Influence of metallurgical parameters on the coercive strength of some carbon steels

被引:0
作者
Gerosa, R. [1 ]
Rivolta, B. [1 ]
Cusolito, M. [2 ]
Valsecchi, M. [2 ]
机构
[1] Politecnico di Milano, Polo Regionale di Lecco, 23900, Lecco
[2] Rodacciai Spa, Bosisio Parini (CO)
来源
Journal of ASTM International | 2007年 / 4卷 / 05期
关键词
Carbon steels; Coercive strength; Heat treatments;
D O I
10.1520/JAI100708
中图分类号
学科分类号
摘要
The final properties of a wire rod for magnetic components are strongly influenced by the specific steps of the industrial cycle which can be different according to the specific chemical composition of the steel. In this experimental work, measurements of coercive strength have been carried out on wire rods in different metallurgical conditions. The influence of work-hardening, as a function of some different drawing ratios, and the restoring of the coercive strength within the accepted values by heat treatments have been investigated. The carbon content and the steel chemical composition have also been evaluated. The obtained results give important information to the wire rods manufacturers for the respect of the technical delivery conditions. Copyright © 2007 by ASTM International.
引用
收藏
相关论文
共 9 条
[1]  
Chen C.W., Magnetism and Metallurgy of Soft Magnetic Materials, (1986)
[2]  
Hou C.K., Hu C.T., Lee S., Effect of Residual Aluminium on the Microstructure and Magnetic Properties of Low Carbon Electrical Steels, Materials Science & Engineering A (Structural Materials: Properties, Microstructure and Processing), A125, 2, pp. 241-247, (1990)
[3]  
Hou C.K., Hu C.T., Lee S., The Effect of Titanium and Niobium on Degradation of Magnetic Properties of Lamination Steels, J. Magn. Magn. Mater, 87, 1-2, pp. 44-50, (1990)
[4]  
Hou C.K., Hu C.T., Lee S., The Effect of Aluminum on the Magnetic Properties of Lamination Steels, IEEE Trans. Magn, 27, 5, pp. 4305-4309, (1991)
[5]  
Hou C.K., Hu C.T., Lee S., Effect of Rolling Strain on the Loss Separation and Permeability of Lamination Steels, IEEE Trans. Magn, 30, 2 PART 1, pp. 212-216, (1994)
[6]  
Hou C.K., Hu C.T., Lee S., Effect of Phosphorus on the Core Loss of Lamination Steels, J. Magn. Magn. Mater, 109, 1, pp. 7-12, (1992)
[7]  
Hou C.K., Effect of Hot Band Temper Rolling Strain on the Magnetic Properties of Low-carbon Electrical Steels, J. Magn. Magn. Mater, 162, pp. 291-330, (1996)
[8]  
Dimensions and Tolerances of Bright Products, (1999)
[9]  
Standard Test Methods for Determining Average Grain Size, Annual Book of ASTM Standards, (1996)