Generation of allowable stress for indigenously developed 304HCu Stainless steel

被引:1
|
作者
Ganesh Kumar J. [1 ]
Ganesan V. [1 ]
Nandagopal M. [1 ]
Reddy G.V.P. [1 ]
机构
[1] Metallurgy and Materials Group, Indira Gandhi Centre for Atomic Research, Kalpakkam
关键词
304HCu SS; Allowable; Creep; Design; Isochronous;
D O I
10.1016/j.ijpvp.2023.105015
中图分类号
学科分类号
摘要
The 304HCu stainless steel (SS) is the candidate material for reheater and superheater tubes in Advanced Ultra Supercritical (AUSC) coal-fired power plants of India. In the present study, the creep design data have been generated for indigenously developed 304HCu SS using the creep properties (creep strain and the rupture life) and tensile properties available at the temperatures 923 K, 973 K and 1023 K. The time dependent allowable stresses were obtained for the above steel according to the stress criteria specified in ASME Section III Division 5 Subsection HB. The allowable stresses were also derived in the creep as well as non-creep regimes as per the guidelines in ASME Section IID. In both the cases, the maximum allowable stress at each temperature was dictated by the stress to cause rupture. The allowable stress determined as per Section IID was the same as that estimated according to section III.5 HB for creep exposure of 100,000 h. Further, it must be mentioned that, at the temperature range 923–1023 K, the indigenously developed 304HCu SS possess allowable stresses that are in par with the corresponding values specified in ASME code case 2328–2. © 2023 Elsevier Ltd
引用
收藏
相关论文
共 50 条
  • [1] Creep Rupture Properties of Indigenously Developed 304HCu Austenitic Stainless Steel
    V. Ganesan
    K. Laha
    A. K. Bhaduri
    Transactions of the Indian Institute of Metals, 2016, 69 : 247 - 251
  • [2] Creep Rupture Properties of Indigenously Developed 304HCu Austenitic Stainless Steel
    Ganesan, V.
    Laha, K.
    Bhaduri, A. K.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2016, 69 (02) : 247 - 251
  • [3] Initial Stage Oxidation of 304HCu Stainless Steel in Oxygen Environment
    Archana, M.
    Rao, Ch. Jagadeeswara
    Ningshen, S.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2025, 78 (02)
  • [4] Characterization of Solidification Cracking in 304HCu Austenitic Stainless Steel Welds
    Ravibharath, R.
    Muthupandi, V.
    Bala Srinivasan, P.
    Devakumaran, K.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2020, 73 (09) : 2345 - 2353
  • [5] Characterization of Solidification Cracking in 304HCu Austenitic Stainless Steel Welds
    R. Ravibharath
    V. Muthupandi
    P. Bala Srinivasan
    K. Devakumaran
    Transactions of the Indian Institute of Metals, 2020, 73 : 2345 - 2353
  • [6] Analysis of creep deformation and damage behaviour of 304HCu austenitic stainless steel
    Sahoo, Kanhu Charan
    Goyal, Sunil
    Ganesan, Vaidyanathan
    Vanaja, Jagannathan
    Reddy, Gondesh Varaprasad
    Padmanabhan, Parameswaran
    Laha, Kinkar
    MATERIALS AT HIGH TEMPERATURES, 2019, 36 (05) : 388 - 403
  • [7] Assessment of creep deformation and rupture behaviour of 304HCu austenitic stainless steel
    Sahoo, K. C.
    Goyal, Sunil
    Laha, K.
    2ND INTERNATIONAL CONFERENCE ON STRUCTURAL INTEGRITY AND EXHIBITION 2018 (SICE 2018), 2019, 14 : 60 - 67
  • [8] Influence of temperature on multiaxial creep behaviour of 304HCu austenitic stainless steel
    Sahoo, K. C.
    Vijayanand, V. D.
    Goyal, Sunil
    Parameswaran, P.
    Laha, K.
    MATERIALS SCIENCE AND TECHNOLOGY, 2019, 35 (18) : 2181 - 2199
  • [9] Effect of notch depth on creep rupture behaviour of 304HCu austenitic stainless steel
    Sahoo, Kanhu Charan
    Goyal, Sunil
    Paul, V. Thomas
    Laha, Kinkar
    MATERIALS AT HIGH TEMPERATURES, 2020, 37 (05) : 295 - 304
  • [10] Evaluation of Boundary Interface Character as a Function of Annealing Temperature in 304HCu Stainless Steel
    Manmath Kumar Dash
    Metallurgical and Materials Transactions A, 2021, 52 : 1180 - 1184