Influence of build orientation and heat treatment on high cycle fatigue of additively manufactured AlSi10Mg

被引:3
作者
Valim, Diego B. [1 ]
Avila, Julian A. [2 ]
Fonseca, Eduardo B. [1 ]
Gabriel, Andre H. G. [1 ]
Jardini, Andre L. [3 ]
Lopes, Eder S. N. [1 ]
机构
[1] Univ Estadual Campinas UNICAMP, Fac Engn Mecan, BR-13083860 Campinas, SP, Brazil
[2] Sao Paulo State Univ UNESP, Sch Engn, Ave Profa Isette Correa Fontao 505, BR-13876750 Sao Joao da Boa Vista, SP, Brazil
[3] Univ Estadual Campinas UNICAMP, Fac Engn Quim, Inst Nacl Biofabricacao, BR-13086852 Campinas, SP, Brazil
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2024年 / 916卷
基金
巴西圣保罗研究基金会;
关键词
Direct aging; Stress relief; PBF-LB; Build orientation; HCF; MECHANICAL-PROPERTIES; LASER; MICROSTRUCTURE; ALLOY; AL; EVOLUTION; PROPERTY; BEHAVIOR;
D O I
10.1016/j.msea.2024.147308
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This study examines how build orientation and heat treatment affect microstructure and, consequently, the mechanical properties in tensile and high cycle fatigue of additively manufactured AlSi10Mg. Specimens were manufactured in two orientations (0 degrees and 45 degrees) using a laser-based powder bed fusion and subsequently subjected to two heat treatments: (i) direct aging at 170 degrees C for 2 h (A170) and (ii) stress relief at 300 degrees C for 2 h (SR300). Two routes for direct aging were previously explored to determine the ideal time and temperature for heat treatment: direct aging at 155 degrees C and direct aging at 170 degrees C, both for up to 10 h. It was found that aging at 170 degrees C for 2 h resulted in higher hardness, yield strength, and ultimate tensile strength than aging at 155 degrees C for 6 h (A155). Based on the run-out specimens, the specimens subjected to heat treatment A170 exhibited similar stress amplitude at 106 fatigue strength than SR300, with 43.8 MPa and 45.6 MPa, respectively. At similar stress amplitudes, below 106 cycles, the build orientation (0 degrees and 45 degrees) slightly affect the high cycle fatigue properties.
引用
收藏
页数:10
相关论文
共 50 条
[1]   Post heat treatment of additive manufactured AlSi10Mg: On silicon morphology, texture and small-scale properties [J].
Alghamdi, F. ;
Song, X. ;
Hadadzadeh, A. ;
Shalchi-Amirkhiz, B. ;
Mohammadi, M. ;
Haghshenas, M. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 783
[2]  
AMERICAN SOCIETY FOR TESTING AND MATERIALS, 2016, ASTM E1479-16
[3]  
AMERICAN SOCIETY FOR TESTING AND MATERIALS, 2019, ASTM 52921 - Standard Terminology for Additive Manufacturing - Coordinate Systems and Test
[4]  
[Anonymous], 2015, E466-Standard Practice for Conducting Force Controlled Constant Amplitude Axial Fatigue Tests of Metallic Materials
[5]   Effects of build orientation and heat treatments on the tensile and fracture toughness properties of additively manufactured AlSi10Mg [J].
Araujo, Luana C. ;
Gabriel, Andre H. G. ;
da Fonseca, Eduardo B. ;
Avila, Julian A. ;
Jardini, Andre L. ;
Seno Junior, Roberto ;
Lopes, Eder S. N. .
INTERNATIONAL JOURNAL OF MECHANICAL SCIENCES, 2022, 213
[6]  
ASTM, 2021, E8E8M ASTM
[7]   Influence of heat treatment on the high-cycle fatigue properties and fatigue damage mechanism of selective laser melted AlSi10Mg alloy [J].
Baek, Min-Seok ;
Kreethi, R. ;
Park, Tae-Hyun ;
Sohn, Yongho ;
Lee, Kee-Ahn .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 819
[8]   On mechanical properties of SLM Al-Si alloy: Role of heat treatment-induced evolution of silicon morphology [J].
Bisht, Manoj Singh ;
Gaur, Vidit ;
Singh, I. V. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 858
[9]   Superheat-dependent microstructure of molten Al-Si alloys of different compositions studied by small angle neutron scattering [J].
Calvo-Dahlborg, M. ;
Popel, P. S. ;
Kramer, M. J. ;
Besser, M. ;
Morris, J. R. ;
Dahlborg, U. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 550 :9-22
[10]   Study on the fatigue behaviour of selective laser melted AlSi10Mg alloy [J].
Ch, Srinivasa Rakesh ;
Raja, A. ;
Jayaganthan, R. ;
Vasa, N. J. ;
Raghunandan, M. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 781