Corrosion mechanisms of Zr-based bulk metallic glasses in NaBr solution

被引:1
作者
Li, Chao-jun [1 ]
Zhang, Hao [2 ]
Wang, Wei [1 ]
Wei, Ran-feng [1 ]
Zheng, Rui [2 ]
Lv, Jing-wang [1 ]
Sun, Qi-jing [1 ]
Zhang, Guo-yang [1 ]
Zhao, Xiang-jin [1 ]
Liu, Li [2 ]
机构
[1] Yantai Univ, Coll Nucl Equipment & Nucl Engn, 30 Qingquan Rd, Yantai 264005, Shandong, Peoples R China
[2] Yantai Univ, Sch Environm & Mat Engn, 30 Qingquan Rd, Yantai 264005, Shandong, Peoples R China
基金
中国国家自然科学基金;
关键词
Bulk metallic glass; Corrosion behavior; Br-Pitting corrosion; Passive film; FORMING ABILITY; THERMAL-STABILITY; PITTING CORROSION; BEHAVIOR; ALLOY; AL; TI; RESISTANCE;
D O I
10.1016/j.jnoncrysol.2024.123069
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this paper, the corrosion mechanisms of Zr55Cu35Al10 and Zr56Co28Al16 bulk metallic glasses (BMGs) in 3.5 wt.% NaBr solution was systematically investigated by the kinetic potential polarization and electrochemical impedance spectroscopy. Both Zr55Cu35Al10 and Zr56Co28Al16 BMGs were subjected to pitting damage during the polarization process in NaBr solution due to the presence of Br- ions. However, Zr56Co28Al16 BMG exhibits better corrosion resistance compared to Zr55Cu35Al10 BMG. Zr55Cu35Al10 BMG experiences selective dissolution of alloying elements under the attack of Br-, and Cu element was enriched in the corrosion pit. The surface of Zr56Co28Al16 BMG shows a more uniform distribution of elements after corrosion. Simultaneously, the substitution of Cu by Co changes the composition of the passive films and increases the relative content of ZrO2, which is a principal factor contributing to the enhanced stability of Zr56Co28Al16 BMG's passive film.
引用
收藏
页数:9
相关论文
共 41 条
  • [1] A novel criterion for predicting the glass-forming ability in Zr-Cu-Al ternary alloys: A molecular dynamics study
    Abbasi, M. H.
    Tavakoli, R.
    Shabestari, S. G.
    [J]. INTERMETALLICS, 2024, 164
  • [2] Atkins P. W., 1997, PHYS CHEM
  • [3] Bard A. J., 1985, Standard Potentials in Aqueous Solution, DOI DOI 10.1201/9780203738764
  • [4] Electrochemical characterization of ZrTi alloys for biomedical applications. Part 2: The effect of thermal oxidation
    Bolat, Georgiana
    Izquierdo, Javier
    Mareci, Daniel
    Sutiman, Daniel
    Souto, Ricardo M.
    [J]. ELECTROCHIMICA ACTA, 2013, 106 : 432 - 439
  • [5] THE ANALYSIS OF ELECTRODE IMPEDANCES COMPLICATED BY THE PRESENCE OF A CONSTANT PHASE ELEMENT
    BRUG, GJ
    VANDENEEDEN, ALG
    SLUYTERSREHBACH, M
    SLUYTERS, JH
    [J]. JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 1984, 176 (1-2): : 275 - 295
  • [6] Mechanical, wetting and corrosion properties of a Zr-based amorphous alloy composite consolidated by spark plasma sintering
    Cai, A. H.
    Zhou, G.
    Li, P. W.
    Ding, D. W.
    An, Q.
    Li, Yixian
    Yang, Q.
    Mao, H.
    [J]. JOURNAL OF NON-CRYSTALLINE SOLIDS, 2023, 621
  • [7] Excellent corrosion and wear resistance of amorphous and crystalline ZrCoAl alloys
    Chae, W. S.
    Li, M. W.
    Cao, Q. P.
    Wang, X. D.
    Ding, S. Q.
    Zhang, D. X.
    Jiang, J. Z.
    Caron, A.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 968
  • [8] Crystallization and corrosion resistance of Zr-Ti-Y-Al-Cu-Ni-Co-Fe complex multi -component bulk metallic glasses
    Chen, Chen
    Zhang, Hang
    Fan, Yanzhou
    Zhang, Weiwei
    Wei, Ran
    Guan, Shaokang
    Wang, Tan
    Kong, Bin
    Zhang, Tao
    Li, Fushan
    [J]. INTERMETALLICS, 2020, 118
  • [9] Corrosion behavior of Pb-39Mg-10Al-1.5B alloy in sodium halide solutions
    Duan, Yonghua
    Li, Ping
    Zhang, Min
    Peng, Mingjun
    Ma, Lishi
    Shu, Baipo
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 729 : 1108 - 1117
  • [10] Thermal stability and mechanical properties of a Zr-based bulk amorphous alloy
    Fátay, D
    Gubicza, J
    Szommer, P
    Lendvai, J
    Blétry, M
    Guyot, P
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 387 : 1001 - 1004