共 50 条
Fracture Toughness of Short Fibre-Reinforced Composites-In Vitro Study
被引:0
|作者:
Kamourieh, Noor
[1
]
Faigenblum, Maurice
[1
]
Blizard, Robert
[1
]
Leung, Albert
[1
]
Fine, Peter
[1
]
机构:
[1] UCL Eastman, Dent Inst, London WC1E 6DE, England
来源:
关键词:
short fibre-reinforced composite;
fracture toughness;
everX Posterior;
everX Flow;
glass fibres;
biomimetics;
MECHANICAL-PROPERTIES;
PHYSICAL-PROPERTIES;
RESIN;
RESTORATIONS;
LONGEVITY;
BEHAVIOR;
MOLARS;
DEPTH;
WEAR;
CURE;
D O I:
10.3390/ma17215368
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
The development of dental materials needs to be supported with sound evidence. This in vitro study aimed to measure the fracture toughness of a short fibre-reinforced composite (sFRC), at differing thicknesses. In this study, 2 mm, 3 mm and 4 mm depths of sFRC were prepared. Using ISO4049, each preparation was tested to failure. A total of 60 samples were tested: 10 samples for each combination of sFRC and depth. Fractured samples were viewed, and outcomes were analysed. EXF showed greater toughness than EXP, with a mean of 2.49 (95%CI: 2.25, 2.73) MPa.m(1/2) compared to a mean of 2.13 (95%CI: 1.95, 2.31) MPa.m(1/2), (F(1,54) = 21.28; p < 0.001). This difference was particularly pronounced at 2 mm depths where the mean (95%CI) values were 2.72 (2.49, 2.95) for EXF and 1.90 (1.78, 2.02) for EXP (Interaction F(2,54) = 7.93; p < 0.001). Both materials performed similarly at the depths of 3 mm and 4 mm. The results for both materials were within the accepted fracture toughness values of dentine of 1.79-3.08 MPa.m(1/2). Analysis showed crack deflection and bridging fibre behaviour. The optimal thickness at the cavity base for EXF was 2 mm and for EXP 4 mm. Crack deflection and bridging behaviour indicated that restorations incorporating sFRCs are not prone to catastrophic failure and confirmed that sFRCs have similar fracture toughness to dentine. sFRCs could be a suitable biomimetic material to replace dentine.