Wear for low friction-running-in and tribochemical wear

被引:0
|
作者
Adachi, Koshi [1 ]
机构
[1] Department of Mechanical Systems Engineering, Tohoku University, 6-6-01. Aoba,Aramaki-aza, Aoba-ku, Sendai-shi, Miyagi,980-8579, Japan
来源
Toraibarojisuto/Journal of Japanese Society of Tribologists | 2019年 / 64卷 / 05期
关键词
Tribology; -; Friction; Textures;
D O I
暂无
中图分类号
学科分类号
摘要
It is well-known that beginning of sliding so-called running-in is an important for stable low friction by formation of well- conformed interface with suitable tribo-chemical product. To form such functional interface, initial wear in the conforming proceb in the early stages of friction is key to lead for changing in the material, physical and chemical properties of the surface. Further, initial wear during running-in leads to continuous self-formation of low friction interface due to tribo-chemical wear at the stable low friction stage. The running-in control technique for self-forming such low friction interface more surely and stably is a low friction technology. The surface texture that can actively control tribo-chemical reaction introduced in this paper is one of the promising low friction technologies.. © 2019 Japanese Society of Tribologists. All rights reserved.
引用
收藏
页码:288 / 293
相关论文
共 50 条
  • [21] Adhesion at friction and wear
    Dmitry P. Markov
    Friction, 2022, 10 : 1859 - 1878
  • [22] Friction evolution in running-in of sliding wear of cast iron processed in Gleeble
    Zhang, Q.
    Jiang, Z. Y.
    Wei, D. B.
    Xie, G.
    Han, J. T.
    ADVANCES IN ABRASIVE TECHNOLOGY XVI, 2013, 797 : 713 - +
  • [23] Friction and wear of human hair fibres
    Bowen, James
    Johnson, Simon A.
    Avery, Andrew R.
    Adams, Michael J.
    SURFACE TOPOGRAPHY-METROLOGY AND PROPERTIES, 2016, 4 (02):
  • [24] Isolating the tribochemical and mechanical effects of nanofillers on PTFE wear
    Alam, Kazi Istiaque
    Bragaw, Pearce
    Burris, David L.
    WEAR, 2022, 494-495
  • [25] A study of the effects of friction on flank wear and the role of friction in tool wear monitoring
    Siddhpura, A.
    Paurobally, R.
    AUSTRALIAN JOURNAL OF MECHANICAL ENGINEERING, 2012, 10 (02) : 141 - 156
  • [26] A low friction and ultra low wear rate PEEK/PTFE composite
    Burris, David L.
    Sawyer, W. Gregory
    WEAR, 2006, 261 (3-4) : 410 - 418
  • [27] Friction and wear behaviour of low-friction coatings in conventional and alternative fuels
    Gustavsson, F.
    Forsberg, P.
    Jacobson, S.
    TRIBOLOGY INTERNATIONAL, 2012, 48 : 22 - 28
  • [28] Wear mechanisms and friction parameters for sliding wear of micron-scale polysilicon sidewalls
    Alsem, D. H.
    van der Hulst, R.
    Stach, E. A.
    Dugger, M. T.
    De Hosson, J. Th. M.
    Ritchie, R. O.
    SENSORS AND ACTUATORS A-PHYSICAL, 2010, 163 (01) : 373 - 382
  • [29] Tailoring polyimide composites with low friction and wear at high temperatures
    Duan, Chunjian
    Gao, Chuanping
    Li, Song
    Yang, Rui
    Yang, Zenghui
    Zhang, Yaoming
    Tao, Liming
    Zhang, Xinrui
    Wang, Qihua
    Wang, Tingmei
    JOURNAL OF APPLIED POLYMER SCIENCE, 2022, 139 (09)
  • [30] Wear Test Apparatus for Friction and Wear Evaluation Hip Prostheses
    Hua, Zikai
    Dou, Pingchuan
    Jia, Haili
    Tang, Fei
    Wang, Xiaojing
    Xiong, Xin
    Gao, Leiming
    Huang, Xiuling
    Jin, Zhongmin
    FRONTIERS IN MECHANICAL ENGINEERING-SWITZERLAND, 2019, 5