Surface integrity investigation of a Zr52.5Ti5Cu17.9Ni14.6Al10 metallic glass after grinding

被引:1
|
作者
Lavisse B. [1 ]
Mendil N. [2 ]
Kapelski G. [1 ]
Cerutti X. [2 ]
Lenain A. [2 ]
Gravier S. [2 ]
Daudin R. [1 ]
机构
[1] SIMaP, CNRS, University of Grenoble Alpes, Grenoble
[2] Vulkam Inc., Amorphous Metal Micro Casting, Vulkam 101 Rue de la Physique, Saint-Martin-d'Hères
关键词
BMG; Bulk metallic glass; Grinding; Surface characterisation; Thermal damaging;
D O I
10.1504/IJMMM.2020.109853
中图分类号
学科分类号
摘要
Crystalline alloys, widely used in the industry, are a topic of important research regarding their integrity resistance towards machining. Such investigations are less intense when dealing with relatively newer and less popular materials such as bulk metallic glasses (BMGs). This is even truer when specific machining techniques, such as grinding, are involved. As BMG are increasingly promoted to diverse industrial areas, the study of the impact of grinding on their microstructural integrity is necessary. Indeed, the amorphous structure of BMG, at the origin of their remarkable properties, is metastable such that any exterior solicitation (heating, cooling, loading, etc.) can induce structural modifications, for instance local crystallisation, and therefore degrade or at least modify their characteristics. Using quick and straightforward characterisation techniques such as SEM imaging, optical microscopy and X-ray diffraction, the microstructural changes occurring in the BMG after severe grinding passes could be identified. It is shown that crystallisation can be detected below the grinded surface even for relatively small depth of cut. The results obtained on this peculiar composition help to propose a more generic methodology to safely use grinding on BMG. Copyright © 2020 Inderscience Enterprises Ltd.
引用
收藏
页码:430 / 441
页数:11
相关论文
共 50 条
  • [21] Study of Collective modes and Elastic Constants of Zr57Ti5Cu20Ni8Al10 Bulk Metallic Glass
    Thakore, B. Y.
    Suthar, P. H.
    Chaudhari, Prakruti
    Gajjar, P. N.
    Jani, A. R.
    ADVANCES IN MATERIALS SCIENCE AND TECHNOLOGY (AMST), 2014, 209 : 62 - +
  • [22] Plastic behavior of Zr51Ti5Ni10Cu25Al9 metallic glass under planar shock loading
    Yu Yu-Ying
    Xi Feng
    Dai Cheng-Da
    Cai Ling-Cang
    Tan Hua
    Li Xue-Mei
    Hu Chang-Ming
    ACTA PHYSICA SINICA, 2012, 61 (19)
  • [23] Volume and enthalpy relaxation in Zr55Cu30Ni5Al10 bulk metallic glass
    Haruyama, O.
    Nakayama, Y.
    Wada, R.
    Tokunaga, H.
    Okada, J.
    Ishikawa, T.
    Yokoyama, Y.
    ACTA MATERIALIA, 2010, 58 (05) : 1829 - 1836
  • [24] Femtosecond laser ablation of Zr55Al10Ni5CU30 bulk metallic glass
    Sano, Tomokazu
    Takahashi, Kengo
    Hirose, Akio
    Kobayashi, Kojiro F.
    THERMEC 2006, PTS 1-5, 2007, 539-543 : 1951 - +
  • [25] Friction Stir Welding of Zr55Cu30Ni5Al10 Bulk Metallic Glass
    Ji, Young Su
    Fujii, Hidetoshi
    Sun, Yufeng
    Maeda, Masakatsu
    Nakata, Kazuhiro
    Kimura, Hisamichi
    Inoue, Akihisa
    Nogi, Kiyoshi
    MATERIALS TRANSACTIONS, 2009, 50 (06) : 1300 - 1303
  • [26] Effect of cold rolling on glass transition of Zr55Al10Ni5Cu30 bulk metallic glass
    Hu Yong
    Li Jin-fu
    Zhang Peng-na
    Zhou Yao-he
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 (01) : 78 - 81
  • [27] Effect of cold rolling on glass transition of Zr55Al10Ni5Cu30 bulk metallic glass
    胡勇
    李金富
    张朋娜
    周尧和
    TransactionsofNonferrousMetalsSocietyofChina, 2010, 20 (01) : 78 - 81
  • [28] Preparation and mechanical properties of a new Zr-Al-Ti-Cu-Ni-Be bulk metallic glass
    Rao, X
    Si, PC
    Wang, JN
    Xu, Z
    Xu, S
    Wang, WM
    Wang, WH
    MATERIALS LETTERS, 2001, 50 (5-6) : 279 - 283
  • [29] Bending property enhancements of Zr55Cu30Al10Ni5 bulk metallic glass: Effects of various surface modifications
    Yu, Chia-Chi
    Chu, Jinn P.
    Lee, Cheng-Min
    Diyatmika, Wahyu
    Chang, M. H.
    Jeng, Jeng-Ywan
    Yokoyama, Yoshihiko
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 633 : 69 - 75
  • [30] Deformation behavior of a Zr55Al10Ni5Cu30 bulk metallic glass at high temperatures
    Shin, HS
    Jung, YJ
    Kim, KH
    Ahn, JH
    Kato, H
    Inoue, A
    Metastable, Mechanically Alloyed and Nanocrystalline Materials, 2005, 24-25 : 359 - 362