共 50 条
- [1] Initial stage of degradation process of alumina-silica refractory by molten Al-5Mg alloy Keikinzoku/Journal of Japan Institute of Light Metals, 2022, 72 (11): : 631 - 637
- [2] Internal corundum growth in alumina-silica refractory during exposure to molten Al-5Mg alloy Keikinzoku/Journal of Japan Institute of Light Metals, 2022, 72 (11): : 638 - 644
- [4] Additives and the corrosion resistance of aluminosilicate refractories in molten Al-5Mg JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 1998, 50 (02): : 30 - 34
- [5] Additives and the corrosion resistance of aluminosilicate refractories in molten Al-5Mg JOM, 1998, 50 : 30 - 34
- [7] Experimental simulation of hot rolling of aluminium alloy Al-5Mg JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2003, 19 : 231 - 233