Research progress on corrosion and hydrogen embrittlement in hydrogen–natural gas pipeline transportation

被引:1
|
作者
Zhang H. [1 ]
Zhao J. [1 ]
Li J. [2 ]
Yu B. [2 ]
Wang J. [1 ]
Lyu R. [1 ]
Xi Q. [3 ]
机构
[1] School of Safety Engineering, Beijing Institute of Petrochemical Technology, Beijing
[2] School of Mechanical Engineering, Beijing Institute of Petrochemical Technology, Beijing
[3] Chengdu Natural Gas Chemical Plant, PetroChina Southwest Oil & Gasfield Company, Sichuan, Chengdu
关键词
Corrosion; H[!sub]2[!/sub]S/CO[!sub]2[!/sub] partial pressure ratio; Hydrogen blending ratio; Hydrogen charging; Hydrogen embrittlement; Hydrogen–natural gas blending; Material strength; Pipeline steel;
D O I
10.3787/j.issn.1000-0976.2023.06.013
中图分类号
学科分类号
摘要
Hydrogen, clean, efficient and zero-carbon, is seen as a most promising energy source. The use of existing gas pipelines for hydrogen–natural gas transportation is considered to be an effective way to achieve long-distance, large-scale, efficient, and economical hydrogen transportation. However, the pipelines for hydrogen–natural gas transportation contain lots of impurities (e.g., CH4, high-pressure H2, H2S and CO2) and free water, which will inevitably lead to corrosion and hydrogen embrittlement. To address this, researches and an outlook for corrosion and hydrogen embrittlement in hydrogen–natural gas pipeline transportation are discussed. The results showed that gas-phase hydrogen charging is suitable for hydrogen–natural gas transportation, but this technique lacks technical standards. Meanwhile, the liquid-phase hydrogen charging technique is more mature, but has large deviation from the engineering reality. In the hydrogen–natural gas transportation pipelines, corrosion and hydrogen embrittlement are synergetic and competitive, but the failure mechanism and change law when corrosion and hydrogen embrittlement coexist remain unclear, which need to be further clarified by experiments. The failure mechanism is believed to be mainly sensitive to three key factors, i.e. the H2S/CO2 partial pressure ratio, the hydrogen blending ratio, and material strength. The increase of the three factors will make the pipeline materials more corrosive and more sensitive to hydrogen embrittlement.
引用
收藏
页码:126 / 138
页数:12
相关论文
共 78 条
  • [1] WANG Minsheng, YAO Yunfei, Development situation and countermeasures of the oil and gas industry facing the challenge of carbon neutrality, Petroleum Drilling Techniques, 49, 5, pp. 1-6, (2021)
  • [2] WANG Zhen, HE Xu, CUI Xin, Strategic choice for oil and gas companies under the vision of carbon neutrality, Oil & Gas Storage and Transportation, 40, 6, pp. 601-608, (2021)
  • [3] YU Zilong, ZHANG Liye, NING Chen, Et al., Natural gas hydrogen mixing pipeline transportation and terminal application, Mechanics in Engineering, 44, 3, pp. 491-502, (2022)
  • [4] XIE Ping, WU Yi, LI Changjun, Et al., Research progress on pipeline transportation technology of hydrogenmixed natural gas, Oil & Gas Storage and Transportation, 40, 4, pp. 361-370, (2021)
  • [5] Transcript of the National Energy Administration's online press conference for the first quarter of 2022
  • [6] LI Jingfa, SU Yue, ZHANG Heng, Et al., Research progresses on pipeline transportation of hydrogen-blended natural gas, Natural Gas Industry, 41, 4, pp. 137-152, (2021)
  • [7] CHENG Yufeng, SUN Yinghao, ZHANG Yindi, Development of hydrogen pipelines and hydrogen embrittlement challenges of pipeline steel, Journal of Yangtze University (Natural Science Edition), 19, 1, pp. 54-69, (2022)
  • [8] ZHONG Bing, ZHANG Xuexiu, ZHANG Bo, Et al., Industrial development of hydrogen blending in natural gas pipelines in China, Strategic Study of CAE, 24, 3, pp. 100-107, (2022)
  • [9] China natural gas development report (2022)
  • [10] MESSAOUDANI Z L, RIGAS F, HAMID M D B, Et al., Hazards, safety and knowledge gaps on hydrogen transmission via natural gas grid: A critical review, International Journal of Hydrogen Energy, 41, 39, pp. 17511-17525, (2016)