substrate by using Ni/Ti/Ni
    Han Linchao
    Shen Huajun
    Liu Kean
    Wang Yiyu
    Tang Yidan
    Bai Yun
    Xu Hengyu
    Wu Yudong
    Liu Xinyu
    JOURNAL OF SEMICONDUCTORS, 2014, 35 (07)
  • [35] Improved adhesion and interface ohmic contact on n-type 4H-SiC substrate by using Ni/Ti/Ni
    韩林超
    申华军
    刘可安
    王弋宇
    汤益丹
    白云
    许恒宇
    吴煜东
    刘新宇
    Journal of Semiconductors, 2014, (07) : 19 - 22
  • [36] High energy electron radiation effect on Ni/4H-SiC SBD and Ohmic contact
    张林
    张义门
    张玉明
    韩超
    马永吉
    Chinese Physics B, 2009, 18 (08) : 3490 - 3494
  • [37] High energy electron radiation effect on Ni/4H-SiC SBD and Ohmic contact
    Zhang Lin
    Zhang Yi-Men
    Zhang Yu-Ming
    Han Chao
    Ma Yong-Ji
    CHINESE PHYSICS B, 2009, 18 (08) : 3490 - 3494
  • [38] Fabrication of Ti ohmic contact to n-type 6H-SiC without high-temperature annealing
    Chang Shao-Hui
    Liu Xue-Chao
    Huang Wei
    Xiong Ze
    Yang Jian-Hua
    Shi Er-Wei
    CHINESE PHYSICS B, 2012, 21 (09)
  • [39] Fabrication of Ti ohmic contact to n-type 6H-SiC without high-temperature annealing
    常少辉
    刘学超
    黄维
    熊泽
    杨建华
    施尔畏
    Chinese Physics B, 2012, 21 (09) : 410 - 413
  • [40] SiC devices for advanced power and high-temperature applications
    Wondrak, W
    Held, R
    Niemann, E
    Schmid, U
    IEEE TRANSACTIONS ON INDUSTRIAL ELECTRONICS, 2001, 48 (02) : 307 - 308