Effect of high energy ball milling washing process on properties of Nd2Fe14B particles obtained by reduction-diffusion

被引:3
作者
Galkin V. [1 ,2 ,3 ]
Haider K. [2 ,3 ]
Ahn J. [2 ,3 ]
Kim D. [2 ,3 ]
机构
[1] Materials Science and Engineering Department, Peter the Great Saint Petersburg Polytechnic University, 29, Polytechnicheskaya, St. Petersburg
[2] Convergence research center for development of mineral resources, Korea Institute of Geoscience and Mineral Resources, 124, Gwahakro, Yuseonggu, Daejeon
[3] Powder & Ceramics Division, Korea Institute of Materials Science, 797, Changwondaero, Seongsangu, Changwon, 51508, Gyeongnam
关键词
Calciothermic reduction; Hard magnetic particles; High-energy ball milling; Nd[!sub]2[!/sub]Fe[!sub]14[!/sub]B; Rare earth;
D O I
10.4028/www.scientific.net/KEM.822.244
中图分类号
学科分类号
摘要
. Nd2Fe14B particles were obtained from mixture of neodymium oxide, iron oxide, boric acid and CaH2 by reduction-diffusion process. Two different washing processes were used for the separation of magnetic particles from Ca and CaO matrix: usual washing with water and planetary ball milling process in ethanol media. Nd2Fe14BHx hydrogenated state was formed after usual washing with water. Ethanol planetary ball milling washing procedure prevented the formation of Nd2Fe14B hydrides during washing. Variation of milling parameters allowed producing particles with different morphology such as spherical or flakes after planetary ball milling washing process. Influence of milling parameters on magnetic properties of Nd2Fe14B powder was investigated. © 2019 Trans Tech Publications Ltd, Switzerland.
引用
收藏
页码:244 / 251
页数:7
相关论文
共 26 条
[1]  
Sagawa M., Fujimura S., Togawa N., Yamamoto H., Matsuura Y., New material for permanent magnets on a base of Nd and Fe (invited), Journal of Applied Physics, 55, pp. 2083-2087, (1984)
[2]  
Kim D., Vasilieva E.S., Nasibulin A.G., Lee D.W., Tolochko O. V., Kim B.K., Aerosol Synthesis and Growth Mechanism of Magnetic Iron Nanoparticles, Materials Science Forum, 534-536, pp. 9-12, (2007)
[3]  
Vasil E.S., Tolochko O. V, Semenov V.G., Volodin V.S., Kim D., Mössbauer Spectroscopy Analysis of the Phase Composition of Iron-Based Nanoparticles, Technical Physics Letters, 33, pp. 40-43, (2007)
[4]  
Choi C.J., Kim B.K., Tolochko O., Li-Da, Preparation and characterization of magnetic Fe, Fe/C and Fe/N nanoparticles synthesized by chemical vapor condensation process, Reviews on Advanced Materials Science, 5, pp. 487-492, (2003)
[5]  
Gonchukova N.O., Larionova T.V., Effect of long-term annealing below the glass transition range on heat capacity and Curie temperature for metallic glasses, Fizika i Khimiya Stekla, 20, pp. 134-135, (1994)
[6]  
Gorkunov E.S., Putilova E.A., Zadvorkin S.M., Makarov A. V, Pecherkina N.L., Fomina O. V, Behavior of Magnetic Characteristics in Promising Nitrogen Containing Steels upon Elastoplastic Deformation, The Physics of Metals and Metallography, 116, pp. 838-849, (2015)
[7]  
Nazarov D. V., Osmolovskaya O.M., Bobrysheva N.P., Smirnov V.M., Murin I. V., Peculiarities of phase transitions in nanosized vanadium dioxide: Magnetic characteristics, Nanotechnologies in Russia, 7, pp. 641-648, (2012)
[8]  
Alexandrov S.E., Protopopova V.S., Chemical Vapor Deposition of Ni-C Films from Bis-(Ethylcyclopentadienyl) Nickel, Journal of Nanoscience and Nanotechnology, 11, pp. 8259-8263, (2011)
[9]  
Burzo E., Permanent Magnets Based on R-Fe-B and R-Fe-C Alloys, Rep. Prog. Phys, 61, pp. 1099-1266, (1998)
[10]  
Jang T. S., Lee D. H., Yu J. H., Choi J. C., Seo S. W., Lee H. Y., Fabrication of ultrafine Nd-Fe-B powder by a modified reduction-diffusion process, Rare Metals, 25, pp. 223-226, (2006)